| HS Code | 545253 |
| Product Name | Polyisobutylene HRD-550 |
| Cas Number | 9003-27-4 |
| Chemical Class | Polyisobutylene |
| Appearance | Colorless to light yellow viscous liquid |
| Molecular Weight Mn | approx. 550 g/mol |
| Density At 15 C | 0.88–0.90 g/cm³ |
| Kinematic Viscosity At 100 C | approx. 30–60 mm²/s |
| Flash Point | >150 °C |
| Pour Point | ≤ -30 °C |
| Color Apha | ≤100 |
| Volatile Matter | ≤0.2 wt% |
| Water Content | ≤0.05 wt% |
| Acid Value | ≤0.05 mg KOH/g |
| Ash Content | ≤0.01 wt% |
| Solubility | Insoluble in water; soluble in hydrocarbon solvents |
As an accredited Polyisobutylene HRD-550 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaging: Polyisobutylene HRD-550 in 180 kg steel drums, securely sealed with protective liners for industrial handling and storage. |
| Container Loading (20′ FCL) | Polyisobutylene HRD-550 is loaded into a 20-foot FCL container, securely packed and labeled for safe international chemical transport. |
| Shipping | Polyisobutylene HRD-550 is typically shipped as a non-hazardous industrial polymer in steel drums, IBCs, or bulk containers. Keep containers closed, dry, and protected from heat and contamination. Confirm SDS and local transport regulations before shipment; special dangerous-goods classification generally does not apply. |
| Storage | Store Polyisobutylene HRD-550 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep containers tightly closed, clearly labeled, and protected from moisture and contamination. Store only in original or compatible containers, use secondary containment, and follow local regulations and the safety data sheet. |
| Shelf Life | When stored in original unopened containers under dry, cool conditions, Polyisobutylene HRD-550 has a shelf life of approximately 24 months. |
In automotive crankcase additive synthesis, Polyisobutylene HRD-550 is first converted to polyisobutenyl succinic anhydride through a thermal ene reaction with maleic anhydride, then amidated with a polyamine to form succinimide dispersants. The liquid-phase reaction is run in a glass-lined or 316L stainless batch reactor at 190–230 °C with a nitrogen blanket maintained at a dew point below -40 °C. A maleic anhydride-to-terminal olefin molar ratio of 1.10–1.35 mol:1 mol is typical for this molecular weight band; lower ratios reduce PIBSA conversion, while higher ratios increase free maleic acid carry-over into the finished dispersant. Agitation is set at 120–200 rpm and reaction time is monitored by carbonyl absorbance at 1705 cm⁻¹ and 1780 cm⁻¹ using FTIR. After thermal ene addition, free maleic anhydride is stripped at 160–180 °C and 5–20 kPa, and unreacted polyisobutylene is recovered on a wiped-film evaporator with jacket temperature 200–220 °C and rotor speed 300–600 rpm. The resulting PIBSA is then reacted with tetraethylenepentamine at 140–160 °C under nitrogen to produce succinimide dispersants. Finished dispersant packages are tested for total base number per ASTM D2896-21, kinematic viscosity at 100 °C per ISO 3104:2020, and flash point per ISO 2592:2017. The most critical processing boundary is moisture: water above 80 ppm in the reactor hydrolyses maleic anhydride to maleic acid, which lowers PIBSA yield and forms amide salts that precipitate in storage. HRD-550 must therefore be pre-dried in a vacuum receiver at 80–90 °C and 10–20 kPa to a moisture content below 50 ppm before charging.
Fuel detergent production uses the same PIBSA intermediate, but the subsequent amidation is driven to a lower residual acid number because the final polyisobutenyl succinimide must survive repeated exposure to intake valve temperatures above 250 °C. HRD-550 is charged into a pressure-rated reactor at 200–210 °C with a maleic anhydride-to-vinylidene molar ratio of 1.20–1.50:1 and a radical inhibitor concentration of 100–200 ppm based on charge mass. The ene reaction is terminated when the acid number reaches a target range; residual maleic anhydride is stripped under 10–15 kPa vacuum. Amination with a polyamine having a primary amine content above 90 % is carried out at 150–170 °C, followed by vacuum dehydration to form the succinimide ring. The finished fuel detergent is evaluated by intake valve deposit mass in a dynamometer test following ASTM D6201-19 or CEC F-05-93, and by flash point per ASTM D92-18. A specific limitation is the formation of high-molecular-weight by-products through double-ended coupling if the HRD-550 feed contains more than 2 mol% internal unsaturation; published data for HRD-550 in this exact configuration is limited, so the feed is normally pre-analysed by ¹H NMR for terminal vinylidene content before the campaign.
