| HS Code | 982016 |
| Productname | Polyisobutylene HRDF-450 |
| Chemicalname | Polyisobutylene |
| Casnumber | 9003-27-4 |
| Numberaveragemolecularweight | 450 |
| Appearance | Colorless to light-yellow viscous liquid |
| Densityat20c | 0.88-0.90 g/cm3 |
| Kinematicviscosityat100c | 4.0-5.0 mm2/s |
| Flashpoint | ≥180 °C |
| Pourpoint | ≤-30 °C |
| Colorapha | ≤50 |
| Iodinevalue | 45-55 g I2/100 g |
| Alphaolefincontent | ≥75% |
| Volatilematter | ≤0.5% |
| Watercontent | ≤0.05% |
| Ashcontent | ≤0.01% |
As an accredited Polyisobutylene HRDF-450 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Polyisobutylene HRDF-450 is packaged in 25 kg net-weight moisture-resistant bags, securely palletized and stretch-wrapped for industrial shipment and storage. |
| Container Loading (20′ FCL) | Polyisobutylene HRDF-450 is packed and loaded in a 20-foot FCL container, properly secured for safe ocean shipment. |
| Shipping | Polyisobutylene HRDF-450 is typically shipped as a non-hazardous, viscous polymer in steel drums or IBCs. Containers should be kept closed, cool, dry, and protected from heat, moisture, and direct sunlight. Follow the SDS and applicable local transport regulations. |
| Storage | Store Polyisobutylene HRDF-450 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers tightly closed, properly labeled, and protected from moisture and contamination. Use secondary containment for spills, maintain good housekeeping, and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Recommended shelf life is 24 months from manufacture when stored in original, tightly sealed containers under cool, dry conditions. |
In fuel additive synthesis, HRDF-450 is not applied as a finished additive. It serves as the olefin backbone for polyisobutylene succinic anhydride, commonly referred to as PIBSA, which is the precursor for succinimide dispersants and quaternary ammonium detergent intermediates. The controlling structural parameter is the terminal vinylidene content. Under uncatalyzed thermal ene conditions, terminal vinylidene isomers react with maleic anhydride at a significantly higher rate than internal olefins. In a 2 m³ glass-lined or 316L stainless steel reactor, HRDF-450 is heated to 60–80°C under a nitrogen pad and transferred from a jacketed day tank. Maleic anhydride is added as a molten stream at 65–75°C. The feed ratio is maintained between 1.2:1 and 1.8:1 maleic anhydride to PIB on a molar basis. The reaction mixture is heated to 200–230°C and held until free maleic anhydride falls below 0.3 wt% by acid number or gas chromatography. The pressure is maintained at 0.10–0.15 MPa with nitrogen. Agitator speed is set between 20 rpm and 40 rpm for an anchor impeller in a 2 m³ vessel. A critical failure mode is wall temperature excursion above 245°C; this initiates radical coupling of the PIB chain and produces toluene-insoluble gel. The acid number of the PIBSA can be shifted from 0.8 mmol/g to 1.4 mmol/g by increasing the maleic anhydride to PIB molar ratio, but excess anhydride above 1.8:1 promotes color formation and requires longer stripping. Unreacted maleic anhydride is removed at 170–190°C under vacuum below 0.01 MPa. The stripped product is filtered through a 10 µm bag filter. Viscosity is tested by ISO 3104:2023 at 100°C. Saponification number is reported by ASTM D94-07(2023). Color is monitored according to ASTM D1500-23.
