| HS Code | 592527 |
| Product Name | Polyisobutylene HRD-850 |
| Chemical Name | Polyisobutylene |
| Cas Number | 9003-27-4 |
| Molecular Weight Mn Typical | 850 g/mol |
| Density At 15 C Typical | 0.89 g/cm³ |
| Kinematic Viscosity At 100 C Typical | 180 cSt |
| Flash Point Typical | >180 °C |
| Pour Point Typical | -20 °C |
| Color Typical | APHA <50 |
| Acid Number Typical | <0.05 mg KOH/g |
| Water Content Typical | <0.05 wt% |
| Ash Content Typical | <0.02 wt% |
| Volatile Matter Typical | <1 wt% |
| Terminal Vinylidene Content Typical | >70% |
| Appearance | Clear, colorless to pale yellow viscous liquid |
| Solubility | Soluble in hydrocarbons; insoluble in water |
As an accredited Polyisobutylene HRD-850 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Polyisobutylene HRD-850 is supplied in 25 kg moisture-resistant, sealed bags, palletized for safe industrial storage and transport. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Polyisobutylene HRD-850 is palletized, shrink-wrapped, and securely loaded into a 20-foot FCL container for safe transport. |
| Shipping | Polyisobutylene HRD-850 is typically shipped as a non-hazardous industrial polymer and is not regulated as dangerous goods for transport. Use clean, closed steel drums or IBCs, protect from heat, moisture, and contamination, and store in a cool, dry, ventilated area away from oxidizers. |
| Storage | Store Polyisobutylene HRD-850 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers tightly closed, clearly labeled, and protected from moisture and contamination. Use appropriate secondary containment and follow the manufacturer’s SDS and local regulations. Avoid prolonged storage at elevated temperatures and inspect containers regularly for damage. |
| Shelf Life | Polyisobutylene HRD-850 typically has a 24-month shelf life when stored unopened in a cool, dry, well-ventilated area. |
Thermal maleation of Polyisobutylene HRD-850 proceeds as an ene reaction between the terminal vinylidene unit and molten maleic anhydride. The reactor is a closed, nitrogen-purged vessel with 316L wetted parts, a hot-oil jacket, and a pressure rating that keeps the anhydride in the liquid phase. The maleic anhydride to terminal double bond charge ratio is commonly set between 1.10 mol/mol and 1.35 mol/mol. Headspace pressure is maintained between 0.15 MPa and 0.35 MPa to suppress maleic anhydride sublimation. Reaction temperature is staged from 180 °C to 220 °C over 6 h to 24 h. The upper boundary is fixed by the onset of terminal double bond isomerization. Above 235 °C, vinylidene groups migrate to internal positions and become unreactive under thermal ene conditions. The resulting polyisobutenyl succinic anhydride is a viscous, amber intermediate. Acid number is measured after hydrolysis by ASTM D974 or ASTM D664. Vinylidene conversion is monitored by NMR or FTIR. The supplier certificate of analysis should report initial terminal vinylidene content because batch-to-batch variation in this value changes the maximum obtainable anhydride functionality. Free maleic anhydride is stripped under vacuum in a wiped-film evaporator at 150 °C to 170 °C. Residual free anhydride above 0.10 wt% interferes with downstream polyamine stoichiometry. Moisture above 0.05 wt% opens the anhydride ring and lowers acid number response. The thermal route is selected for HRD-850 when ashless intermediates are required because it avoids chlorine and metal residues. The main production conflict is fouling. Maleic anhydride sublimation deposits crystals in overhead lines if the partial condenser is not kept above the sublimation point. Agitator torque increases as conversion proceeds. A high-vinylidene batch may show a faster initial exotherm. Staged maleic anhydride addition and a tempered water circuit hold the reaction within ±5 °C of the target profile.