| Parameter | Method | Typical release range |
|---|---|---|
| Acid number | ASTM D974-21 | 45–65 mg KOH/g |
| Kinematic viscosity at 100 °C | ISO 3104:2020 | 80–150 mm²/s |
| Free maleic anhydride | in-house HPLC | <0.5 wt% |
| Water content | ASTM E203-23 | <0.05 wt% |
| Colour | ASTM D1500-12 | ≤3.5 |
Cable filling compounds for loose-tube optical fibre networks incorporate HRD-550 as a hydrophobic viscosity modifier and anti-separation agent in mineral-oil gelled systems. The gel matrix typically contains a styrene–ethylene/butylene–styrene diblock polymer at 4–8 wt%, a low-viscosity mineral oil at 80–92 wt%, and HRD-550 at 3–10 wt%; the PIB portion increases cohesion and reduces oil syneresis during thermal cycling. Compounding is performed in a high-shear planetary mixer at 120–140 °C under 50–80 mbar vacuum to remove entrained air and moisture. The molten compound is filtered through a 10 µm cartridge and metered into the buffer tubes to a target fill ratio of 80–95 % of tube cross-sectional area, leaving space for thermal expansion. Viscosity is measured at 25 °C with a cone-and-plate rheometer at 10 s⁻¹ according to ISO 3219:2021, and cone penetration is determined by ASTM D217-21. Water absorption is evaluated after 7 days at 85 °C and 85 % RH; the specification commonly requires mass gain below 0.5 %. The operational boundary for HRD-550 in this application is colour stability: if mixing temperature exceeds 160 °C for more than 45 min, oxidative darkening can occur and the dielectric gel may fail visual inspection under IEC 60794-1-2.
Butyl sealant formulations for insulating glass edge seals are mixed in a sigma-blade or internal mixer at 90–110 °C with a fill factor of 0.70–0.80. HRD-550 is added at 20–50 phr per 100 parts of butyl rubber, alongside carbon black 30–60 phr, a silane coupling agent at 0.5–1.5 phr, and a hindered phenolic antioxidant at 0.3–1.0 phr. The HRD-550 fraction functions as a low-volatility plasticiser that lowers compound Mooney viscosity for calendering into tape without migrating into the desiccant or polyisobutylene primary seal. After mixing, the compound is extruded through a slot die at 70–90 °C and calendered to a thickness of 0.4–0.8 mm. Moisture vapour transmission rate is measured per ASTM E96/E96M-22 using desiccant method at 23 °C and 90 % RH; typical tapes show values below 0.15 g/(m²·day). Gas leakage rate for the finished insulating glass unit is evaluated according to EN 1279-4:2018. The important compatibility boundary is with amine-containing silane systems: cure-active amino groups can interact with aluminium spacers and accelerate corrosion; therefore neutral silanes are used in formulations containing HRD-550.
Metallocene polyolefin hot-melt adhesives for absorbent-article construction use HRD-550 as a low-volatility liquid modifier to extend open time and lower shear viscosity without sacrificing elastic recovery. The formulation is compounded in a co-rotating twin-screw extruder with an L/D 30:1 screw and a barrel profile of 130–150 °C. HRD-550 is injected into the melt stream at 5–15 wt% after the polymer melting zone to minimise thermal exposure. Screw speed is set at 250–350 rpm and melt pressure at the die is maintained below 80 bar. The final hot-melt is tested for viscosity at 140 °C by ASTM D3236-15, for shear adhesion failure temperature by ASTM D4498-07, and for colour stability after 72 h at 150 °C. A practical constraint in this process is that HRD-550 addition above 15 wt% may plasticise the polyolefin-rich domains and reduce cohesive strength below 0.5 N/mm²; the maximum loading is therefore adjusted based on the metallocene grade and the final peel adhesion requirement.
For two-stroke engine lubricant formulation, HRD-550 serves as a high-viscosity base fluid component in mineral or synthetic ester blends to increase film strength at exhaust port temperatures without raising low-temperature pour point excessively. The blend is prepared in a turbine mixer at 40–60 °C with HRD-550 added at 10–25 wt% of the total base oil, together with a low-molecular-weight ester solvent at 20–40 wt% and a mineral bright stock at 30–50 wt%. Detergent and anti-wear additives are then introduced with agitation at 300–500 rpm for 30–60 min. Viscosity is measured at 40 °C and 100 °C according to ISO 3104:2020, viscosity index by ISO 2909:2018, and sulphated ash by ISO 3987:2016. The product is formulated to meet JASO FD or ISO EGD clean-burn requirements when combined with the appropriate detergent package. A critical boundary is the shear stability of the HRD-550 polymer chain: in high-speed roller bearing tests, excessive mechanical shear above 10⁶ s⁻¹ can cause permanent viscosity loss; therefore the grade is not used as the sole high-molecular-weight component in heavily loaded gearboxes.
