| HS Code | 380717 |
| Grade | HRDF-350 |
| Chemicalname | Polyisobutylene |
| Appearance | Colorless to light yellow transparent liquid |
| Numberaveragemolecularweight | 350 g/mol |
| Polydispersityindex | ≤1.8 |
| Densityat15c | 0.88-0.90 g/cm3 |
| Kinematicviscosityat100c | 20-50 mm2/s |
| Flashpoint | >150 °C |
| Pourpoint | < -30 °C |
| Colorapha | ≤50 |
| Terminalvinylidenecontent | ≥80% |
| Iodinevalue | 55-70 g I2/100 g |
| Watercontent | ≤0.05% |
| Volatilematter | ≤0.5% |
| Ashcontent | ≤0.01% |
| Acidvalue | ≤0.05 mg KOH/g |
As an accredited Polyisobutylene HRDF-350 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Polyisobutylene HRDF-350 is packaged in 25 kg net moisture-resistant bags, palletized and shrink-wrapped for safe industrial storage and transport. |
| Container Loading (20′ FCL) | Polyisobutylene HRDF-350 industrial chemical is loaded into a 20-foot FCL container, properly secured, labeled, and prepared for safe ocean shipment. |
| Shipping | Polyisobutylene HRDF-350 is not classified as dangerous goods for transport; no UN number, hazard class, or packing group applies. Ship in sealed drums or containers at ambient temperature, protecting from moisture, heat, direct sunlight, and contamination. Keep containers closed and label according to the supplier SDS and local regulations. |
| Storage | Store Polyisobutylene HRDF-350 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, ignition sources, and strong oxidizing agents. Keep containers tightly closed, clearly labeled, and protected from moisture and contamination. Use appropriate personal protective equipment when handling, and follow the manufacturer’s safety data sheet and local regulations for storage and spill control. |
| Shelf Life | Shelf life is typically 24 months when stored in a cool, dry, well-ventilated area in tightly closed containers. |
Competitive Polyisobutylene HRDF-350 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@alchemist-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@alchemist-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Polyisobutylene HRDF-350 is a low-molecular-weight, highly reactive polyisobutylene supplied as a clear, viscous liquid with a faint hydrocarbon odour. The product is registered under CAS 9003-27-4 and is produced by cationic polymerization of isobutylene followed by molecular-weight adjustment and terminal olefin isomerization. Manufacturer batch-release data for the HRDF series list terminal vinylidene content above 70 mol% by 1H NMR; conventional polybutene of similar number-average molecular weight typically contains less than 10 mol% vinylidene, with the balance distributed among trisubstituted and tetrasubstituted internal olefins. Number-average molecular weight is centred near 350 g mol⁻¹, and gel permeation chromatography with refractive index detection is used for molecular-weight distribution control. The suffix 350 denotes the nominal number-average molecular weight rather than a kinematic viscosity grade.
HRDF-350 is manufactured as a reactive intermediate rather than as a finished lubricant, fuel, or adhesive additive. The primary downstream conversion route is thermal ene reaction with maleic anhydride to yield polyisobutenyl succinic anhydride, which is then amidated with polyamines or esterified with polyols to form ashless dispersants, detergents, and corrosion inhibitors. Secondary evaluation routes include alkylation of phenols and aromatic amines, where narrow molecular-weight distribution and low halogen content reduce the formation of tar-like by-products. Published data for the product in high-solids polyisobutylene sealants is limited, and any such application requires a separate compatibility study.
The terminal vinylidene content is the controlling structural parameter. In conventional polybutene, the terminal carbon-carbon double bond is predominantly trisubstituted, and only a minor fraction of chains terminate in the vinylidene configuration. The vinylidene group in HRDF-350 is sterically accessible, allowing maleic anhydride to add through a thermal ene mechanism without chlorine or radical initiators. This structural difference reduces halogen carryover into the final polyisobutenyl succinic anhydride and lowers the corrosion burden in downstream lubricant additive packages. In addition, the high vinylidene content allows lower maleic anhydride excess and shorter hold time under otherwise comparable reactor conditions.
| Parameter | HRDF-350 | Conventional PIB Mn ≈350 | HR-PIB Mn ≈1300 |
|---|---|---|---|
| Terminal vinylidene content | >70 mol% | <10 mol% | >70 mol% |
| Trisubstituted olefin content | <5 mol% | 40–60 mol% | <5 mol% |
| Kinematic viscosity at 100 °C | 3–8 mm² s⁻¹ | 2–5 mm² s⁻¹ | 200–300 mm² s⁻¹ |
| Maleic anhydride feed ratio | 1.2:1–1.5:1 | 1.6:1–2.2:1 plus promoter | 1.3:1–1.6:1 |
| Chlorine content | ≤20 mg kg⁻¹ | 100–300 mg kg⁻¹ | ≤20 mg kg⁻¹ |
| Volatility at reaction temperature | Moderate; closed-loop venting required | Moderate; promoter handling required | Low; high-viscosity transfer required |
The comparative profile explains why HRDF-350 is selected for low-molecular-weight dispersant synthesis. The low viscosity permits neat metering at moderate temperatures, while the high vinylidene content supports reduced maleic anhydride excess and faster conversion. The main trade-off relative to Mn ≈1300 HR-PIB is higher volatility, which requires closed-loop venting and nitrogen blanketing during storage and reactor charging.