The reaction mass is held at the final temperature until the acid number plateaus. Sampling through a bottom valve is preferred because top-entry sampling can pull unmixed anhydride into the sample line. At high vinylidene content, the initial exotherm can exceed 20 °C above jacket temperature if the anhydride is charged too rapidly. Batch records from production-scale maleation show that the first hour of the exotherm is the period of greatest risk for runaway viscosity and localized hot spots. A recirculation loop with an external heat exchanger improves heat removal in vessels larger than 5 m³. The intermediate is then cooled to 100 °C before vacuum stripping. Attempts to strip free anhydride above 180 °C darken the product and accelerate thermal oxidation. A nitrogen sparge under the liquid surface improves maleic anhydride removal but can entrain low molecular weight polyisobutylene fragments in the overheads. This production trade-off determines the final acid number and odor profile of the PIBSA batch.
| Control point | Method | Batch release purpose |
|---|---|---|
| Vinylidene content before charge | ¹H NMR supplier CoA | Sets maleic anhydride charge ratio |
| Acid number after hydrolysis | ASTM D974 | Confirms anhydride formation |
| Free maleic anhydride | HPLC | Prevents downstream amine imbalance |
| Water content | ASTM D6304 | Prevents anhydride ring opening |
| Kinematic viscosity at 100 °C | ASTM D445 | Batch-to-batch consistency |
| Residual chlorine | ASTM D5384 | Chlorinated-route quality check |
When the HRD-850-derived PIBSA is converted to an ashless polyisobutenyl succinimide dispersant, the process constraint shifts from maleation conversion to amine/anhydride balance. The PIBSA is reacted with tetraethylenepentamine or a heavy polyamine mixture under vacuum at 140 °C to 165 °C. Water formed by imidization is removed through a vacuum receiver. The reaction is exothermic early in the temperature ramp. Batch viscosity rises as polyamide and succinimide chains form. Gelation occurs when the primary amine charge is too low relative to anhydride equivalents. The ratio of primary amine to succinic anhydride is usually held above 1.0 eq/eq to avoid crosslinked gel. The endpoint is determined by total base number, residual acid number, and vacuum dehydration.
The finished dispersant is evaluated as a concentrate in a Group II 100N oil. Physical-chemical tests include ASTM D2896 for total base number, ASTM D445 for kinematic viscosity at 100 °C, ASTM D5800 for NOACK volatility, and ASTM D874 for sulfated ash. The sum of these results does not predict engine wear or deposit performance. Engine sequence tests and bench tests are required for finished oil qualification. In heavy-duty diesel formulations, the dispersant concentrate is typically blended from 2 wt% to 8 wt% into the finished additive package. The exact treat rate depends on the dispersant nitrogen content and the piston cleanliness target. A production-scale bottleneck is the viscosity rise during amidation. The vacuum pump and condenser must handle water and light amine vapors without backstreaming. Poor vacuum control produces a cloudy concentrate and increases free amine odor. The amidation reactor must be cleaned after each batch because a film of succinimide residue on the hot wall decomposes and darkens subsequent batches.
In production, the amidation reactor is usually a carbon steel or stainless vessel with a hot oil system and vacuum receiver. The polyamine is added below the liquid surface to minimize side reactions. The temperature ramp is held at 80 °C to 90 °C for the initial amine charge, then raised to 150 °C after gas evolution stops. The main field failure is amine carbonate formation from carbon dioxide ingress. This causes high viscosity and haze in the finished dispersant. Nitrogen covering is therefore required during storage of both polyamine and PIBSA. The second field failure is incomplete dehydration. Residual water in the dispersant concentrate above 0.10 wt% can hydrolyze the succinimide during storage and lower total base number. The batch is dried under vacuum until the water content meets the plant specification.
In chlorinated maleation, Polyisobutylene HRD-850 is first reacted with chlorine at 110 °C to 140 °C under a radical initiator. The chlorinated intermediate is then condensed with maleic anhydride at 140 °C to 180 °C. Hydrogen chloride is liberated continuously. The line must be built with acid-resistant scrubbers, and the reactor overhead must be maintained under slight vacuum. This route improves the anhydride-to-chain ratio for low-reactivity polyisobutylene grades. With HRD-850, the thermal ene route avoids organochlorine residue. If the chlorinated route is selected for conversion or cost reasons, residual chlorine in the PIBSA must be checked by ASTM D5384. Chlorine above specification causes corrosion in finished lubricants or fuel additive packages and interferes with elastomer compatibility. The process bottleneck on a production line is not the reactor but the HCl scrubbing system. Scrubber liquor disposal and gasket failure are the dominant maintenance causes. Published data for this specific HRD-850 configuration is limited. Batch trials are required to set the chlorine addition profile and initiator loading.