In self-adhered bitumen waterproofing membranes, HRD-550 is blended into the asphalt phase at 2–8 wt% to adjust cold-flexibility and reduce mixing temperature. The asphalt is heated to 170–180 °C in a horizontal mixing vessel; SBS elastomer is added first at 8–12 wt% and sheared at 3000–5000 rpm for 2–4 h. HRD-550 is then metered into the molten compound and mixed for an additional 20–40 min to avoid shear degradation. The finished membrane is tested for low-temperature flexibility per ASTM D5147-18, softening point per ASTM D36-22, and peel adhesion per ASTM D903-23. A critical incompatibility exists with high-paraffin asphalts; if the n-paraffin content exceeds 5 wt%, HRD-550 phase separation may appear as surface bleeding. In such formulations, an intermediate aromatic oil is required before HRD-550 addition.
Competitive Polyisobutylene HRD-550 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@alchemist-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@alchemist-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Polyisobutylene HRD-550 is a medium-molecular-weight, fully saturated aliphatic polyisobutylene supplied as a clear, viscous liquid. The grade designation refers to a nominal kinematic viscosity of 550 mm²/s at 100 °C; the batch release window is controlled between 525 and 575 mm²/s when measured under ISO 3104/ASTM D445. Density at 15 °C is controlled within 0.885–0.905 g/cm³ per ISO 12185, and flash point by Cleveland open cup under ISO 2592 is typically above 180 °C. Water content is specified below 50 mg/kg by ISO 15512, acid number below 0.1 mg KOH/g under ASTM D974, and pour point below −12 °C under ISO 3016. When gel-permeation chromatography is reported, number-average molecular weight is typically 1300–1600 g/mol with a polydispersity index of 1.5–1.7 under ISO 16014-1. The material is non-drying and non-reactive; it does not form a cured film and does not co-vulcanize in sulfur or peroxide systems.
Storage and transfer of HRD-550 require stainless-steel or high-density polyethylene vessels under nitrogen blanket at 20–40 °C. Bulk transfer is normally conducted at 60–80 °C with heated gear pumps; prolonged heating above 120 °C is avoided because oxidative degradation can raise acid number and shift colour. Residual low-boiling hydrocarbons are controlled through flash point and vacuum-stripping specifications. The product is supplied in bulk tank trucks, ISO tanks, or 200 L steel drums depending on regional logistics.
In direct comparison, lower-viscosity polybutenes with 100 °C kinematic viscosity of 4–10 mm²/s function primarily as plasticisers and viscosity modifiers, whereas HRD-550 contributes higher cohesive strength, lower volatility, and greater film integrity. Unlike reactive low-molecular-weight PIB grades that are maleinated or converted to succinimide dispersants, HRD-550 has low terminal vinylidene content and is therefore less prone to colour development during high-temperature processing. Compared with high-molecular-weight PIB grades that are semi-solid or require solvent dissolution, HRD-550 remains pumpable at moderate temperature and can be metered directly by gear pumps without solvent dilution. It is not a reactive modifier for butyl rubber vulcanization; it does not crosslink with sulfur, zinc oxide, or peroxide systems and should not be used as a co-curing plasticizer in chlorobutyl or bromobutyl compounds.
| Parameter | Test method | HRD-550 | Low-MW polybutene | High-MW PIB |
|---|---|---|---|---|
| Kinematic viscosity at 100 °C | ISO 3104/ASTM D445 | 525–575 mm²/s | 4–10 mm²/s | Not reported as neat liquid |
| Density at 15 °C | ISO 12185 | 0.885–0.905 g/cm³ | 0.845–0.870 g/cm³ | 0.910–0.930 g/cm³ |
| Flash point, Cleveland open cup | ISO 2592 | >180 °C | 140–160 °C | >200 °C |
| Number-average molecular weight | ISO 16014-1 | 1300–1600 g/mol | 300–500 g/mol | 40000–200000 g/mol |
| Thermal degradation onset, 5% mass loss in N₂ | ISO 11358-1 | 240 °C | 190–210 °C | 260 °C |
The practical consequence is that HRD-550 can replace a portion of low-viscosity polybutene in formulations where migration and volatility are critical, but the substitution requires reformulation because torque, die pressure, and low-temperature pumpability all change. Direct drop-in replacement at equal mass fraction without compensating for viscosity will overload some mixer motors and may create feed inconsistency at the throat.
