| HS Code | 525197 |
| Productname | Polyisobutylene HRDF-750 |
| Chemicaltype | High reactive polyisobutylene |
| Appearance | Colorless to pale yellow viscous liquid |
| Numberaveragemolecularweight | 750 g/mol |
| Densityat15c | 0.89 g/cm3 |
| Kinematicviscosityat100c | 130 mm2/s |
| Flashpoint | ≥180 °C |
| Pourpoint | ≤-30 °C |
| Colorapha | ≤50 |
| Watercontent | ≤0.05 wt% |
| Acidvalue | ≤0.01 mg KOH/g |
| Reactivedoublebondcontent | ≥75% |
| Residualchlorine | ≤10 ppm |
| Volatilematter | ≤0.5 wt% |
As an accredited Polyisobutylene HRDF-750 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Polyisobutylene HRDF-750 is supplied in sealed 25 kg containers, labeled with product name, batch number, and handling information. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Polyisobutylene HRDF-750, securely stowed and lashed in export-grade packaging for ocean shipment. |
| Shipping | Polyisobutylene HRDF-750 is a non-hazardous polymer, generally not regulated for transport (verify against current SDS/regulations). Ship in sealed original drums or IBCs, protect from heat, sunlight, moisture, and contamination, secure the load, and label with product name, batch number, and handling information. |
| Storage | Store Polyisobutylene HRDF-750 in tightly closed original containers in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Protect from moisture, dust, and contamination; avoid freezing or excessive temperatures. Keep containers clean, labeled, and properly stacked. Maintain good housekeeping, spill containment, and follow the supplier’s SDS and local regulations. |
| Shelf Life | Shelf life: typically 24 months in original, unopened containers stored cool, dry, and away from direct sunlight. |
Polyisobutylene HRDF-750 is charged to a glass-lined stirred reactor blanketed with nitrogen because free radical oxidation at the terminal vinylidene group creates color bodies that interfere with downstream imidation. The number-average molecular weight is specified near 750 g/mol. The grade is selected for high terminal vinylidene content. When the vinylidene content falls below 70 mol% by proton nuclear magnetic resonance, maleation conversion drops and unreacted PIB carry-over rises. Maleic anhydride is metered into the reactor at a mole ratio of 1.05:1 to 1.40:1 relative to the olefinic end group. The reactor bulk temperature is held between 180 °C and 220 °C with a hot-oil jacket. The Alder-ene addition is exothermic. Jacket cooling is modulated to prevent local hot spots above 220 °C. After maleation, vacuum stripping at 15 kPa to 40 kPa absolute removes unreacted maleic anhydride below 0.5 wt% before the amine charge. The stripped anhydride number is determined by ASTM D974. The resulting polyisobutenyl succinic anhydride is transferred to a second reactor and reacted with tetraethylenepentamine or a heavy polyamine at 150 °C to 170 °C. The imidation step is monitored by Fourier-transform infrared spectroscopy. The amide carbonyl band at 1,650 cm⁻¹ is reduced below detection before final neutralization. The succinimide dispersant is then introduced into passenger car and heavy-duty crankcase formulations at 2 wt% to 8 wt% on a neat-additive basis. The formulated engine oil must retain total base number under ASTM D2896 and meet sulfated ash limits under ASTM D874. This balance is sensitive to residual free maleic anhydride because carboxylic acid functionality consumes base and promotes sludge. The processing incompatibility with amine-based additives is avoided only when stripping is complete. HRDF-750 is not employed as a stand-alone lubricant or as a viscosity modifier. The molecular weight is too low to produce high-temperature high-shear viscosity under SAE J300. Its terminal product function is confined to the succinimide intermediate and the final dispersant molecule. Batch-to-batch variance in unreacted PIB must remain below 2 wt% to avoid cold-start sludge in the formulated oil.
