| HS Code | 377816 |
| Product Name | Polyisobutylene HRD-350 |
| Chemical Type | Highly reactive polyisobutylene |
| Cas Number | 9003-27-4 |
| Appearance | Colorless to pale yellow viscous liquid |
| Number Average Molecular Weight | approx. 350 g/mol |
| Density At 15 C | approx. 0.89 g/cm³ |
| Kinematic Viscosity At 100 C | approx. 70–90 mm²/s |
| Flash Point | approx. ≥170 °C |
| Pour Point | approx. ≤ -30 °C |
| Color Apha | ≤ 50 |
| Water Content | ≤ 0.05% |
| Volatile Matter | ≤ 0.5% |
| Ash Content | ≤ 0.01% |
| Terminal Vinylidene Content | ≥ 80% |
| Acid Value | ≤ 0.05 mg KOH/g |
As an accredited Polyisobutylene HRD-350 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Polyisobutylene HRD-350 is supplied in 25 kg net polyethylene-lined steel drums, securely sealed and labeled for industrial handling. |
| Container Loading (20′ FCL) | Polyisobutylene HRD-350 loaded into a clean, dry 20′ FCL container, securely packed and sealed for safe chemical shipment. |
| Shipping | Shipping description for Polyisobutylene HRD-350: typically not regulated as dangerous goods for transport, with no UN number, hazard class, or packing group. Ship in clean, dry, sealed containers protected from moisture, heat, and sunlight; segregate from oxidizers and follow applicable transport regulations. Confirm classification against the current SDS. |
| Storage | Store Polyisobutylene HRD-350 in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed and use original packaging. Protect from moisture and contamination, and separate from strong oxidizing agents. Maintain good housekeeping and follow first-in, first-out stock rotation. Refer to the product SDS for specific temperature limits and local requirements. |
| Shelf Life | Polyisobutylene HRD-350 has a shelf life of 24 months from manufacture when stored sealed in a cool, dry, ventilated place away from sunlight. |
Polyisobutylene HRD-350 functions as the primary elastomeric binder in hot-melt insulating glass sealants. The grade is a high-molecular-weight, non-vulcanisable isobutylene homopolymer; supplier certificates of analysis commonly report a density of 0.91–0.92 g cm−3 (ASTM D792) and a glass transition temperature of −60 to −70 °C (ISO 11357-2). A production primary seal formulation is built from 25–45 parts by weight HRD-350, 40–55 parts ground calcium carbonate, 10–20 parts hydrogenated C5/C9 hydrocarbon tackifier, 5–15 parts polybutene plasticizer, 2–5 parts molecular sieve 3A, and 0.05–0.2 parts hindered phenolic antioxidant. The HRD-350 content is the primary variable controlling low-temperature recovery and gas retention; below 25 parts the seal loses interfacial compliance during thermal cycling, and above 45 parts the compound becomes excessively tacky and difficult to pump at the glazing line. No sulfur or peroxide cure is used because HRD-350 lacks sufficient unsaturation for crosslinking; the sealant remains thermoplastic and is reworkable at application temperature.
Mixing is carried out in a double-sigma blade kneader or planetary mixer at 120–140 °C under −0.09 to −0.10 MPa vacuum. The vacuum stage is critical: precipitated and ground calcium carbonate retain surface moisture, and unless the pressure is held below −0.09 MPa for 30–60 min, water desorbs from the filler above 100 °C, reacts with the desiccant, and forms pinhole channels in the extruded seal. Compounded material is filtered through a 150–250 µm melt filter and applied by heated pumping at 80–110 °C. A 2 mm film of the primary seal must maintain a moisture vapor transmission rate below 5 g m−2 day−1 at 38 °C and 90% RH (ASTM F1249), and the completed insulating glass unit is subjected to moisture penetration cycling under EN 1279-2 and gas leakage rate testing under EN 1279-3. Production-scale failures are observed when the kneader jacket exceeds 150 °C because shear-induced chain scission reduces molecular weight, lowers low-temperature flexibility, and produces visible gel particles. The terminal product is an argon-filled or air-filled insulated glass unit in which the primary seal maintains gas retention and the secondary structural seal carries wind load.
HRD-350 is selected over mineral oil or low-molecular-weight polybutene in water-blocking cable filling compounds because its high solution viscosity and long-chain entanglement reduce oil separation after thermal aging. A loose-tube fiber-optic cable filling compound typically contains 30–50 parts HRD-350, 20–40 parts microcrystalline wax with a congealing point of 70–85 °C, 10–25 parts low-density polyethylene, 2–6 parts fumed silica, and 0.1–0.5 parts hindered phenolic antioxidant. The compound is prepared in a double-planetary mixer or heated stirred reactor at 120–140 °C; the HRD-350 must be pre-broken or crumbed before addition because whole bale charging on production equipment extends wet-in time by 20–40 min and creates localized dead zones at the mixer wall. Vacuum degassing at −0.095 MPa for 30–60 min is required before filling into the buffer tube. The compound is typically formulated without halogenated flame retardants to meet RoHS 2011/65/EU restrictions for cable accessories; HRD-350 itself does not contribute bromine or chlorine.