| Parameter | Lower bound | Upper bound | Method/equipment | Consequence outside window |
|---|---|---|---|---|
| Maleic anhydride/PIB molar ratio | 1.2:1 | 1.8:1 | Acid number titration, FTIR | Low conversion below; haze and color above |
| Reactor internal temperature | 200°C | 230°C | Calibrated thermocouple, ASTM E2877 | Incomplete ene reaction below; gel formation above |
| Hold time after anhydride addition | 6 h | 24 h | Periodic acid number sampling | Low vinylidene conversion; product darkening |
| Vacuum strip pressure | 0.005 MPa | 0.02 MPa | Pressure transmitter, vacuum pump | Residual maleic anhydride above 0.3 wt% |
| Filtration mesh | 5 µm | 25 µm | Bag filter housing | Gel carryover to downstream amidation |
Once the PIBSA intermediate from HRDF-450 is transferred to the amidation vessel, the process economics shift toward polyamine stoichiometry and vacuum profile control. The PIBSA is reacted with triethylenetetramine or heavy polyamine bottoms at a charge ratio between 0.4:1 and 0.8:1 amine to PIB chain. A lower ratio limits bis-succinimide formation and viscosity build, while a higher ratio leaves unreacted amine that can attack fluoroelastomer seals in downstream oil blending plants. The condensation is carried out at 140–170°C under staged vacuum from 0.08 MPa to 0.002 MPa. The vacuum is pulled in 3–5 steps to control foaming. The resulting alkenyl succinimide is diluted in Group I or Group II process oil to a nitrogen content of 0.35–0.5 wt% by ASTM D4629. Total base number is adjusted to 15–25 mg KOH/g by ASTM D2896-23. The dispersant thickening index is evaluated in a reference oil at 100°C by ASTM D445-24. A production-scale bottleneck is the narrow window between full imidization and color formation: at 200°C the product darkens beyond the ASTM D1500 limit of 2.0 within 1–2 h if vacuum is lost. In fuel detergent applications, the same PIBSA is amidated with a polyether amine at a molar ratio of 0.9:1 to 1.05:1; residual amine is then stripped or neutralized to avoid fuel filter plugging in direct-injection systems. Engine deposit control is evaluated by ASTM D6201-19 or a vehicle test aligned with CEC F-05-93 for intake valve cleanliness. Because HRDF-450 sits in the low molecular weight range, its dispersant chain contributes less viscosity to the finished lubricant, but the polar head group density must be raised to compensate for the shorter oleophilic tail. That trade-off is measured by comparing soot-thickening performance in a bench test such as ASTM D5967-23.
In insulating glass edge sealant and construction butyl tape formulations, HRDF-450 functions as a non-volatile plasticizer and tack regulator. It is compounded into a high molecular weight butyl rubber matrix together with polyisobutylene, carbon black, calcium carbonate, and silane adhesion promoters. The addition range is typically 5–25 phr. Below 5 phr, the kneader drive load can exceed the rated torque of a 500 L double-arm kneader, and the compound may not wet out the filler. Above 25 phr, the compound loses die-cutting integrity and slumps on vertical joints at 40°C. Mixing is performed in a sigma-blade or double-arm kneader at 100–130°C until the filler is wetted and the compound forms a cohesive mass; a typical mixing cycle is 45–90 min. Viscosity is measured by ISO 2555:2018 or by capillary rheometry at 100 s⁻¹. Compatibility is confirmed by thermal aging at 85°C for 14 days according to ISO 37:2017; a loss of tensile elongation greater than 30% relative to unaged material indicates plasticizer migration or volatile loss. The saturated backbone of HRDF-450 does not rely on antiozonant migration, so the sealant retains low-temperature flexibility according to ASTM D2137-22 for brittleness at -30°C. Adhesion to coated aluminum or glass is evaluated by ASTM C794-18 or EN 1279-4. Because the product is hydrophobic, moisture vapor transmission through the sealant is reduced in proportion to the polymer fraction; however, the cohesive strength of the butyl network controls the upper loading limit. In food-contact sealant applications, use is permitted only when the specific HRDF-450 grade is covered by a regional positive list; otherwise the sealant is restricted to structural glazing and non-contact construction applications.
On hot melt adhesive compounding lines running styrene-isoprene-styrene and styrene-butadiene-styrene triblock copolymers, HRDF-450 is introduced as a low-viscosity diluent and mid-block tackifying phase. The liquid feed is injected into a co-rotating twin-screw extruder with an L/D ratio of 25:1 to 40:1. Barrel zones are set from 120°C near the feed throat to 150–165°C at the die. In styrene-isoprene-styrene systems, the resin split between C5 tackifier and HRDF-450 is adjusted to keep melt viscosity below 15 Pa·s at 160°C while preserving loop tack. The recommended HRDF-450 addition falls between 10 wt% and 30 wt% of the formulation. Above 30 wt%, tensile strength declines below 0.5 MPa when measured by ASTM D638-14 on a 2 mm compression-molded sheet because the low molecular weight fraction dilutes the elastomer network. The open time at 130°C can be extended by 10–25 s when HRDF-450 replaces part of the C5 resin, depending on substrate heat loss. The finished adhesive is tested by ASTM D6195-23 for loop tack and by ASTM D3330/D3330M-23 for 180° peel against stainless steel. Moisture vapor transmission is measured by ASTM E96/E96M-23; the saturated backbone of HRDF-450 reduces water uptake, but the effect is lost if process temperatures exceed 200°C and initiate depolymerization. In-line filtration through a 100 µm screen before the coating head removes gel specks formed by thermal shearing. Because the neat liquid can form a combustible mist in the feed zone, extraction and zone classification follow IEC 60079-10-1:2024. The process boundary at the lower end is set by pumpability: if HRDF-450 is stored below 20°C, its viscosity may exceed the suction limit of the gear pump, requiring drum heating to 40–50°C.