PIBA gasoline detergent production differs from succinimide dispersant chemistry because the PIB tail is converted to a primary amine without a succinic acid bridge. HRDF-750 is first hydroformylated with synthesis gas over a phosphine-modified rhodium catalyst at 120 °C to 180 °C and 10 MPa to 30 MPa. The terminal vinylidene group reacts to a terminal alcohol with high selectivity only when the feed is free of sulfur and chloride. Catalyst poisons must be limited to 5 mg/kg sulfur and 3 mg/kg chloride. The resulting polyisobutyl alcohol is then subjected to reductive amination in a fixed-bed reactor over a nickel or cobalt catalyst. The amine product is a clear liquid. It is combined with carrier oil and solvent to produce a fuel detergent concentrate. The concentrate is dosed into gasoline at 50 ppm to 300 ppm actives. In port-fuel-injector engines, the polar amine head adsorbs onto metal surfaces and the PIB tail provides a soluble hydrocarbon shield. Deposit control performance is measured by ASTM D6201 for intake valve deposits and by CEC F-05-93 for keep-clean performance. The fuel detergent must not increase combustion chamber deposits. Therefore the base PIB backbone must be saturated and free of olefin oligomers that crack in the combustion chamber. HRDF-750 is advantageous because its narrow molecular weight distribution reduces heavy oligomer carry-over. The product is not a deposit remover in the absence of the amine head group. Unreacted polyisobutylene carry-over into the finished detergent above 10 wt% dilutes the active species and raises the dosage required to pass ASTM D6201. This is an economic and compositional boundary, not a lubricant-performance advantage. The hydroformylation catalyst activity also declines if the PIB feed contains residual maleic anhydride or chloride from upstream. Feed specifications therefore limit residual maleic anhydride to below 0.1 wt% and chloride to below 5 mg/kg.
The following compliance matrix identifies the standard designations used for each downstream segment and the measured endpoint.
| Application | Relevant standard | Measured endpoint |
|---|---|---|
| PIBSA succinimide dispersant | ASTM D874 | Sulfated ash of formulated oil |
| PIBSA succinimide dispersant | ASTM D2896 | Total base number retention |
| PIBA gasoline detergent | ASTM D6201 | Intake valve deposit mass |
| Diesel deposit control | CEC F-98-08 | Injector needle lift loss |
| Metalworking fluid | ASTM D2783 | Four-ball weld point |
| Two-stroke oil | JASO M345/ISO 13738 | Lubricity and exhaust system blocking |
In diesel fuel deposit control chemistry, the HRDF-750 backbone is converted into a higher-molecular-weight succinimide by the same maleation route used for crankcase lubricants. The separation is made at the imidation stage. Diesel fuel detergents require complete imide ring formation rather than partial amide termination because the imide ring has higher thermal stability in high-pressure common-rail injectors. The reaction is carried out in a continuous high-shear reactor at 160 °C to 180 °C. The imidation endpoint is confirmed by infrared spectroscopy until the amide carbonyl band at 1,650 cm⁻¹ disappears. The resulting succinimide is blended into diesel fuel at 40 ppm to 250 ppm actives. It is evaluated under CEC F-98-08 for common-rail injector needle lift loss and under ASTM D6468 for high-temperature distillate fuel deposits. The material is not a cetane improver and does not raise the derived cetane number under ASTM D6890. It also does not correct poor lubricity as measured by ASTM D6079. Therefore the commercial fuel additive package must contain separate lubricity improvers and cetane improvers. The compatibility issue is that high concentrations of ethylhexyl nitrate cetane improver can reduce the shelf life of the succinimide. The additive package is stored in nitrogen-blanketed tanks to prevent oxidative darkening. The concentration of HRDF-750-derived succinimide in the final diesel fuel is low. However, the upstream concentrate may contain 30 wt% to 60 wt% active material. The concentrate viscosity at 40 °C is controlled below 1,000 mm²/s for accurate injection into the diesel blending stream.
Medium-speed trunk piston engine oils for marine and stationary power generation require a balance between water separation and corrosion protection in the presence of condensed water. A HRDF-750-derived succinate half-ester is prepared by ring-opening the PIBSA intermediate with a short-chain polyol. The residual carboxyl group is then neutralized with calcium hydroxide to form a calcium carboxylate rust inhibitor. The product is introduced into the formulated engine oil at 0.05 wt% to 0.50 wt% active. Water separability is evaluated by ASTM D1401 at 54 °C. A pass requires complete water separation within 30 min. Rust inhibition is validated by ASTM D665 B in synthetic seawater. Over-neutralization is a defined processing limit. If the total acid number before neutralization is below 1.0 mg KOH/g, the resulting ester is over-neutralized and the free calcium content destabilizes the zinc dialkyldithiophosphate antiwear additive. If the total acid number exceeds 5.0 mg KOH/g, the product itself becomes acidic and fails the ASTM D665 B rust test. Therefore the neutralization endpoint is controlled within 1.0 mg KOH/g to 5.0 mg KOH/g by potentiometric titration. The low pour point of HRDF-750-derived ester reduces the concentrate viscosity compared with high-molecular-weight PIB derivatives. Cold-start filter plugging is monitored by ASTM D6749 pour point measurement. The product is not a primary demulsifier. It requires a separate polyalkylene glycol demulsifier when the oil contacts high volumes of fresh water. The HRDF-750 succinate ester must not be combined with amine-based dispersants in the same concentrate without prior compatibility testing because carboxylate-amine interaction can form high-viscosity salts.
