Products

Polyisobutylene HRD-500

    • Product Name: Polyisobutylene HRD-500
    • Factroy Site: Yuanbaoshan District, Chifeng City, Inner Mongolia, P.R. China
    • Price Inquiry: sales8@alchemist-chem.com
    • Manufacturer: Inner Mongolia Eppen Biotech Co., Ltd.
    • CONTACT NOW
    VTB
    Specifications
    HS Code 835171
    Product Name Polyisobutylene HRD-500
    Chemical Name Polyisobutylene
    Cas Number 9003-27-4
    Molecular Weight Mn ≈500 g/mol
    Appearance Clear, bright, viscous liquid
    Color Astm D1500 ≤1.0
    Density At 15 C ≈0.89 g/cm³
    Kinematic Viscosity At 100 C ≈4.5–6.5 cSt
    Flash Point Coc ≥160 °C
    Pour Point ≤-30 °C
    Viscosity Index ≈90
    Bromine Number ≈32–38 g Br₂/100 g
    Acid Value ≤0.05 mg KOH/g
    Water Content ≤0.05 wt%
    Ash Content ≤0.01 wt%
    Chlorine Content ≤20 ppm

    As an accredited Polyisobutylene HRD-500 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Polyisobutylene HRD-500 is supplied in 25 kg net, polyethylene-lined fiber drums, palletized, clearly labeled, and sealed for industrial shipment.
    Container Loading (20′ FCL) 20′ FCL container loading for Polyisobutylene HRD-500: cargo securely stowed, labeled, and documented for safe export transport.
    Shipping Polyisobutylene HRD-500 is generally shipped as a non-hazardous solid polymer in sealed bags, drums, or boxes. Keep packaging dry and intact, away from heat, moisture, and strong oxidizers. Confirm classification with the current SDS and applicable transport regulations before shipment.
    Storage Store Polyisobutylene HRD-500 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep containers tightly closed and properly labeled; protect from moisture, dust, and physical damage. Maintain good housekeeping and follow local regulations. Avoid excessive temperatures to prevent degradation or softening. Use secondary containment where required and keep containers sealed when not in use.
    Shelf Life Polyisobutylene HRD-500 has a shelf life of approximately 24 months when stored in original, unopened containers under cool, dry conditions.
    Application of Polyisobutylene HRD-500

    How Does HRD-500’s Vinylidene Content Dictate Thermal Ene Reactor Throughput in Succinimide Dispersant Production?

    In polyisobutenyl succinic anhydride (PIBSA) synthesis, HRD-500 is charged into a stirred pressure reactor with maleic anhydride at a maleic anhydride-to-HRD-500 molar ratio of 1.05:1 to 1.30:1. The terminal vinylidene double bond, which is present in HRD-500 above 70 mol%, permits the thermal Alder-ene reaction to proceed between 200 °C and 230 °C; below 200 °C, conversion drops below 50% within a 6 h residence time, while above 230 °C maleic anhydride sublimation and oligomerization raise the intermediate colour beyond ASTM D1500 colour 5.0. Pre-drying of HRD-500 to a water content below 100 ppm is required before charging because moisture above 200 ppm hydrolyses maleic anhydride to maleic acid and reduces PIBSA acid number. Production-scale reactors use a nitrogen sparge of 0.2–0.4 m³/h per m³ liquid volume and a slight positive pressure of 0.2–0.5 barg to strip water and exclude oxygen. The resulting PIBSA intermediate is amidated with tetraethylenepentamine or a mixed ethyleneamine bottoms stream at a PIBSA-to-polyamine equivalent ratio of 1.0:0.45 to 1.0:0.55. Residual acid number after amidation is controlled to 70–120 mg KOH/g by potentiometric titration per ASTM D2896, and post-treatment with 0.2–1.0 wt% boric acid raises the total base number of the succinimide dispersant. In finished heavy-duty diesel engine oil, the HRD-500-derived dispersant typically comprises 1.5–4.5 wt% of the oil, corresponding to a PIBSA precursor input of 1–3 wt%. Compliance is evaluated against API 1509 Engine Oil Licensing and Certification System, ILSAC GF-6A, and REACH Regulation (EC) No 1907/2006 Annex XVII; finished-lubricant kinematic viscosity is measured by ASTM D445. Terminal products include API CK-4 and FA-4 heavy-duty diesel engine oils, low-ash natural gas engine oils, and marine trunk piston engine oils.

