| HS Code | 718279 |
| Appearance | Colorless to light yellow transparent viscous liquid |
| Molecularweightmn | ≈650 g/mol |
| Densityat20c | ≈0.89 g/cm³ |
| Kinematicviscosityat100c | ≈8–12 mm²/s |
| Flashpoint | ≥180 °C |
| Colorptco | ≤50 |
| Volatilematter | ≤0.5% |
| Watercontent | ≤0.05% |
| Acidvalue | ≤0.1 mg KOH/g |
| Ashcontent | ≤0.02% |
| Chlorinecontent | ≤0.01% |
| Alphaolefincontent | ≥70% |
| Solubilityinwater | Insoluble |
| Solubilityinaliphatichydrocarbons | Soluble |
As an accredited Polyisobutylene HRDF-650 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Polyisobutylene HRDF-650 is supplied in 200 kg steel drums, palletized and securely sealed for industrial transport. |
| Container Loading (20′ FCL) | Polyisobutylene HRDF-650 is floor-loaded into a 20′ FCL container with protective lining, secured, sealed, and documented for safe transport. |
| Shipping | Polyisobutylene HRDF-650 is typically shipped in sealed drums or IBCs under ambient conditions. Protect from moisture, excessive heat, and contamination; secure packaging to prevent leakage. Use standard freight and comply with local transport regulations, shipping documentation, and the current SDS. |
| Storage | Store Polyisobutylene HRDF-650 in original, tightly closed containers in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and strong oxidizers. Protect from moisture, contamination, and extreme temperatures. Keep containers clean, labeled, and properly sealed; follow the SDS and local regulations. Avoid prolonged storage near ignition sources. |
| Shelf Life | Shelf life: 24 months when stored in original unopened containers under cool, dry conditions away from direct sunlight. |
Within the lubricant additive value chain, HRDF-650 is first converted to polyisobutenylsuccinic anhydride through a thermal ene reaction with maleic anhydride. The terminal vinylidene content of the starting polyisobutylene is the critical quality parameter; HRDF-650 is typically released with vinylidene functionality above 70% by ¹H NMR, which permits grafting efficiencies close to one succinic anhydride unit per chain. Maleation is run in a 316L stainless steel batch reactor with an anchor agitator, external hot-oil heating, a nitrogen sparge below the liquid surface, and an overhead reflux condenser. A typical charge molar ratio is 1.15–1.40 mol maleic anhydride per mole of HRDF-650, with the reaction mass held at 195–215°C for 18–26 h. The process window is narrow: below 195°C conversion slows to impractically long residence times, while sustained operation above 225°C accelerates vinylidene isomerization and tar formation, producing color bodies measurable as an increase in ASTM D1500 color beyond 2.5. Unconsumed maleic anhydride is removed by vacuum stripping at 12–18 kPa absolute and 150–160°C, after which acid value titration by ASTM D664 is used to confirm maleation extent. The resulting PIBSA intermediate is the principal building block for ashless succinimide dispersants used in passenger car and heavy-duty diesel crankcase additives. It is transported as a viscous liquid with viscosity reported by ASTM D445; nitrogen blanketing during storage prevents hydrolytic ring opening. Compliance obligations include EU REACH registration for the polyisobutylene starting material and downstream product notification where the anhydride intermediate is not isolated.
Boronated succinimide dispersants derived from HRDF-650 are manufactured in two stages after PIBSA formation. The PIBSA intermediate is condensed with a polyethyleneamine mixture—commonly triethylenetetramine, tetraethylenepentamine, or a commercial heavy polyamine—at a molar ratio of 0.45–0.55 mol amine per mole of PIBSA. The condensation is run under vacuum at 140–160°C for 4–6 h, with water of reaction removed through a condensate trap. The exotherm during the early amine-addition phase is controlled by keeping the jacket at 90–110°C until the initial temperature spike subsides; failure to stage the amine feed can create localized gel particles that are detectable as filter plugging during final filtration through 10 μm cartridge filters. Boron post-treatment with boric acid is then applied to raise thermal stability and control sludge handling. The boric acid charge is commonly limited to 0.5–1.2 wt% boron in the final dispersant because higher boron content drives total base number measured by ASTM D2896 upward beyond the additive package rebalancing window and can increase copper corrosion measured by ASTM D130 in finished lubricant formulations. The finished dispersant is diluted to 40–50 wt% active content in process oil for storage, and its kinematic viscosity at 100°C is monitored by ASTM D445 to preserve pumpability in additive blending plants. Typical finished oil treat rates are 3–7 wt% for passenger car motor oil and 7–12 wt% for heavy-duty diesel engine oil, depending on the base oil group and soot-handling target.