For two-stroke gasoline engine oil blending, Polyisobutylene HRDF-750 is added in the final trim stage as a low-viscosity hydrophobic diluent, not as a primary polymer tackifier. A typical two-stroke lubricant contains a high-molecular-weight polyisobutylene or bright stock, a biodegradable ester, and a mineral oil. HRDF-750 lowers the kinematic viscosity of the blend without adding a low-boiling petroleum distillate that increases smoke. The dosage is limited to 5 wt% to 15 wt% of the lubricant. Higher addition rates reduce the film thickness of the lubricant and promote piston ring sticking in air-cooled engines. The finished oil is tested under JASO M345/ISO 13738 for lubricity, smoke, and exhaust system blocking. The low molecular weight of HRDF-750 means that it does not contribute high-temperature high-shear viscosity. The product is dissolved into the blend at 60 °C to 70 °C with constant agitation. The pour point of the finished oil is measured by ISO 3016. In pre-mix applications with high methanol content, phase separation occurs below 0 °C. This incompatibility must be addressed by adjusting the ester co-solvent content.
Replacement of chlorinated paraffins in metalworking fluid packages places a narrow solubility constraint on the carrier oil because the PIB tail is nonpolar but the succinate ester head is polar. A HRDF-750 succinate ester is synthesized by ring-opening the PIBSA intermediate with a long-chain alcohol or a hindered polyol. The residual acid is neutralized with potassium hydroxide or an alkanolamine. The molecule is evaluated as a lubricity additive in neat and emulsion-type metalworking fluids at 0.5 wt% to 3.0 wt% active. Extreme pressure performance is measured by ASTM D2783 four-ball weld point. Copper corrosion is tested by ASTM D130. Aluminum staining is controlled by limiting chloride content to below 10 mg/kg in the finished ester. The esterification temperature is held below 160 °C to prevent thermal decarboxylation of the half-ester. Above 160 °C, the acid number drifts upward and the product darkens. The darkening is measured by ASTM D1500 color. The HRDF-750 backbone provides a lower neat viscosity than an equivalent C20-C28 linear alpha-olefin succinate ester. The resulting fluid is used in high-speed grinding operations where low mist and fast chip settling are required. However, published data for this specific HRDF-750 metalworking configuration is limited compared with engine oil and fuel additive applications. Pilot-scale validation in a ball-on-flat tribometer or a double-disk tribometer is required before production qualification.
Competitive Polyisobutylene HRDF-750 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@alchemist-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@alchemist-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Polyisobutylene HRDF-750 is a high-viscosity, fully saturated polyisobutylene homopolymer supplied as a pale yellow to translucent bale for adhesive, sealant, and polymer modification applications. The numerical suffix 750 identifies the high-retention, low-flow grade range; the manufacturer’s certificate of analysis remains the controlling document for lot-specific molecular weight, intrinsic viscosity, and volatile content. The material is produced by cationic polymerization of isobutylene and contains no diene-derived unsaturation. Sulfur-accelerated vulcanization is therefore ineffective, but the saturated backbone contributes to low gas permeability and resistance to ozone-induced chain scission when assessed by oxygen transmission per ASTM D3985-17 and ozone resistance per ISO 1431-1:2022 on formulated articles. Representative density values for high-molecular-weight polyisobutylene fall between 0.91 g/cm³ and 0.93 g/cm³ at 25 °C according to ISO 1183-1:2019. The glass transition temperature is approximately -70 °C when measured by differential scanning calorimetry per ISO 11357-2:2020; the polymer remains flexible at low temperatures, but cold flow under static load is lower than that of low-molecular-weight PIB fluids. Published data for this precise HRDF-750 configuration is limited, and representative ranges must not be read as lot-specific specifications.
For incoming inspection, the following methods are used: intrinsic viscosity in cyclohexane at 30 °C per ISO 1628-3, density per ISO 1183-1:2019, volatile matter per ISO 3251:2019, ash per ISO 3451-1:2019, and water content per ISO 15512:2019. The supplier may also report melting range by differential scanning calorimetry per ISO 11357-3:2018. Because HRDF-750 is not a flowable melt at conventional melt-flow test temperatures, melt mass-flow rate per ISO 1133-1:2022 is generally not applied to this grade.