    Deposit control additives for gasoline and diesel fuel systems can be manufactured from HRD-500 through hydroformylation of the terminal vinylidene double bond followed by reductive amination with ammonia or a short-chain amine. The first stage is conducted in a high-pressure stirred autoclave at 160–200 °C and 150–200 bar synthesis gas using a rhodium-triphenylphosphine catalyst, converting HRD-500 into a polyisobutenyl alcohol mixture; conversion is monitored by loss of the vinylidene peak and iodine number decrease. The hydroformylated intermediate is then subjected to reductive amination over a fixed-bed nickel catalyst at 180–220 °C under excess hydrogen to yield polyisobutylene amine (PIBA). Treat rate in finished gasoline is 20–400 mg/kg of PIBA, with lower rates for maintenance dosing and higher rates for clean-up of existing injector deposits. Critical quality control responses are intake valve deposit weight by ASTM D6201 and electronic port fuel injector flow loss by ASTM D5598; additive packages must also comply with fuel additive registration requirements under EPA 40 CFR Part 79 and applicable regional fuel quality standards. Terminal products include port fuel injector detergents for gasoline, deposit control packages for diesel fuel systems, and aftermarket fuel system cleaner concentrates. Published data specific to HRD-500 in direct injection gasoline engines is limited; the above treat rates are derived from analogous low-Mn HR-PIB-based PIBA formulations.

    Downstream applicationPrimary compliance anchorCharacterisation standardsTerminal product classes
    Succinimide dispersant for engine oilAPI 1509, ILSAC GF-6AASTM D445, ASTM D2896, ASTM D1500HDEO, NGEO, marine trunk piston oil
    Fuel deposit control additiveEPA 40 CFR Part 79ASTM D6201, ASTM D5598Gasoline and diesel fuel detergents
    Hot-melt pressure-sensitive adhesiveFDA 21 CFR 175.105ASTM D6195, ASTM D3654Labels, tapes, hygiene adhesives
    Cable flooding and water-blocking gelRoHS 2011/65/EUASTM D217, IEC 60794-1-2Fibre optic gels, metallic cable floodants
    Butyl rubber processing aidFDA 21 CFR 177.2600ASTM D1646, ASTM D412Innerliners, pharmaceutical stoppers
    LLDPE stretch film cling additiveFDA 21 CFR 177.1520ASTM D882, ASTM D1894Pallet wrap, silage wrap, stretch hoods

    Hot-Melt Pressure-Sensitive Adhesive Compounding with HRD-500 as an Aliphatic Tackifier and Plasticizer

    SIS- and SBS-based hot-melt pressure-sensitive adhesives are compounded with HRD-500 to lower rubber-phase glass transition temperature and to reduce melt viscosity in a heated sigma-blade mixer or a 44:1 L/D co-rotating twin-screw extruder. Addition levels are typically 5–15 phr relative to the styrenic block copolymer, with an optimum processing window of 8–12 phr for label and tape formulations; at 15–20 phr, shear adhesion failure temperature and room-temperature shear adhesion measured by ASTM D3654 fall rapidly because HRD-500 dilutes the styrenic endblock network. Loop tack measured by ASTM D6195 may increase up to 10 phr, but higher loadings produce a soft, stringing adhesive with excessive residue on stainless steel test panels. Processing in a heated mixer at 130–170 °C should use staged addition of HRD-500 after the block copolymer has melted; adding it simultaneously with high-acid rosin ester tackifiers above 180 °C can trigger acid-catalysed depolymerisation and generate low-molecular-weight volatiles. Production-scale 44:1 L/D co-rotating twin-screw compounding with screw speeds above 200 rpm and HRD-500 above 12 phr can exhibit pressure fluctuation and screw slippage due to low melt viscosity; barrel temperatures should be reduced by 5–10 °C in later zones to maintain viscosity. A nitrogen blanket is applied to prevent oxidative colour development beyond Gardner colour 3. The compounded hot melt is applied to facestock by slot die coating or roller coating at 150–170 °C. Compliance for food-contact label and tape constructions falls under FDA 21 CFR 175.105, with additional REACH and RoHS declarations for imported articles. Terminal products include clear film label facestocks, hygiene construction adhesives for disposable absorbent articles, and low-noise packaging tape adhesives.