The scrubber system for hydrogen chloride must handle high gas flow during the first maleation phase. A packed column with caustic circulation is commonly used. The treated vent must meet local acid gas emission limits. Waste brine from the scrubber contains sodium chloride and sodium hypochlorite. Disposal through the wastewater treatment plant requires pH adjustment and redox control. Materials of construction downstream of the scrubbing tower should be acid-resistant polymer or rubber-lined steel. Standard carbon steel piping fails quickly in this service. These auxiliary systems add fixed cost and complicate batch scheduling. Consequently, chlorinated maleation of HRD-850 is normally reserved for cases where thermal maleation cannot reach the required succinic anhydride ratio.
The fuel additive route uses the same PIBSA intermediate but terminates it with amines or alkoxylated polyamines to make a deposit control component for gasoline or diesel. The key distinction from engine oil dispersants is the requirement for volatility and fuel solubility. High-molecular-weight material that remains in the combustion chamber can contribute to intake valve deposits. Formulators therefore select a narrow molecular weight cut and separate the polyamine-capped product. Engine testing follows ASTM D6201 for intake valve deposit formation in gasoline engines. The test result is not inferable from physical properties alone. Treat rate in finished fuel is determined by deposit test response. Published data for HRD-850-based fuel additives in this exact formulation is limited, but conventional PIB succinimide detergents are screened at active levels between 50 mg/kg and 400 mg/kg. Direct injection engines require higher thermal stability and reduced deposit formation at the injector tip. Additive packages may combine the HRD-850-derived succinimide with mineral oil carrier and a demulsifier. The final blend must remain clear at -20 °C and show no precipitate after storage. ASTM D445 viscosity at 40 °C is used for handling; ASTM D4052 density is used for blending calculations. Premature contact between the PIBSA intermediate and free amine generates heat and raises viscosity before the intended amidation step. Storage tanks and transfer lines for PIBSA must be purged of amine residues and kept under dry nitrogen.
Fuel additive evaluation starts with blend stability. The HRD-850-derived succinimide is dissolved in an aromatic or high-solvency carrier at 40 °C. The solution is then diluted into reference gasoline at active dose. Filterability is checked after cold soaking at 0 °C to 5 °C. Water tolerance is measured because fuel distribution systems contain dissolved water. An additive that emulsifies water will form persistent haze and may fail deposit control tests. For diesel fuel, end-use evaluations include injector nozzle coking on a bench engine and OEM-specific fouling cycles. The distinction between laboratory dispersancy and field deposit performance is significant. A dispersant can pass bench tests but increase combustion chamber deposits if the carrier and active component are not balanced. Published data for HRD-850 in this exact application is limited, so engine testing is the only reliable acceptance route.
For oilfield corrosion inhibitor and demulsifier intermediates, the terminal vinylidene content of HRD-850 determines the maximum obtainable succinic anhydride functionality per molecule. That functionality is converted to amide, imide, or ester derivatives for use as film-forming corrosion inhibitors in oilfield brines. The synthesis usually combines HRD-850-derived PIBSA with fatty acids, aminoethyl ethanolamine, or polyalkylene polyamines. The product is then diluted in heavy aromatic naphtha or an environmentally preferred solvent. Performance is evaluated by ASTM D665 for oil-phase rust prevention and by wheel tests where sour hydrocarbon phases are contacted with brine. Batch acceptance includes cloud point, pour point, and compatibility with calcium chloride brine. The key processing conflict is incomplete amidation. If the reaction is stopped too early, residual succinic anhydride hydrolyzes in the brine phase and produces acidic species that undermine the corrosion inhibitor film. The conversion endpoint is monitored by acid number and FTIR imide/amide bands. Published data for HRD-850 in specific oilfield corrosion inhibitor formulations is limited. The product is accepted as a building block rather than as a ready-to-dose field chemical.
Demulsifier derivatives from HRD-850 are made by introducing ethylene oxide or propylene oxide chains onto the PIBSA-derived intermediate. The alkoxylation step requires a high-pressure reactor capable of handling ethylene oxide. Safety instrumented systems for pressure, temperature, and oxygen ingress are mandatory. The resulting surfactant is evaluated by bottle tests that measure water drop-out rate and interface quality. Field trial data from produced-water systems show that molecular weight distribution influences demulsifier over-dose behavior. Published data for this specific HRD-850 derivative in demulsifier service is limited. The intermediate is therefore shipped with a specification for acid number and water content, and the formulator adjusts the alkoxylation ratio based on brine properties.