Gasoline deposit control packages based on HRDF-650 enter formulation as a succinimide-amide intermediate with a lower amine stoichiometry than crankcase dispersants. The molecular weight of the HRDF-650 chain is selected to provide enough nonpolar anchoring to dissolve in the gasoline delivery system while keeping the additive thermally unstable residue below intake valve deposit limits. The condensation step is stopped at an amine-to-PIBSA molar ratio of 0.35–0.45, and the product is stripped under vacuum at 150–170°C to remove free amine. The active deposit control additive is handled as a concentrated solution at 50–60 wt% in an aromatic solvent such as Aromatic 150, then metered into finished gasoline at 80–180 ppm by mass active. Deposit performance is evaluated by the intake valve deposit test specified in ASTM D6201 and the port fuel injector fouling test specified in ASTM D5598. The additive is designed to be ash-free; therefore sodium, potassium, and calcium are controlled below 5 mg/kg by inductively coupled plasma analysis to avoid combustion chamber deposit precursors. Storage tanks require dry nitrogen pads because the imide intermediate can absorb moisture and hydrolyze to a free acid-amine species that destabilizes the concentrate. Batch-to-batch variation in the degree of amidation is tracked by total base number according to ASTM D2896, with a common release window of 25–45 mg KOH/g for the diluted concentrate.
In oilfield paraffin-control packages for crude oils with asphaltene content above 2.0 wt%, HRDF-650 is converted into a low-molecular-weight ester or amide derivative that acts as a wax crystal modifier and emulsion breaker. The synthesis route for this application is partial esterification with polyethylene glycol having a molecular weight of 400–600 g/mol, catalyzed by 0.15–0.30 wt% p-toluenesulfonic acid under xylene reflux at 140–150°C. Water is removed azeotropically, and the acid value is reduced to below 5 mg KOH/g by ASTM D974 before the solvent is removed under vacuum at 80–100°C. The resulting polyisobutenyl succinate ester is dosed into production chemicals at 5–30 ppm based on field trials, where it interferes with the ordered packing of long-chain paraffin crystals and reduces pour point when measured by ASTM D97. The product is typically blended with alkylphenol-formaldehyde resins and heavy aromatic solvent to make a winterized paraffin dispersant for offshore flow lines. Viscosity at 40°C is monitored by ASTM D445 to ensure injectability through capillary chemical injection lines. Compatibility with high-asphaltene crudes is evaluated by bottle tests using ASTM D4007, with water drop and interface quality recorded at 60°C. The operational boundary is defined by the pour point of the neat product; below 0°C, the concentrate must be stored in heated or trace-lined tanks to maintain transfer viscosity.
Metalworking fluid concentrates formulated with polyisobutenyl succinate esters use HRDF-650 as the hydrophobic segment that stabilizes water-in-oil emulsions during the cutting operation. The PIBSA intermediate is esterified with trimethylolpropane or pentaerythritol at a polyol-to-anhydride ratio of 1.2–1.5 mol/mol, with 0.10–0.20 wt% dibutyltin oxide or p-toluenesulfonic acid as catalyst. The esterification is run at 180–210°C under 30–50 mbar vacuum with nitrogen sparging to strip water. The acid value is driven to 3.5–5.0 mg KOH/g by ASTM D974, which reduces free acid that would otherwise soften the emulsion and increase rust potential. The ester is incorporated into soluble oil concentrates at 10–25 wt%, together with naphthenic base oil, corrosion inhibitors, and alkanolamine pH buffers. The final metalworking fluid is diluted with water at 1:20 by volume before use. Emulsion stability is evaluated according to DIN 51367, and corrosion protection is tested by the chip/filter paper method in DIN 51360-2. The operating pH window of 9.0–9.5 is maintained by the alkanolamine buffer; outside this window the ester hydrolyzes progressively, increasing acid value and reducing emulsion droplet size. Stainless steel mixing tanks with high-shear dispersion blades are used to pre-emulsify the concentrate, and the final batch is filtered through 25 μm bag filters to remove gel particles.