    For optical fibre water-blocking gels and metallic cable flooding compounds, HRD-500 is used at addition levels of 10–35 wt% relative to a hydrocarbon oil base to raise cone penetration stability and to reduce oil bleed across thermal cycling. The compound is prepared in a heated planetary mixer at 80–110 °C, where HRD-500 is first dissolved into the mineral oil or polyalphaolefin base before fumed silica is dispersed under vacuum. A small amount of SEBS or low-density polyethylene may be added at 120–130 °C to build yield stress, but published data for HRD-500 specifically in cable gel matrices is limited and formulation ranges are transferred from analogous low-Mn HR-PIB grades. Cone penetration is measured by ASTM D217 at 25 °C; target penetration for loose tube gels is commonly 350–450 dmm, while metallic floodants may require 250–350 dmm. Water penetration resistance is evaluated according to IEC 60794-1-2 method F5 or equivalent industry standards, and electrical safety compliance for final cables is assessed under RoHS 2011/65/EU. Processing must avoid temperatures above 140 °C in the presence of air because oxidative chain scission of HRD-500 changes gel viscosity and increases oil separation. Terminal products include fibre optic loose tube filling compounds, buffer tube gels, copper telecom cable floodants, and moisture-barrier gels for metallic conductors.

    When HRD-500 Replaces Paraffinic Oil in Butyl Innerliner Compounds, Air Retention and Processing Balance Change

    In butyl and chlorobutyl innerliner compounds, HRD-500 acts as a low-volatility aliphatic plasticiser at 3–10 phr, allowing a reduction in Mooney viscosity without the high-temperature volatility of paraffinic oil. The compound is mixed in an internal mixer with two-stage mixing: first stage at 140–160 °C ram temperature with carbon black, plasticiser, and zinc oxide; second stage below 110 °C for vulcanisation accelerators. Oscillating disc rheometer kinetics are used to set cure parameters, and Mooney scorch time is measured by ASTM D1646; the actual scorch shift must be confirmed on factory-scale extrusion lines because HRD-500 can alter die swell and green strength above 10 phr. Tensile strength and elongation at break are evaluated by ASTM D412, and air retention is measured by a permeability cell at 60 °C under 0.5–1.0 bar differential pressure. Compliance for pharmaceutical stopper applications is established under FDA 21 CFR 177.2600 for rubber articles intended for repeated food contact or under applicable pharmacopoeia monographs. Avoid combination with high zinc oxide loadings above 5 phr and amine-based accelerators at high mixing temperatures because premature crosslinking can occur and reduce scorch safety margin. Terminal products include tyre innerliners, bicycle inner tubes, chlorobutyl pharmaceutical stoppers, and protective rubber sheets.