Optical fiber and submarine copper cable flooding compounds use HRDF-450 as the base liquid when the specification requires a thixotropic water block that remains deformable at low temperature. The base fluid is compounded with fumed silica or SEBS as a thixotropic agent, plus microcrystalline wax and an antioxidant package. A production-scale formula typically comprises 70–85 wt% HRDF-450, 5–12 wt% thixotropic agent, and 1–5 wt% antioxidant. The mixture is processed under vacuum in a planetary mixer at 80–105°C; residual vacuum below 0.005 MPa is held for 30–60 min to remove entrained air. Water blocking performance is tested by IEC 60794-1-22:2025 or a cable water penetration rig applying 1 m water head for 72 h. Low-temperature slump is assessed by cone penetration at -40°C according to ASTM D217-23. The low glass transition temperature of HRDF-450 permits the compound to remain deformable after cable bending at cold installations, but high thixotropic agent loadings above 15 wt% can create a yield stress above 150 Pa, which impedes injection into the cable core. The flash point of the final compound is reported by ASTM D92-24 or ISO 2592:2017. A supplier may blend a higher molecular weight PIB to raise the flash point, but this increases low-temperature cone penetration and slows water-blocking speed. Batch records from filling lines show that gel viscosity decays under extended shear; therefore the compound is specified by a shear viscosity at 25°C and 10 s⁻¹ of 5–15 Pa·s prior to injection. A nitrogen blanket on the storage tank is recommended to prevent oxidative viscosity drift. The limiting operational boundary is oxygen exposure during high-temperature vacuum mixing; if the free surface is not blanketed, the final product may show a viscosity increase of more than 20% after 48 h storage at 60°C.
Paraffin wax and corrugated board coating operations use HRDF-450 as a flexibility modifier at loadings between 2 wt% and 10 wt%. Fully refined paraffin is heated to 80–95°C in a jacketed vessel; HRDF-450 is metered by gear pump and dispersed with a low-shear impeller for 20 min. The blend is applied by a curtain coater or roller applicator at 60–70°C. The addition of HRDF-450 broadens the paraffin melting peak and depresses the onset temperature by 1–3°C at 5 wt%, as measured by differential scanning calorimetry according to ASTM D4419-22. The coated board is tested for water vapor transmission by ASTM E96/E96M-23 and for blocking resistance at 40°C under a 3 kPa load for 24 h. A processing boundary occurs above 10 wt% because the surface becomes tacky and the coefficient of friction measured by ASTM D1894-24 exceeds 0.35, causing feed jams in carton erecting lines. Published data for HRDF-450 in paraffin modification is limited; the cited addition range derives from PIB grades of similar molecular weight and should be confirmed by pilot coating trials. In some sealing applications, the same blend is used as a moisture barrier on paperboard; the oxygen and water vapor transmission rates are inversely related to the paraffin coat weight and are not directly improved by HRDF-450 beyond the flexibility contribution.
Competitive Polyisobutylene HRDF-450 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@alchemist-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@alchemist-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Polyisobutylene HRDF-450 is a high-molecular-weight saturated aliphatic homopolymer produced by cationic polymerisation of isobutylene. The Chemical Abstracts Service registry number is 9003-27-4. In supplier documentation the suffix 450 is conventionally read as a nominal viscosity-average molecular weight near 450,000 g/mol, although this value is not assigned under an ISO nomenclature rule and must be confirmed by dilute-solution viscometry using ISO 1628-1 or an equivalent supplier procedure. The material is normally supplied in bale or slab form and is differentiated from low-molecular-weight polybutenes by its higher zero-shear viscosity, pronounced cold flow, and lower solubility in aliphatic hydrocarbons at equal temperature. Because HRDF-450 contains no deliberate unsaturation, it is outside the cure chemistry of isoprene-containing butyl rubber and does not respond to sulfur or quinoid vulcanisation systems. The fully saturated backbone contributes chemical inertness but also limits the options for covalent crosslinking; compound design must therefore rely on physical entanglement, tackifier interaction, or radiation-induced chain modification where a thermoset response is required.
The lot-release and characterisation matrix applicable to HRDF-450 is built around methods that separate molecular weight, contamination, and process consistency. The table below lists reference methods rather than fixed numerical limits because published certificate-of-analysis data for HRDF-450 remain supplier-controlled and lot-specific.