Low-molecular-weight polyisobutylene grades, typically with viscosity-average molecular weights between 500 g/mol and 5,000 g/mol, are used as plasticizers, tackifiers, and lubricant additives. HRDF-750 belongs to the high-molecular-weight class with a representative viscosity-average molecular weight range of 450,000 g/mol to 750,000 g/mol when measured by ISO 1628-3 in cyclohexane at 30 °C. The practical consequence is a reduction in cold flow, lower volatile loss, and higher cohesive strength. At 105 °C for 2 h per ISO 3251:2019, low-molecular-weight PIB fluids may show volatile losses above 5 wt%, whereas high-molecular-weight PIB grades are typically below 1 wt%. In tackified adhesive formulations, substitution of a low-molecular-weight PIB fluid with HRDF-750 raises static shear resistance as measured by ASTM D3654-22 but requires reformulation of tackifier content to maintain loop tack per ASTM D6195-22. The saturated structure also distinguishes HRDF-750 from butyl rubber; butyl rubber contains isoprene units for sulfur cure, while HRDF-750 cannot be crosslinked by sulfur and is used as an uncured high-viscosity modifier.
HRDF-750 also differs from high-molecular-weight PIB grades supplied as solutions in mineral oil. The neat-bale form requires more mixing energy but eliminates the diluent oil from the final formulation and permits higher PIB content in sealants and adhesives. Compared with styrene-isoprene-styrene block copolymers, HRDF-750 has a lower plateau modulus at 100 °C and a broader damping peak when measured by dynamic mechanical analysis per ISO 6721-1; it is therefore not a total replacement for styrenic block copolymers in high-temperature structural adhesives, but it contributes gas-barrier and low-temperature tack performance in multilayer constructions.
| Parameter | Test method | Low-MW PIB | HRDF-750 class | Butyl rubber |
|---|---|---|---|---|
| Viscosity-average molecular weight | ISO 1628-3 | 500–5,000 g/mol | 450,000–750,000 g/mol | high; Mooney viscosity controls |
| Volatile loss at 105 °C / 2 h | ISO 3251:2019 | can exceed 5 wt% | typically <1 wt% | low |
| Sulfur cure response | ISO 6502 | not applicable | not applicable | applicable |
| Static shear on pressure-sensitive adhesive | ASTM D3654-22 | lower | higher | not typically used |
Representative values only; lot-specific certificates of analysis supersede this table.
In hot-melt pressure-sensitive adhesive lines, HRDF-750 is added at 5 wt% to 20 wt% of the elastomer fraction to increase cohesive strength without adding a second curing stage. The addition is normally pre-blended with a liquid aliphatic tackifier at a 1:1 ratio before entering the main mixing zone. On a 40 mm corotating twin-screw extruder with an L/D ratio of 44:1, pre-blending at 60 °C to 80 °C reduces motor load by approximately 15% compared with direct bale addition. Static shear holding power is measured with a 1 kg load and 1.0 in² contact area per ASTM D3654-22; loop tack is measured per ASTM D6195-22. The peel-shear balance shifts toward higher shear when HRDF-750 is substituted for a low-molecular-weight PIB plasticizer at constant tackifier content. Cohesive failure at elevated temperature is reduced when evaluated by shear adhesion failure temperature per ASTM D4498-07(2015), but immediate wet-out on polyethylene and recycled board may decrease, as reflected in lower loop tack values. The operating window for the adhesive mixing zone is restricted: melt temperature at the die must remain below 180 °C because chain scission accelerates above this threshold. When higher line speed is required, shear heating must be controlled by screw design rather than by raising barrel set points; excessive viscous dissipation can produce local temperatures 15 °C above the barrel set point.