Packaging hot-melt formulations that require extended open time blend HRDF-650 at 5–15 phr into metallocene polyolefin elastomer or ethylene-vinyl acetate systems. The addition takes place in a twin-screw extruder with an L/D 40:1 barrel configuration and zone temperatures set between 150°C and 175°C. Screw speed is adjusted to maintain a residence time of 35–60 seconds, and the melt is pelletized underwater to prevent agglomeration. The plasticising effect is tracked by Brookfield viscosity at 180°C using ASTM D3236; typical release targets range from 1500–4500 mPa·s, depending on the base polymer and tackifier level. Loop tack and peel adhesion are measured according to PSTC-16 and PSTC-101 after coating onto 36 μm polyester film. A processing constraint is the low flash point of residual volatile oligomers; devolatilization is not used in hot-melt compounding, so the HRDF-650 batch must be low in volatile content below 0.2 wt% as measured by ASTM D1160 distillation. For indirect food-contact packaging adhesives, the formulated adhesive component must meet the applicable requirements of 21 CFR 175.105 when the polyisobutylene grade is listed in the relevant regulatory inventory. Performance limitations include reduced heat resistance and potential migration into low-polarity substrates; therefore the HRDF-650 content is capped below 15 phr in carton-sealing adhesives where cold flow would otherwise cause bond failure at 55°C.
For butyl rubber damping compounds used in engine mounts and bridge bearing pads, the addition of HRDF-650 at 8–15 phr reduces compound Mooney viscosity by 10–25 Mooney units when measured by ASTM D1646 at 125°C. Mixing is performed in an internal mixer with a fill factor of 0.70–0.75 and a starting temperature of 60–80°C, followed by a two-roll mill at 40–50°C for sulfur or resin curative addition. The low molecular weight of HRDF-650 influences the tan δ peak and broadens the damping response in dynamic mechanical analysis conducted under ASTM D5992. Vulcanizate hardness measured by ISO 48-4 decreases by approximately 4–8 IRHD relative to a non-plasticized control, while tensile strength is monitored by ASTM D412 to ensure the compound retains structural integrity. The plasticizer migrates slowly in thick sections; published data for this specific configuration in large bearing pads is limited, so aging behavior must be verified by a 70°C air-oven test for 168 h according to ISO 188. Because HRDF-650 contains residual double bonds, it participates in sulfur vulcanization to a limited extent and can consume a small portion of the cure package. The compounding window is therefore narrow: below 8 phr viscosity reduction is insufficient for transfer molding, while above 15 phr tensile retention and compression set measured by ASTM D395 method B degrade rapidly.
| Application route | Primary test method | Typical monitored parameter |
|---|---|---|
| PIBSA maleation | ASTM D664 | Acid value for maleation extent |
| Succinimide dispersant | ASTM D445, ASTM D2896 | Kinematic viscosity, total base number |
| Fuel deposit control additive | ASTM D6201, ASTM D5598 | Intake valve deposit mass, injector fouling |
| Oilfield paraffin dispersant | ASTM D97, ASTM D4007 | Pour point, water drop time |
| Metalworking fluid emulsifier | DIN 51367, DIN 51360-2 | Emulsion stability, corrosion protection |
| Hot-melt adhesive plasticiser | ASTM D3236 | Brookfield viscosity at 180°C |
| Butyl rubber damping modifier | ASTM D1646, ASTM D5992 | Mooney viscosity, tan δ damping response |
Competitive Polyisobutylene HRDF-650 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@alchemist-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@alchemist-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Polyisobutylene HRDF-650 is a high-molecular-weight homopolymer obtained by cationic vinyl-addition polymerization of isobutylene at process temperatures below −80 °C. The HRDF-650 designation is supplier-managed, and the numeric suffix is interpreted as a target molecular-weight class rather than a measured property. Because the saturated main chain contains no unsaturation, the polymer does not respond to sulfur-based cure packages and follows a different thermo-oxidative degradation pathway from isobutylene-isoprene copolymers. The grade is supplied in solid bale form for compounding operations; for adhesive and sealant applications it is usually reverse-melted or dispersed into hydrocarbon solvents or plasticizing oils before formulation.