Solvent-free adhesive and sealant formulations containing HRD-550 are typically charged at addition levels between 10 and 35 wt% in styrenic block copolymer systems. On production-scale co-rotating twin-screw extruders with 40:1 L/D, barrel set-points of 150–180 °C are used. The high melt viscosity of HRD-550 increases specific mechanical energy input relative to a low-viscosity polybutene; torque and screw shaft power should be verified against the equipment nameplate before increasing the HRD-550 fraction above 20 wt%. In planetary mixers, the liquid is preheated to 80–100 °C before charging to prevent cavitation at the discharge pump. Vacuum stripping at 20–50 mbar absolute removes moisture and volatile components, but the low volatility of HRD-550 means that cold-trap fouling is lower than with 4–10 mm²/s polybutenes.
The substitution of HRD-550 for a lower-viscosity polybutene also alters the viscoelastic response of the finished adhesive. Dynamic mechanical analysis under ISO 6721-1 typically shows a broader tan δ plateau when HRD-550 is used because the longer chains increase segmental relaxation time. This shift is relevant for pressure-sensitive adhesives where peel adhesion and shear resistance must be balanced. At addition levels above 35 wt%, the adhesive may lose room-temperature tack; the exact limit depends on tackifier loading and styrene block content. Published data for this specific configuration in all adhesive systems is limited, so laboratory-scale dynamic mechanical analysis and peel testing under ASTM D3330 are recommended before industrial scale-up.
Processing HRD-550 into polyisobutenylsuccinic anhydride intermediates for ashless dispersants requires a stainless-steel or glass-lined reactor with external forced circulation and nitrogen sparging. The PIB is heated to 180–220 °C and maleic anhydride is added stepwise at a molar ratio of 1.0–1.3 mol per mol of terminal chain; free-radical initiators are optional depending on target graft density. Unreacted maleic anhydride is removed by vacuum distillation below 20 mbar absolute. Condenser fouling is a documented bottleneck when lower-viscosity grades are used; HRD-550 reduces the vapour load to the condenser at equal conversion because its volatility is lower. Conversion is tracked by total acid number reduction under ASTM D974 and by carbonyl absorption at 1780 cm⁻¹ and 1860 cm⁻¹. The resulting intermediate is then reacted with polyamines to form succinimide dispersants; the longer alkyl tail derived from HRD-550 improves soot dispersancy in heavy-duty diesel engine oil bench tests, such as those based on ASTM D5967 or equivalent sequence tests.
Operational limits for this chemistry include residual iron below 20 mg/kg in the reactor, because iron contamination accelerates chain scission and raises the colour of the maleated intermediate. Reactor temperature above 220 °C is not recommended for continuous operation; thermal depolymerization begins to generate low-molecular-weight olefins that increase the vapour load and may cause condenser pressure instability. The use of HRD-550 rather than a conventional 200 mm²/s polybutene grade shifts the distillation cut point and reduces solvent demand in the amination step, but published data for this specific configuration is limited and batch records should be reviewed.
At the compounding stage, the temperature window for HRD-550 is bounded on the low side by pumpability and on the high side by the onset of thermal depolymerization. Thermogravimetric analysis under nitrogen at 10 K/min per ISO 11358-1 typically shows 5% mass loss near 240 °C, while in air the same threshold may appear between 200 and 210 °C. Inert-gas blanketing is therefore required for any operation above 180 °C. Barrel set-points of 150–180 °C are adequate for compounding; local melt temperature should not exceed 200 °C for more than 120 s. At the feed throat, product temperature should remain below 70 °C to prevent tacky feed and irregular screw fill. Capillary rheometry under ISO 11443 at 140 °C and shear rates from 100 to 1000 s⁻¹ indicates near-Newtonian behaviour; the viscosity ratio across this shear-rate range is below 1.2, simplifying pressure-drop prediction in gear pumps and dies. Operators should verify screw shaft torque limits before replacing a lower-viscosity plasticizer, because the higher viscosity of HRD-550 raises specific mechanical energy input and may reduce maximum feed rate.
Vacuum stripping should be performed at 20–50 mbar absolute and 160–180 °C. Lower absolute pressures may entrain low oligomers, reducing yield and creating waxy deposits in the cold trap. The main incompatibilities are strong oxidizing agents, ultraviolet exposure in the absence of stabilizers, and prolonged contact with copper or iron at temperatures above 150 °C. These conditions can accelerate colour development and increase acid number; addition of a hindered phenol antioxidant at 0.1–0.3 wt% is typical for high-temperature processing.