Before charging, HRDF-350 should be stored in carbon steel or stainless-steel vessels under a nitrogen pad to limit oxygen ingress. Heating to 40–60 °C is normally required for low-shear transfer because ambient-temperature viscosity can exceed 10 mm² s⁻¹. In continuous metering, positive-displacement gear pumps with heated heads and mass-flow feedback are preferred over centrifugal pumps, which can exhibit slip losses when viscosity rises during cold-start conditions. Pre-drying at 60 °C and 10 kPa absolute pressure is advised if water content exceeds 100 mg/kg.
At reaction temperature, the primary conflict is between ene-reaction rate and double-bond isomerization. The rate of vinylidene consumption becomes practicable above 180 °C, while isomerization to less reactive internal olefins becomes measurable above 210 °C. In agitated vessels with poor heat transfer, local film temperatures can exceed the bulk temperature by 10–20 °C, creating a practical bulk setpoint ceiling of 215 °C. This processing window is narrower than that of conventional PIB, which is less sensitive because its reactivity is already constrained by low vinylidene content. On a pilot-scale batch reactor with jacket oil temperature controlled at 205 °C, the temperature difference between reactor wall and bulk liquid was maintained at 8–12 °C, and final polyisobutenyl succinic anhydride colour remained below Gardner 4 by ASTM D1544. When a faulty thermal regulator allowed wall temperature to reach 230 °C, the same formulation darkened to Gardner 7 and produced a gelatinous heel on the wall.
Continuous polyisobutenyl succinic anhydride production with HRDF-350 is performed in a jacketed stirred reactor equipped with an external recycle loop and a positive-displacement gear pump. The feed is preheated to 40–60 °C before mass-flow metering. Maleic anhydride is added as a molten stream at 60–70 °C, and the reaction mass is held at 180–220 °C under nitrogen. Industrial campaigns target a maleic anhydride to terminal vinylidene molar ratio of 1.2:1 to 1.5:1. Lower ratios reduce conversion and leave unreacted vinylidene that can oxidize during storage. Ratios above 1.8:1 increase residual free maleic anhydride, which must be stripped or neutralized before amidation. In a 10 L glass-lined steel reactor with pitched-blade turbine agitation at 80–120 min⁻¹, maleic anhydride addition is completed over 60–120 min to prevent localized temperature excursions above 230 °C. Exceeding that temperature causes double-bond migration and thermal oligomerization; the reaction mixture darkens and kinematic viscosity rises even though acid number may remain within specification.
Batch-to-batch variation in terminal vinylidene content of ±5 mol% has been observed in campaigns where isobutylene feed purity varied. The resulting polyisobutenyl succinic anhydride acid number, measured by ASTM D974, shifted by approximately 2–4 mg KOH/g. The ene reaction is therefore monitored by simultaneous acid number titration and FTIR disappearance of the vinylidene absorbance near 890 cm⁻¹, not by acid number alone. This dual monitoring prevents premature termination of a batch that appears in specification on total acidity but still contains unreacted terminal olefin.
The specification matrix below lists indicative control ranges for the HRDF series rather than contractual acceptance limits. Lot-specific certificates of analysis should be referenced for guaranteed values, test frequency, and current production-site methods.
| Property | Test method | Indicative range or limit |
|---|---|---|
| Kinematic viscosity at 100 °C | ASTM D445 | 3.0–8.0 mm² s⁻¹ |
| Density at 15.6 °C | ASTM D4052 | 0.82–0.86 g cm⁻³ |
| Flash point, Cleveland open cup | ASTM D92 | ≥110 °C |
| Water content | ASTM D6304 | ≤100 mg kg⁻¹ |
| Chlorine content | ASTM D5808 or XRF | ≤20 mg kg⁻¹ |
| Sulfur content | ASTM D5453 | ≤10 mg kg⁻¹ |
| Colour, APHA | ASTM D1209 | ≤50 |
| Acid number | ASTM D974 | ≤0.05 mg KOH g⁻¹ |
| Number-average molecular weight | GPC | 315–385 g mol⁻¹ |
| Terminal vinylidene content | 1H NMR | ≥70 mol% |
HRDF-350 should not be combined with free-radical initiators, strong oxidizing agents, or active copper alloys during storage. Oxygen exposure promotes peroxide formation that can initiate radical coupling and increase viscosity. Where water content exceeds 100 mg/kg, vacuum drying at 60 °C and 10 kPa absolute pressure is applied before maleic anhydride charging to avoid ring-opening to maleic acid. The product is not recommended for use with primary or secondary amines before the ene reaction because amine addition can form high-viscosity imides prematurely. Downstream regulatory status must be confirmed for each formulation; formulators seeking incidental food-contact status should verify the final lubricant package against 21 CFR 178.3570 or the relevant national measure. Base polymer compliance with REACH registration and safety data sheet obligations should be verified before shipment into the European Economic Area.