For specification work, the class is bracketed by density, limiting viscosity number, Mooney viscosity, ash, volatile matter, and stabilizer content. A representative high-molecular-weight polyisobutylene in this nominal range shows density of 0.91–0.92 g/cm³ when tested in accordance with ISO 1183-1, ash content below 0.1 wt% by ISO 3451-1, and volatile loss below 0.3 wt% by ISO 3251. Glass transition temperature is near −65 °C by differential scanning calorimetry according to ISO 11357-2. Published data specific to HRDF-650 are limited; the surrounding homopolymer class provides the boundary, while the supplier certificate of analysis remains the controlling document.
Differences from other polyisobutylene grades and related elastomers are best defined by the role the molecular weight plays after formulation. The comparison below is class-level; HRDF-650-specific values appear only on the lot certificate.
| Material class | Sulfur cure | Physical form | Typical molecular-weight class | Glass transition | Primary function |
|---|---|---|---|---|---|
| Low-Mv liquid PIB | No | Viscous liquid | 40,000–400,000 g/mol | −60 to −65 °C | Plasticizer, tackifier diluent |
| HRDF-650 class | No | Solid bale | 6.0–6.5 × 10⁵ g/mol target | −65 °C | Elastomeric backbone |
| Butyl rubber | Yes | Solid bale | 300,000–500,000 g/mol | −67 °C | Vulcanizable rubber |
| Bromobutyl | Yes | Solid bale | 400,000–600,000 g/mol | −66 °C | Vulcanizable rubber, low permeability |
Receiving specifications for HRDF-650 target process-critical variables: elastic response under shear, molecular-weight integrity, and low inorganic contamination. An incoming lot is not released solely on visual appearance; it moves to quarantine pending a certificate that reports lot-specific values for the following properties. Where a generic public specification is unavailable, the acceptance basis is the supplier-managed target band.
The Mooney viscosity value is not a complete descriptor of processing behavior because high-molecular-weight polyisobutylene is strongly non-Newtonian and does not show the same pseudoplastic response as EPDM or butyl rubber at equivalent Mooney values. A lot at the upper end of the target range may require longer incorporation time in a low-shear kneader, while a lot at the lower end may produce lower die swell and reduced cohesiveness in pressure-sensitive adhesive films. Manufacturing checks therefore compare the lot value not only against the specification limit but also against the running excipient range for the specific adhesive or sealant formulation.
Limiting viscosity number in toluene at 30 °C derives from the Mark-Houwink-Sakurada relation. For high-molecular-weight polyisobutylene, the exponent a is typically between 0.60 and 0.70, so a small shift in intrinsic viscosity corresponds to a large shift in Mv. A certificate that reports a 10% variation in limiting viscosity number determined by ISO 1628-1 can therefore alter the elastic response of the formulated adhesive more than a similar variation in density. Incoming quality control compares both the viscosity and the lot-specific molecular-weight estimator rather than accepting one in isolation.
In compounding, HRDF-650 is processed in internal mixers, co-rotating twin-screw extruders, and two-roll mills. On a 50 mm co-rotating twin-screw extruder with an L/D ratio of 40:1, the critical constraint is thermal history. When barrel zones 6–9 exceed 160 °C, the polymer undergoes chain scission, evidenced by a drop in specific energy input, reduced melt pressure, and lower die swell. This failure mode differs from bromobutyl or EPDM, where excessive energy more commonly produces precure or gel formation. Because HRDF-650 is a saturated homopolymer, uncontrolled energy input degrades molecular weight rather than building crosslinks.