    Blown film lines processing LLDPE-based stretch film commonly use HRD-500 at 1–3 wt% to control unwind noise and cling force by migrating to the film surface over 24–72 h after extrusion. The additive is incorporated by dry blending with LLDPE granules and fed directly to a single-screw blown film extruder with a die gap of 1.5–2.5 mm and melt temperature of 180–220 °C; die temperatures are maintained below 230 °C to avoid oxidative gel formation that can clog screen packs and cause melt fracture. Cling force is influenced by surface migration and is evaluated by the coefficient of friction method ASTM D1894, while film tensile properties are measured by ASTM D882 for machine-direction and transverse-direction specimens. For food-contact stretch wrap, the final film must meet FDA 21 CFR 177.1520 for olefin polymers used in contact with food; specific conditions of use and additive concentration limits should be verified against the current regulation. Production bottlenecks occur when the film is wound at high tension immediately after extrusion; if rewinding is done before surface bloom is complete, cling force may be low and blocking may vary across the roll. Terminal products include pallet wrap, silage wrap, stretch hoods, and antistatic films for packaging applications.

    Free Quote

    Competitive Polyisobutylene HRD-500 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@alchemist-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@alchemist-chem.com

    Inquiry

    Get Free Quote of Inner Mongolia Eppen Biotech Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Polyisobutylene HRD-500 is a high-molecular-weight isobutylene homopolymer supplied for non-vulcanizing adhesive, sealant, lubricant-additive, and polymer-modification applications. The grade designation HRD-500 is a manufacturer-specific product identifier; it does not represent a direct molar mass in kilograms per mole. Chemical identification is established by CAS registry number 9003-27-4. The polymer consists of a saturated hydrocarbon backbone with terminal microstructures that depend on the polymerization and quenching chemistry. That structural feature separates HRD-500 from isobutylene-isoprene copolymers such as butyl rubber, which contain main-chain unsaturation and can be sulfur-vulcanized. The product is non-polar, non-aqueous, and is normally supplied in bale or pellet form; the exact physical form should be confirmed on the supplier’s certificate of analysis.

    Because the manufacturer has not released a complete public datasheet for HRD-500, the property envelope below is class-typical for high-molecular-weight polyisobutylene and is not a substitute for lot-specific data. Published data for this specific configuration is limited, particularly for melt rheology and batch-to-batch variation. Density values for high-Mw PIB are commonly reported between 0.91 g/cm³ and 0.93 g/cm³ at 20 °C under ISO 1183-1. Differential scanning calorimetry under ISO 11357-2 generally records glass transition values between -60 °C and -70 °C. The material is not sulfur-curable; the absence of significant unsaturation can be confirmed by iodine value testing. Melt flow rate is not a suitable specification for HRD-500 because the high molecular weight produces melt-flow values that are not representative of processability.

    Representative property and behavior comparison for high-Mw PIB class and low-molecular-weight polybutene; HRD-500-specific values require supplier certificate of analysis.
    ParameterTest method or referenceHigh-Mw PIB class, HRD-500 referenceLow-molecular-weight polybutene
    Density at 20 °CISO 1183-10.91–0.93 g/cm³0.88–0.92 g/cm³
    Glass transitionISO 11357-2-60 °C to -70 °C-60 °C to -75 °C
    Entanglement stateClass behaviorAbove critical entanglement threshold; elastic plateau presentBelow or near threshold; predominantly viscous response
    VulcanizabilitySulfur cure, rheometerNot sulfur-curableNot sulfur-curable
    Cold flow under loadASTM D621 or internal creep methodLower than low-Mw PIB but measurableHigher flow, especially above 40 °C
    Ozone resistanceISO 1431-1High; saturated backboneHigh; saturated backbone
    Adhesive shear responseASTM D3654Higher cohesive strength potentialLower cohesive strength; higher migration

    What Distinguishes HRD-500 from Low-Molecular-Weight Polybutene in Pressure-Sensitive Formulations?

    In hot-melt pressure-sensitive adhesive systems, the main difference between HRD-500 and low-molecular-weight polybutene is topological entanglement. HRD-500 chains exceed the critical molecular weight for entanglements, which generates elastic character at short deformation times and improves resistance to shear flow under sustained load. Low-molecular-weight polybutene behaves as a viscous liquid and migrates more readily to bond lines and substrates. This migration can provide temporary tack but reduces cohesive strength and long-term shear holding. The trade-off is measurable: replacing a portion of low-Mw polybutene with HRD-500 at equal total polymer content raises mix viscosity and may reduce initial loop tack under ASTM D6195, while increasing shear holding time under ASTM D3654. Published data for this specific configuration is limited; the direction and magnitude of these effects depend on tackifier softening point, oil loading, and end-block content.