HRD-850-derived PIBSA can be esterified with pentaerythritol, sorbitan, or trimethylolpropane to produce emulsifier and extreme-pressure additive intermediates for metalworking fluids. The esterification is run at 160 °C to 190 °C with an acid catalyst and continuous water removal. The resulting ester is evaluated for acid number, hydroxyl value, and hydrolytic stability. In water-miscible fluids, the ester is neutralized with an alkanolamine and blended with mineral oil, corrosion inhibitors, and biocides. Emulsion stability is evaluated by ASTM D1479 where applicable. The final fluid must be tested under specific machining conditions because the ester derivative is a component, not a finished fluid. The short-chain ester can compete with the lubricant film at high shear. The formulation must be checked for pH drift, copper staining, and microbial growth. The esterification reactor must be vented because polyol dehydration produces water and light acidic vapors. Residual acid catalyst above specification will accelerate hydrolysis in the finished fluid. The operational boundary is moisture contamination during storage; open drums of PIBSA-derived esters should be blanketed with dry nitrogen to prevent acid number drift.
Emulsion stability in hard water is a critical field issue. The metalworking fluid is diluted with factory water containing calcium and magnesium salts. The HRD-850-derived ester must resist precipitation when the water hardness exceeds 300 mg/L as CaCO₃. Formulators use co-emulsifiers such as petroleum sulfonates and alcohol ethoxylates to maintain a stable macroemulsion. The ester itself is not corrosion-inhibiting until neutralized. The neutralization endpoint is set by pH; a target pH of 8.5 to 9.5 in the concentrate is common for ferrous machining. The finished coolant is monitored for total alkalinity, pH drift, and soluble oil concentration by refractometer. A batch that shows rapid oil separation in the ASTM D1479 test is rejected because tramp oil and filter blockage increase on the production floor.
Competitive Polyisobutylene HRD-850 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@alchemist-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@alchemist-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Polyisobutylene HRD-850 is a polyisobutylene product designation associated with the high-reactivity homopolymer class. The HRD prefix is consistent with grades in which terminal unsaturation is predominantly the vinylidene isomer, a structural feature that governs later functionalization reactivity. Because the designation alone does not fix lot-specific specification limits, the current certificate of analysis and technical data sheet are the controlling references. The grade is characterized by methods that include kinematic viscosity at 100°C under ISO 3104 or ASTM D445, density at 15°C under ISO 12185 or ASTM D4052, flash point by Cleveland open cup under ISO 2592 or ASTM D92, and water content by ASTM D6304 or coulometric Karl Fischer titration. In many polyisobutylene nomenclature systems, a suffix numeral such as 850 is assigned from a nominal kinematic viscosity at 100°C expressed in mm²/s. If that convention applies to HRD-850, the material is expected to lie in the high-viscosity region of the reactive polyisobutylene range; however, suffix conventions are not standardized across manufacturers, and numerical equivalence should not be assumed without a product data sheet.
The molecular weight distribution and terminal unsaturation are more relevant to functional performance than a nominal viscosity grade. High-reactive polyisobutylene is produced by cationic polymerization of isobutylene with a boron trifluoride-based initiator system; the resulting polymer carries a terminal vinylidene group in high proportion, commonly above 70 mol% as measured by proton nuclear magnetic resonance in comparative grades. Conventional low-reactivity polyisobutylene produced with aluminum chloride initiation contains terminal vinylidene levels below 10 mol%, with the remaining unsaturation distributed among internal or β-olefin isomers. Published data for HRD-850 specifically is limited; classification and intended reactivity should therefore be verified by terminal vinylidene analysis or by a standardized PIBSA conversion test when the material is routed to polyisobutylene succinic anhydride production.