On a production two-roll mill with roll diameter 150 mm and friction ratio 1.2:1, band formation is stable when the front roll surface is held between 70 °C and 80 °C. Below 65 °C, the polymer loses compatible ribboning and can release from the slower roll; above 85 °C, the band becomes excessively tacky and may wrap to the faster roll. The use of a minimum roll gap of 0.5 mm during the first five passes improves dispersion of antioxidant masterbatches and lowers the incidence of undispersed white specks in calendered sheet.
In high-shear internal mixing, the addition sequence is the main lever for controlling heat. A typical sequence begins with a 70% fill factor, a rotor speed of 30–40 min⁻¹, and polymer addition before filler or plasticizer. Rotor speed is increased to 60 min⁻¹ only after the polymer forms a coherent flux. If the batch temperature approaches 150 °C, the ram is lifted and the rotor speed reduced; this is the processing boundary recommended for current stabilizer packages. Published data for HRDF-650 in continuous twin-screw lines are limited, but the generic high-Mv polyisobutylene envelope described here is consistent with manufacturer technical bulletins for similar grades.
Laboratory solution processing is a separate constraint. When HRDF-650 is dissolved at 20 wt% solids in a 60:40 cyclohexane–toluene solvent blend at 23 °C, the Brookfield viscosity at 10 min⁻¹ exceeds the measurable range of a conventional LV spindle and requires an HB or HR spindle. After film casting, residual solvent retention is determined by gas chromatography using ASTM D4526. Solvent retention above 0.5 wt% in pressure-sensitive adhesive films correlates with reduced shear adhesion and can create micro-blisters in laminated constructions. Drying tunnels are therefore configured to maintain web surface temperature below 90 °C during the constant-rate drying zone and below 120 °C in the final zone; higher temperatures accelerate surface skinning and trap solvent.
HRDF-650 differs from lower-molecular-weight liquid polyisobutylene in its effect on adhesive architecture. Liquid PIB grades with molecular weights below 100,000 g/mol function mainly as tackifying diluents and viscosity depressants. In contrast, HRDF-650 contributes elastic recovery and shear resistance; the same addition level of 10 wt% in a solvent-borne pressure-sensitive adhesive increases room-temperature shear adhesion failure time when measured according to ASTM D3654, but it also raises application viscosity. Formulators typically reduce the solvent content by 5–10 percentage points to maintain coatability.
Migration resistance is evaluated by peel adhesion and bleeding tests. In plasticized film formulations, low-molecular-weight species migrate to the substrate interface and reduce tack. The higher molecular-weight distribution of HRDF-650 reduces the concentration of migratory oligomers, but quantification requires oligomer extraction followed by gas chromatography rather than inference from viscosity alone. When the material is compounded with a tackifier at 60 parts per hundred resin, migration to polyethylene substrate is assessed after 7 days at 70 °C by comparing peel adhesion before and after aging using ASTM D3330.
The difference from butyl rubber is the absence of isoprene-derived unsaturation. Butyl rubber can be vulcanized with sulfur or quinoid systems; HRDF-650 cannot. In an uncured sealant, the homopolymer exhibits lower green strength because there is no crosslinked network. However, the saturated backbone provides a narrower thermo-oxidative degradation envelope; in circulating-air oven aging at 120 °C for 168 h per ISO 188, the retention of elongation in a calcium-carbonate-filled compound is more dependent on the antioxidant package than on the polymer microstructure.
Production-scale batch-to-batch variation in HRDF-650 tends to appear in three places: die swell, cold flow, and solution viscosity. In a hot-melt pressure-sensitive adhesive run on a 75 mm single-screw extruder, a shift in die swell of 5% changes coat weight by a measurable amount on the same gear pump setting. Cold flow is evaluated by creep compliance on a parallel-plate rheometer; a lot with lower viscosity-average molecular weight exhibits greater creep after 24 h at 25 °C. The manufacturer-recommended control is to retain a reference sample for each silo discharge and to compare new lots by small-angle oscillatory shear at 100 rad/s.