    Adhesive formulators should not treat HRD-500 as a direct drop-in for low-Mw polybutene because melt viscosity rises disproportionately as molecular weight increases. If a plant uses a hot-melt mixer set at 150 °C for a low-Mw PIB formulation, the same mixer may require a temperature increase of 10 °C to 15 °C or a longer incorporation pass for HRD-500. Capillary rheometry under ISO 11443 or oscillatory shear under ISO 6721-10 should be used to establish the melt-viscosity difference before scale-up. The saturated backbone provides high resistance to ozone and ultraviolet degradation, but no polar adhesion sites are present; substrate wetting is controlled by resin modification rather than by polymer functionality.

    Compared with butyl rubber, HRD-500 does not contain sufficient isoprene-derived unsaturation for sulfur crosslinking. Butyl rubber is typically copolymerized with a small molar percentage of isoprene and can develop a true thermoset network under vulcanization. HRD-500 remains a high-viscosity viscoelastic fluid after heating and cooling; it may exhibit cold flow under load unless compounded with fillers, crystalline waxes, or crosslinkable co-curable elastomers. This limitation is an intentional design feature for non-curing sealants and adhesives but it disqualifies HRD-500 from use as the sole elastomer in a thermoset rubber specification.

    Viscosity-Temperature Response and High-Shear Processing Boundaries

    HRD-500 is a viscoelastic melt with strong shear-thinning behavior. Oscillatory shear measurements under ISO 6721-10 are more informative than melt flow rate, which is unsuitable for high-Mw PIB. The material exhibits a relatively high zero-shear viscosity and a broad relaxation spectrum; small changes in temperature produce large changes in viscosity. This imposes narrow processing temperature control. Processing below approximately 150 °C may generate excessive torque and poor dispersion in high-shear mixers. Class-equivalent high-Mw polyisobutylene is typically mixed at 150 °C to 180 °C. Above 200 °C, thermal degradation becomes more pronounced, and random chain scission reduces molecular weight. Published data for HRD-500-specific degradation kinetics is limited; the 200 °C upper boundary is drawn from class-wide polyisobutylene degradation behavior.

    In production-scale compounding, temperature control must include shear heating, not only barrel set points. The polymer’s high viscosity causes dissipative heating in the melt zone. A corotating twin-screw extruder with L/D ratio between 40:1 and 52:1 can compound HRD-500 with fillers and tackifiers, but the screw profile should include gentle melting elements followed by distributive mixing rather than aggressive high-shear kneading blocks throughout. If the feed is a dry blend, localized overheating may occur at filler-polymer interfaces; published data for this specific configuration is limited, but equivalent high-Mw PIB grades show improved uniformity when the polymer is pre-blended with a portion of the plasticizer or low-Mw polybutene.

    Processing failure modes include throat bridging, melt fracture at the die, and torque spikes at filler loadings above 30 phr. These are not unique to HRD-500 but are common to high-molecular-weight polyisobutylene. Preconditioning bales at ambient temperature for 24 h to 48 h before mixing can reduce feed variability. Moisture condensation on cold polymer surfaces should be avoided at relative humidity above 60 %; the polymer itself is not hygroscopic, but condensed water can create steam porosity in extruded profiles.