The primary structural distinction is terminal vinylidene content, which controls thermal ene reaction kinetics with maleic anhydride. In high-reactive grades such as the class to which HRD-850 belongs, maleic anhydride grafting proceeds through a thermal ene pathway at temperatures typically between 190°C and 230°C in nitrogen-blanketed batch reactors. Conventional low-reactivity PIB, by contrast, contains mostly internal unsaturation and requires chlorine-assisted functionalization or harsher radical conditions to reach acceptable maleation yields. The absence of chlorine in high-reactive PIB maleation is a process difference, not merely a compositional one: it eliminates the corrosion load associated with chlorine-containing intermediates and reduces the formation of chlorinated by-products. Polybutene, which is a copolymer of isobutene and n-butenes with a lower average molecular weight and broader distribution, has a different unsaturation profile and lower thickening efficiency in lubricant formulations. Therefore, HRD-850 intended as a dispersant intermediate should not be treated as a drop-in equivalent to either conventional PIB or polybutene without verifying terminal vinylidene content and maleation yield.
| Attribute | Conventional PIB | High-reactive PIB class (HRD-850 class) | Polybutene |
| Terminal vinylidene content | <10 mol% | ≥70 mol% in class | variable, typically lower |
| Functionalization route to PIBSA | chlorine-assisted or radical | thermal ene | not typical |
| Chlorine introduced in process | yes in conventional maleation | no | no |
| Thickening contribution in lubricant | moderate | high | low |
| Application focus | sealants, adhesives, cable gels | lubricant and fuel additive intermediates | base stock modifiers, lower-viscosity sealants |
Specification assessment for HRD-850 should include viscosity-temperature behaviour rather than a single-point viscosity. A high-viscosity polyisobutylene grade with a nominal 100°C kinematic viscosity near 850 mm²/s would normally be handled at temperatures above its pour point; heating to 60–80°C is common for transfer but is not a specification limit. Flash point determined by Cleveland open cup for high-viscosity polyisobutylene grades of this molecular weight range generally exceeds 180°C. The exact flash point, volatility, and pour point of HRD-850 are lot-dependent and should be taken from the certificate of analysis. Gel permeation chromatography provides number-average and weight-average molecular weight values. For high-reactive polyisobutylene in the viscosity range associated with an 850 suffix, number-average molecular weight is commonly in the low thousands of daltons, but the calibration method should be recorded because polystyrene-equivalent and polyisobutylene-equivalent calibration can shift reported molecular weight by a significant margin.
Laboratory characterization of HRD-850 should distinguish terminal vinylidene from internal unsaturation because the two structures differ in thermal ene activity. Gel permeation chromatography with differential refractive index detection is used for molecular weight distribution; when available, triple detection with a viscometer and light-scattering detector reduces the uncertainty associated with polystyrene-equivalent calibration. The molecular weight distribution of high-reactive polyisobutylene can affect the maleation conversion at a given temperature, as low-molecular-weight fractions are consumed more readily in the ene reaction while high-molecular-weight fractions contribute to viscosity. Therefore, incoming inspection should not rely on a single bulk viscosity value alone.
Transfer and storage conditions affect the integrity of the terminal double bond. Because polyisobutylene undergoes oxidative chain scission at elevated temperature, prolonged heating above 200°C without antioxidant protection can reduce molecular weight and alter the terminal double bond distribution. Nitrogen blanketing or dry inert gas blanketing is specified for reactor charging. Water content is controlled because residual moisture can hydrolyze maleic anhydride to maleic acid in PIBSA preparation, lowering anhydride titre and shifting the acid number response under ASTM D664 or ISO 6619. Bulk storage should be at a temperature sufficient for pumpability but below the threshold at which thermal-oxidative degradation becomes measurable. For the class represented by HRD-850, storage under dry inert gas at 40–60°C is typical, but the exact recommended range is manufacturer-specific.
One process conflict occurs when the maleation reactor is charged with high-viscosity HRD-850 at temperatures below 130°C, because the high viscosity reduces mass transfer and creates stagnant regions near the vessel wall. If the reactor uses a conventional axial-flow impeller, local overheating can occur; helical ribbon or double-helix impellers are typical for reaction masses above 50 Pa·s. The terminal vinylidene group is thermally stable up to approximately 220°C, but prolonged residence beyond 240°C can isomerize the double bond and lower maleation yield. Therefore, reactor temperature control should be maintained within the specified ene reaction corridor; published data for HRD-850 specifically is limited.
HRD-850 is primarily evaluated in the synthesis of polyisobutylene succinic anhydride by reaction with maleic anhydride. The reaction is conducted in a stirred batch reactor with nitrogen sparging; maleic anhydride is charged at a molar ratio relative to terminal vinylidene, and the temperature is ramped to the ene reaction window. For high-terminal-vinylidene polyisobutylene, thermal grafting at 190–230°C proceeds without chlorine. The resulting PIBSA is then condensed with polyethylene polyamines such as tetraethylenepentamine or heavy polyamine bottoms to produce polyisobutylene succinimide dispersants used in lubricant packages. The reaction endpoints are monitored by acid number or saponification number according to ASTM D664 or ASTM D94. A high terminal vinylidene content is desirable because unconverted polyisobutylene remains in the final dispersant and contributes to viscosity without contributing to polar dispersancy performance. Therefore, HRD-850 should be benchmarked against other high-reactive PIB grades by maleation conversion and residual free PIB, not by viscosity alone.