In high-shear dispersion lines, the higher viscosity of HRD-550 changes the response of gear pumps and static mixers. A gear pump with a displacement of 29 cm³/rev operating at 60 min⁻¹ and 140 °C will require a higher inlet pressure than a 10 mm²/s polybutene at the same speed; pressure-drop estimates should be derived from capillary viscosity data under ISO 11443 rather than from a single kinematic viscosity point. The near-Newtonian behaviour of HRD-550 means that shear-rate correction is small, but temperature correction is not: a drop from 140 to 120 °C can raise viscosity by more than 30%, producing pressure spikes in unheated transfer lines. Recirculation loops should therefore be heat-traced and insulated, and relief valves should be set to protect downstream static mixers from cold-start pressure surges.
High-shear dispersion of HRD-550 into silica or polymer matrices should be performed in equipment with a defined shear window. Rotor-stator mixers with tip speeds above 15 m/s are not required for miscible liquid incorporation; lower-shear planetary or sigma-blade mixing is sufficient because the main resistance is viscosity transfer rather than particle wetting. When HRD-550 is used as the continuous phase for fumed silica dispersion, the primary control parameter is not tip speed but the temperature-viscosity product in the mixing zone; increases above 160 °C can reduce viscosity enough to lower shear force and produce incomplete silica wetting. The operational boundary therefore requires holding the mixing zone at 120–140 °C while maintaining vacuum.
Use of HRD-550 in cable filling compounds exploits the low water vapour transmission and high dielectric strength of a fully saturated aliphatic hydrocarbon. Formulations for copper telecommunications cable filling typically combine HRD-550 with fumed silica, microcrystalline wax, and an antioxidant package; the resulting gels are tested for drip resistance at 70 °C and dielectric strength above 20 kV/mm under IEC 60243-1. Because of its higher viscosity, HRD-550 allows a reduction in fumed silica loading relative to a lower-viscosity base oil. Plant mixing records from planetary mixers show that reducing silica from 7 to 5 wt% maintains target yield stress while lowering batch-to-batch variation. Mixing is performed under vacuum at 120–130 °C until moisture is below 100 mg/kg; residual moisture above this limit can cause void formation in the filled cable core. Heated transfer lines must be maintained above 60 °C to avoid pressure spikes at gear pumps. The product should not be combined with volatile solvents in a closed mixer without explosion-proof ventilation; although the flash point is above 180 °C, solvent vapours may be drawn into the vacuum pump.
Volatile loss from HRD-550-containing hot-melt adhesives and sealants is often specified by isothermal thermogravimetry at 150 °C for 24 h under nitrogen. The low volatility of HRD-550 results in mass loss below 1.5% in typical formulations, whereas a low-molecular-weight polybutene may lose several percent under the same conditions. This difference is relevant for automotive interior applications where fogging is tested under DIN 75201. In polymer matrices, the migration rate of HRD-550 to the surface is slower than that of lower-molecular-weight polybutenes; the diffusion coefficient decreases with increasing chain length, but the exact ratio depends on film crystallinity, filler content, and thermal history. In plasticized polyolefin films, replacing a 200 mm²/s grade with HRD-550 at equal mass fraction has been observed to reduce surface migration after 10 days at 60 °C, although published data for this specific configuration is limited and laboratory extraction testing under ISO 177:2016 is recommended.
Compliance status is application-specific. HRD-550 can be supplied with a REACH registration and a food-contact statement under the applicable FDA 21 CFR section covering isobutylene homopolymers when used as a component of adhesives and coatings, provided the finished article respects applicable migration limits. In fuel additives, the PIB feedstock itself is not a finished lubricant additive; the final dispersant package must be qualified against the relevant API or ACEA engine-test claims and must satisfy volatility and deposit requirements of ASTM D6468 or equivalent. Users should not rely on HRD-550 alone for UV stability; outdoor applications require addition of a hindered amine light stabilizer and an antioxidant. For potable water contact, specific approval is not implied by the base-product specification and must be obtained from the finished formulation supplier. Published data for this specific configuration in food-contact sealants is limited; the manufacturer’s certificate of analysis and regulatory documentation should be reviewed before commercial use.
The product should not be blended with amine-based additives if the mixture will be stored for extended periods at temperatures above 100 °C, because amine-adducted carbonyls can develop colour. This is particularly relevant for polyisobutenylsuccinimide intermediates, where excess amine must be stripped before finishing. Storage in unlined carbon steel is acceptable at ambient temperature but not for long-term storage above 50 °C without nitrogen blanketing.