    Differences from medium-molecular-weight PIB grades appear in processing and end-use properties. Medium-Mw PIB grades often have viscosity-average molecular masses in the range of 150,000 g/mol to 400,000 g/mol; they are easier to compound and can be processed at lower temperatures, but they provide less resistance to cold flow and lower shear holding. HRD-500 is positioned in a higher molecular-weight envelope. The exact viscosity-average molecular mass of HRD-500 is not published; process and property comparisons must rely on supplier certificate of analysis. Compared with metallocene polyolefin elastomers, HRD-500 lacks crystallinity and has a lower density and a lower modulus at room temperature, but it provides excellent moisture-vapour barrier and broad tackifier compatibility. Those characteristics are relevant in butyl tape and sealant compounds where amorphous polyolefins often require higher filler loadings to control slump.

    When HRD-500 Replaces Amorphous Polyolefins in Hot-Melt Sealant Applications

    HRD-500 may replace amorphous polyolefins or low-molecular-weight polybutene in hot-melt sealant and butyl tape formulations when a non-curing polymer with better cohesive strength and lower migration is required. The replacement is not one-to-one. The higher entanglement density reduces slump and cold flow, but also reduces wet-out on rough or dusty substrates unless tackifier and processing oil ratios are adjusted. In hot-melt sealants, low surface energy substrates may require additional tackifier, while polar substrates may require a separate adhesion promoter because HRD-500 has no carboxyl, hydroxyl, or maleic functionality.

    For butyl tape-style sealants, HRD-500 can serve as a non-curing modifier to improve shape retention and moisture-vapour barrier properties. However, ultimate cohesive strength remains lower than that of a vulcanized butyl compound, and compression set is not comparable to a crosslinked network. If a specification requires compression set testing under ISO 815-1 at 70 °C for 22 h, the compound containing HRD-500 will typically show substantial deformation unless a co-curable elastomer and curative package are included. The material is not sulfur-curable by itself.

    In high-viscosity lubricant and grease applications, HRD-500 may be used as a thickener or oil-retention additive. The saturated backbone provides good compatibility with mineral oils, but oxidative stability at temperatures above 120 °C in continuous air exposure requires an antioxidant package. Oxidation induction time testing under ISO 11357-6 should be performed on the final blend, not on the raw polymer. The high molecular weight of HRD-500 can contribute stringiness and tackiness in grease formulations; published data for this specific application is limited.

    Application-specific evaluation matrix for Polyisobutylene HRD-500.
    Application sectorRelevant test method or standardHRD-500-specific limitation or control
    Hot-melt pressure-sensitive adhesiveASTM D3654, ASTM D6195High mix viscosity; pre-blend with tackifier or oil; published data limited for HRD-500
    Butyl tape and non-curing sealantISO 815-1, ASTM D471Not sulfur-curable; cold flow remains measurable unless filled
    Grease and high-viscosity lubricantISO 11357-6Antioxidant required above 120 °C; compatibility with base oil should be tested
    Food-contact adhesiveFDA 21 CFR 177.1420End-use limitations and finished-article migration control; raw polymer CofA not sufficient
    Electrical/electronic sealingASTM F2617, IEC 62321RoHS applied to finished article; halogen-free claims require specific testing

    For food-contact articles, polyisobutylene may be evaluated under FDA 21 CFR 177.1420 as an isobutylene polymer, subject to limitations in the regulation and to overall migration testing in the final article. The raw polymer certificate of analysis cannot by itself establish food-contact compliance of a finished adhesive or sealant. For European supply, REACH registration under EC 1907/2006 must be confirmed with the supplier, and any Annex XVII restrictions relevant to the final article must be reviewed. Halogenated solvent content, heavy metals, and other potential extraneous residues should be tested according to supplier methods or applicable finished-article standards. RoHS obligations generally apply to the finished electrical or electronic equipment, not to the raw polymer.

    Solvent resistance is limited with aromatic hydrocarbons, chlorinated solvents, and some low-molecular-weight mineral oils at elevated temperature. Swelling and mass change under ASTM D471 should be evaluated for sealing applications. Strong oxidizing agents should not be melted with HRD-500. The polymer should be stored below 40 °C and away from direct sunlight. The product is not biodegradable and is not intended for uncontrolled environmental release; disposal and recycling must follow local polymer waste regulations.