Downstream use of HRD-850 is concentrated in lubricant and fuel additive intermediates, sealants, adhesives, and high-viscosity compatibilizing components. In lubricant dispersant synthesis, the grade functions as a hydrocarbon tail that confers oil solubility while the amine-derived head group provides soot and sludge suspension. In sealant and adhesive applications, polyisobutylene homopolymer of this class contributes high tack, low oxygen permeability, and resistance to moisture ingress; oxygen transmission can be tracked by ASTM D3985. Published data for HRD-850 in formulated downstream products is limited, and performance ranking should be verified by formulated bench tests such as viscosity index improvement, shear stability, and seal compatibility under the relevant OEM or industry specification.
Process differences accompany a switch from conventional PIB to HRD-850. The thermal ene route removes the requirement for chlorine gas or chlorine-containing reagents, but the reactor must still be designed for viscous reaction mass and efficient heat transfer. Agitated reactors with close-clearance impellers or recirculation loops are required because the reaction mixture remains viscous at temperatures below 100°C. For a nominal 850 mm²/s product, pump selection should account for high positive displacement pressure drop, and jacketed lines may be necessary to maintain flow. In comparison with lower-viscosity PIB grades, HRD-850 contributes greater thickening efficiency in the final lubricant package, but it also demands higher processing temperatures during transfer and filtration; published data for this specific configuration is limited. The absence of chlorine reduces corrosion risk in downstream wastewater and lowers the colour of the PIBSA intermediate; colour can be tracked by ASTM D1500 or Gardner ASTM D1544.
Compared with lower-suffix reactive polyisobutylene grades, HRD-850 provides a higher viscosity contribution per unit mass but may require dilution solvent to meet the kinematic viscosity targets of finished lubricant packages. The higher molecular weight tail can improve high-temperature high-shear viscosity retention, but it also increases the energy required for pumping and tightens the filtration window. A comparison should therefore be made on the basis of kinematic viscosity at 100°C, terminal vinylidene content, maleation conversion, and final dispersant viscosity rather than on product designation alone.
Operational boundaries include avoidance of open exposure to strong oxidizers and prolonged high-shear heating. Polyisobutylene is not intrinsically biodegradable and should be handled as a viscous hydrocarbon; disposal must follow local regulations. Regulatory inventory coverage for HRD-850 must be confirmed with the supplier under REACH, TSCA, and other regional chemical inventories. Users contemplating food-contact or pharmaceutical applications should not infer approval from the HRD-850 designation alone. Polyisobutylene grades may have specific food-contact listings under FDA 21 CFR 177.1420 for certain homopolymer compositions, but each supplier grade and migration limit must be documented separately.
| Property | Test method | Reporting basis |
| Kinematic viscosity at 100°C | ISO 3104 / ASTM D445 | mm²/s |
| Density at 15°C | ISO 12185 / ASTM D4052 | g/cm³ |
| Flash point, Cleveland open cup | ISO 2592 / ASTM D92 | °C |
| Water content | ASTM D6304 | mg/kg |
| Acid number | ASTM D664 / ISO 6619 | mg KOH/g |
| Ash content | ASTM D482 / ISO 6245 | % by mass |
| Colour | ASTM D1500 / ASTM D1544 | scale value |
| Terminal vinylidene content | ¹H NMR comparative class data | mol% |
Batch-to-batch variation in polyisobutylene of this class is typically observed in kinematic viscosity, terminal vinylidene content, and colour. The user should request statistical process control data from the supplier and align incoming inspection limits with the reactor's PIBSA conversion requirements. Because the product designation HRD-850 is not a specification, two shipments bearing the same designation may differ within the supplier's release range; the release range is the binding commercial specification. For operations where terminal vinylidene content below 70 mol% would reduce maleation yield, incoming ¹H NMR screening or a small-scale PIBSA conversion test is advised before bulk charging.