Brominated butyl and HRDF-650 are used in constrained-layer damping sheets because of high internal friction and gas impermeability, but the substitution is not drop-in. The saturated homopolymer has no allylic halogen sites, so cure systems based on zinc oxide and stearic acid are ineffective. The formulation must be redesigned around thermoplastic or pressure-sensitive adhesive behavior rather than vulcanization. Process adjustments include lower mixing temperatures, because bromobutyl tolerates a wider temperature range before scorching, whereas HRDF-650 degrades by chain scission and loses viscosity. On the same 40:1 L/D twin-screw line, the melt pump inlet pressure is more sensitive to screw speed; when screw speed rises from 250 min⁻¹ to 350 min⁻¹, the pressure drop across a 60/80 mesh screen pack increases by a larger factor than with bromobutyl, indicating higher elastic entry pressure loss. It is necessary to keep screen pack differential below 70 bar to avoid melt fracture at the die lip.
For a vibration-damping sheet formulation, adhesion to aluminum is validated by T-peel testing according to ASTM D1876; substitution is rejected if peel strength after 7 days at 70 °C falls below the lot-specific control limit. If the application is an insulating glass spacer sealant, the relevant performance requirement is moisture vapour transmission, tested according to ASTM F1249. Published data for HRDF-650 in this specific configuration is limited; a direct substitution trial should include a full factorial comparison with the incumbent bromobutyl grade using the same desiccant loading and extrusion line.
Typical applications are solvent-borne pressure-sensitive adhesives, adhesive transfer tapes, construction sealants, vibration damping sheets, and high-purity gum-base ingredients. In tape formulations, HRDF-650 is added at 5–20 wt% based on solids; loop tack is tested by ASTM D6195, peel adhesion by ASTM D3330, and shear adhesion failure temperature by ASTM D4498 if the system is hot-melt. In construction sealants, the polymer is compounded with polybutene, tackifier, filler, and anti-sag additives; slump is controlled to below 3 mm by ASTM D2202, and adhesion to concrete and glass is tested after 7 days at 23 °C and 50% RH. Published data for HRDF-650 in these exact formulations are limited; the applications are transferred from the known performance of high-molecular-weight polyisobutylene homopolymers.
Regulatory documentation for HRDF-650 is specific to the supplier and to the supplied physical form. Materials intended for repeated food-contact use are typically evaluated under the framework of FDA 21 CFR 177.1420, and the supplier letter should confirm the lot-specific status. Electrotechnical or consumer articles are assessed for restricted substances under RoHS 2011/65/EU; the analytical certificate reports lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE concentrations. REACH obligations follow EC 1907/2006.
| Regulation or standard | Scope | Typical documentation |
|---|---|---|
| FDA 21 CFR 177.1420 | Isobutylene polymers in rubber articles for repeated food-contact use | Supplier food-contact declaration |
| REACH 1907/2006 | Registration, evaluation, authorisation, restriction of substances | Safety data sheet, candidate list check |
| RoHS 2011/65/EU | Lead, mercury, cadmium, hexavalent chromium, PBB, PBDE | Analytical certificate |
| ASTM D1646-19 | Mooney viscosity of raw rubber | Lot test report |
| ISO 1183-1:2019 | Density of non-cellular plastics | Certificate of analysis |
| ISO 1628-1 | Limiting viscosity number of dilute polymer solution | Certificate of analysis |
Operational boundaries are specific to the formulated system. The polymer itself is hydrophobic, but compounded masterbatches containing hygroscopic fillers require filler pre-drying at 70 °C to moisture below 0.1 wt% when storage relative humidity exceeds 60%. Avoid storage near strong oxidizing agents. Do not combine with amine-based accelerators in an attempt to cure HRDF-650; they do not crosslink the saturated backbone and may exude as surface bloom. If photostability is required, formulate with 0.2–0.5 wt% of a polymeric hindered amine stabilizer and 0.2–0.5 wt% of a benzotriazole UV absorber, then validate weathering performance by ISO 4892-2. Any substitution into a production line should be preceded by a small-scale rheological comparison using the exact filler, plasticizer, and tackifier package, because the high-molecular-weight polyisobutylene class is more sensitive to shear heating than lower-molecular-weight plasticizing grades.