Pre-compounding of HRDF-750 with fillers and tackifiers is performed in a sigma-blade mixer or a corotating twin-screw extruder. For filler-loaded sealants, the mixer is charged with HRDF-750 and a portion of the process oil at 60 °C to 80 °C; filler addition begins only after the polymer has formed a coherent flux. If the filler moisture content exceeds 0.5 wt% as measured by ISO 15512:2019, pre-drying at 80 °C for 4 h is required to prevent void formation and reduced adhesion to polar substrates. The polymer itself absorbs less than 0.1 wt% water at 23 °C and 50% RH per ISO 62:2008. Direct bale addition without pre-blending can cause feed-throat smearing and screw-root build-up on grooved-barrel extruders; the material can block the feed throat if the feed zone temperature exceeds 90 °C. Internal mixer drop temperatures are maintained between 130 °C and 150 °C; the compound is discharged before 160 °C to prevent molecular weight loss. Production records from high-viscosity PIB compounding lines show that lot-to-lot intrinsic viscosity variation can influence motor load by ±5% when the same mixer fill factor is used. The fill factor is adjusted according to lot-specific intrinsic viscosity rather than holding a fixed charge mass. Dilution of HRDF-750 is carried out in aliphatic or aromatic hydrocarbons; polar solvents such as ethanol and acetone are not suitable. Contact with strong oxidizing agents, nitric acid, or high-pressure oxygen is to be avoided because radical chain scission degrades the polymer instead of forming a crosslink network. Peroxide curing is generally ineffective for HRDF-750 and may accelerate molecular weight loss. Storage at or below 35 °C, protected from sunlight, and with bale stack heights below 1.5 m reduces cold-flow deformation during warehouse storage.
The rheological profile of HRDF-750 is characterized by high viscosity at low shear and pronounced shear thinning in hot-melt mixing. Dynamic shear measurements on a parallel-plate rheometer per ISO 6721-10 at 160 °C show that complex viscosity at 0.1 rad/s is several orders of magnitude higher than at 100 rad/s. This shear-thinning response is exploited in screw plasticization but complicates laboratory comparison of different lots. Lot acceptance therefore uses intrinsic viscosity per ISO 1628-3 or Mooney viscosity if agreed. Melt rheology is not typically specified by melt mass-flow rate because the values are below the practical resolution of ISO 1133-1:2022 at standard temperatures. Oxidative induction time per ISO 11357-6:2018 is formulation-dependent and is used only to verify stabilizer package activity, not as a specification for the neat polymer. Published data for the HRDF-750-specific rheological master curve is limited, so processing trials should be based on small-scale torque rheometry and then scaled to the production line.
Regulatory status for HRDF-750 is end-use dependent. The polymer is subject to REACH registration in the European Union; a valid registration number must be provided in Section 1 of the safety data sheet. Food-contact suitability is not assumed from the polymer composition alone and must be confirmed for the finished article under the applicable national or regional regulation, such as FDA 21 CFR 177.1570 or EU Regulation (EU) No 10/2011. RoHS Directive 2011/65/EU screening for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE is typically performed by X-ray fluorescence on homogeneous polymer layers; report limits of 1000 ppm for lead and 100 ppm for cadmium are commonly applied, but supplier documentation is required. Low volatile content below 1 wt% per ISO 3251:2019 supports low emission potential in indoor adhesive applications, although finished-product emission testing per ISO 16000-6 or ASTM D5116-17 is required for specific compliance claims.
| Regulation or standard | Scope | Relevant parameter | Data requirement |
|---|---|---|---|
| REACH | EU market supply | registration number | SDS Section 1 |
| 2011/65/EU | RoHS homogeneous polymer fraction | Pb, Cd, Hg, Cr6, PBB, PBDE | XRF screening; report limits |
| FDA 21 CFR 177.1570 | US food contact | migration | end-use confirmation |
| EU 10/2011 | EU food contact | overall migration | finished article testing |
| ISO 16000-6 | indoor VOC emissions | volatile organic compounds | product-specific emission test |
In butyl sealant and cable flooding compounds, HRDF-750 serves as a high-viscosity modifier. In a butyl sealant formulation, replacement of 10 wt% of a medium-molecular-weight PIB with HRDF-750 reduces slump when tested per ISO 7390:2003 and improves low-temperature flexibility at -40 °C per ISO 9047:2001. Water vapour transmission rate is assessed by ASTM E96/E96M-22; high-molecular-weight PIB-rich formulations are specified when moisture ingress must remain below the project-specific threshold. For cable flooding compounds, HRDF-750 is blended with microcrystalline wax and polyolefin oil to increase compound viscosity. D.C. volume resistivity at 23 °C typically exceeds 1×10¹⁴ Ω·cm according to ASTM D257-14. In stretch film cling layers, HRDF-750 is not a direct substitute for low-molecular-weight cling agents because its high molecular weight reduces immediate surface migration; if used, it is pre-compounded into a carrier concentrate at low addition levels. This formulation constraint is an operational boundary, not a defect: the grade is intended for applications requiring retention under load rather than rapid exudation to a surface.