Table 1. Analytical methods used for polyisobutylene HRDF-450 lot certification
| Parameter | Reference method | Reported basis |
|---|---|---|
| Ash content | ISO 3451-1 | % mass |
| Volatile matter | ISO 3251 | % mass |
| Density | ISO 1183-1 | g/cm³ |
| Mooney viscosity | ISO 289-1 | Mooney units |
| Intrinsic viscosity | ISO 1628-1 | mL/g |
| Water content | ISO 15512 | mg/kg |
Mooney viscosity under ISO 289-1 is the most informative single-point processing indicator because it captures resistance to rotor shear at a defined temperature. Melt flow-rate testing under ISO 1133-1:2022 may have limited utility for HRDF-450 if the melt viscosity falls outside the practical range of the piston and die geometry; dynamic shear rheometry under ISO 6721-10 is preferred for capillary-flow and coating simulation. Procurement without an agreed internal specification is not recommended, and published data for this specific configuration are limited.
In high-shear compounding, pre-mastication of HRDF-450 with a portion of the plasticiser or process oil is required to reduce peak torque in batch mixers. On co-rotating twin-screw extruders with a length-to-diameter ratio of 40:1, filler side feeding after the polymer is fluxed prevents excessive motor draw and localised thermal degradation. Bale cutters or dicers are used because the material deforms plastically at room temperature. Production-scale observations for similar high-molecular-weight PIB grades indicate that filler addition at oil-extended PIB temperatures below 120 °C can generate un-dispersed agglomerates; thermocouple placement at the feed throat and mid-barrel zones is therefore used to confirm thermal homogeneity before filler incorporation.
The molecular weight distribution of HRDF-450 controls the balance between surface wetting and cohesive failure resistance. Higher molar mass fractions increase zero-shear viscosity and slow chain interdiffusion across adhesive interfaces; lower molar mass fractions can plasticise the matrix and reduce plateau modulus. Peel performance is assessed under ASTM D903-98(2017) or FINAT FTM 1 loop tack, while cohesive strength is measured through static shear holding power under ASTM D3654. Adhesive performance cannot be inferred from molecular weight alone; tackifier compatibility, resin loading, coating thickness, and substrate roughness shift the failure mode.
A saturated PIB backbone has limited specific interactions with polar additives. Hydrocarbon tackifier compatibility is normally evaluated by cloud-point observation or differential scanning calorimetry under ISO 11357-2 to detect phase separation. Because HRDF-450 has no measurable gel content, its green strength in sealants can be lower than that of vulcanisable butyl-based systems. The absence of sulfur crosslink density contribution is an operational boundary that must be considered during equipment and formulation design.
Relative to polybutenes with number-average molecular weights below 5,000 g/mol, HRDF-450 functions less as a plasticiser or viscosity modifier and more as a high-molecular-weight elastomeric base. The substitution of a low-molecular-weight polybutene by HRDF-450 raises melt viscosity and shortens wet-out time unless processing temperature is increased. The grade change is therefore not a direct viscosity swap; it alters the energy balance of the coating head and may require higher preheat capacity in slot-die applications. Published comparative peel and shear data for HRDF-450 against other commercial grades are limited; equivalent testing under identical resin and coating weights is required before line qualification.
Equipment modifications are necessary when substituting HRDF-450 into a line designed for fluid polybutenes. Storage and feeding move from heated tank systems to bale handling and dicers; drum melters are generally unsuitable because the polymer does not flow at room temperature. Pumping requires gear pumps with hardened wear surfaces and jacket temperatures above the softening point, with recirculation loops designed to avoid stagnant zones. In continuous sealant extrusion, head pressure and barrel temperature are monitored to prevent local shear heating above 160 °C, above which thermal-oxidative chain scission can reduce molecular weight and shift the molecular weight distribution downward.
Coextrusion with butyl-based edge tapes or polyolefin backings is possible when contact temperatures are controlled. Untreated polypropylene adhesion is typically low and must be confirmed by ASTM D903-98(2017) rather than inferred from surface energy. Where food-contact suitability is claimed, the finished article must meet the relevant migration limits and end-use restrictions in 21 CFR 177.1420 or Regulation (EU) 10/2011; no polymer datasheet claim replaces finished-article testing.
Unmodified HRDF-450 should not be exposed to strong oxidising agents, chlorine, or concentrated nitric acid. The polymer is insoluble in polar solvents such as methanol and acetone but swells in aliphatic, aromatic, and chlorinated solvents; this swelling is a handling constraint. Storage areas should be kept away from copper, copper alloys, and manganese salts where trace metal residues are not desired because transition metals can accelerate thermal-oxidative degradation of high-molecular-weight PIB. Bale surfaces can be dusted with a release agent such as stearate; if employed, ash testing under ISO 3451-1 should be re-validated to account for the surface additive. Cold flow limits bale stacking height and requires non-stick release liners at ambient temperatures. Published data for this specific configuration are limited; internal storage studies under actual warehouse conditions are preferred over generic guidance.