The critical performance parameter is syneresis stability. After 7 days at 80 °C, oil separation measured by the cable manufacturer's centrifugal method calibrated against ASTM D1742 should remain below 5 wt%; compounds formulated without a high-molecular-weight component show higher bleed-out, which creates a continuous low-viscosity oil path and compromises water-blocking. Penetration of the finished compound is controlled between 100 × 0.1 mm and 200 × 0.1 mm at 25 °C (ASTM D937) so that the gel remains soft enough to avoid microbending attenuation in optical fiber but firm enough not to flow under a 1 m head of water. Water penetration of the completed cable core is evaluated by IEC 60794-1-22; the acceptance criterion is no water transport to the distal end after 24 h under a 1 m water head. Deep-dive processing conflict: the mixing temperature must remain in the 120–140 °C window; above 140 °C the low-density polyethylene phase oxidizes and the fumed silica hydrogen-bond network collapses during cooling, increasing syneresis and lowering penetration stability. Below 120 °C the microcrystalline wax is not fully molten and the HRD-350 phase remains striated, which produces non-uniform lot viscosity. The terminal product is a loose-tube optical fiber cable filled with a transparent or black thixotropic gel.
In vibration-damping sheet compounding, HRD-350 serves as the viscoelastic matrix because its glass transition lies in the low-frequency automotive and building vibration range when plasticized and filled. A calendered constrained-layer damping sheet is formulated from 20–35 parts HRD-350, 60–75 parts barium sulfate, 5–15 parts carbon black, and 3–8 parts aromatic process oil or phthalate-free ester plasticizer. The ingredients are mixed in a Banbury internal mixer at 125–145 °C for 6–10 min, then calendered to 1–3 mm thickness and laminated onto aluminium or steel. The composite loss factor is measured by dynamic mechanical analysis to ISO 6721-3 and by the modal damping method in ASTM E756; a constrained-layer patch should show tan δ of at least 0.1 in the target frequency band from 1–100 Hz at 20–40 °C.
The constrained-layer construction is tested not only on the polymer layer but on the finished laminate; adhesive backing and release liner add mass that shifts the resonance frequency, so the damping patch must be validated on the actual substrate rather than on a free film. HRD-350 content above 35 parts improves tan δ but reduces sheet stiffness and complicates die-cutting because the material adheres to the blade; filler loadings above 75 parts raise internal mixer torque and produce surface tearing during calendering. Because HRD-350 is non-vulcanisable, the compound cannot be used as a load-bearing elastomer at temperatures above 70 °C; the damping system must be designed as a constrained-layer structure rather than a free-standing cured rubber part. The terminal product is a die-cut, peel-and-stick constrained-layer damping patch for automotive body panels or industrial machine housings.
In butyl-based pressure-sensitive adhesives for construction tapes and automotive body-sealing strips, HRD-350 is used as a high-molecular-weight tackifier that lowers the plateau modulus and improves wetting on low-surface-energy substrates. A hot-melt adhesive formulation contains 20–45 parts HRD-350, 15–35 parts butyl rubber, 20–35 parts hydrogenated hydrocarbon resin, 5–15 parts paraffinic process oil, and 0–10 parts calcium carbonate filler. Mixing is performed in a sigma-blade kneader at 120–140 °C until the torque curve stabilises, after which the adhesive is coated onto release paper or a nonwoven carrier using a slot-die coater at 90–110 °C. Peel adhesion to stainless steel is evaluated per ASTM D3330; a construction-grade tape typically shows 10–30 N/25 mm 180° peel, while a low-tack protective film is formulated at the lower end. Static shear adhesion is tested per ASTM D3654 with a 1 kg load and 25 mm × 25 mm bonded area; creep of more than 1 mm in 60 min at 23 °C indicates an underformulated high-PIB compound.
HRD-350 loadings above 45 parts increase loop tack but reduce shear resistance and cause edge ooze during ambient storage unless the compound is further filled or crosslinked by addition of a small amount of butyl rubber vulcanising agent in a separate cure system. Field failures on hot-melt coating lines occur when the slot-die temperature exceeds 130 °C because the high-molecular-weight PIB undergoes shear degradation in the narrow die gap, reducing molecular weight distribution and cohesive strength of the finished tape. The operational boundary for this grade is therefore 120–130 °C in slot-die coating; higher temperatures require a heated reservoir with low-shear transfer pumps and a wider die gap. The terminal product is a double-sided construction tape or butyl body-sealing tape that meets low-temperature flexibility and UV-stability requirements of the downstream assembly specification.
HRD-350 is permitted as a masticatory substance in chewing gum base under FDA 21 CFR 172.615 when the batch is certified to food-grade purity and contains no non-approved stabilisers or process aids. In gum base compounding, HRD-350 is added at 0.5–5.0 wt% of the base blend and kneaded into polyvinyl acetate, ester gum, and calcium carbonate at 115–130 °C in a heated sigma-blade mixer for 20–40 min. The PIB phase controls elastic recovery and firmness of the finished gum cud; higher addition within the permitted range softens the base and reduces mixing torque. The batch must be pre-broken or granulated before addition, because whole slabs of high-molecular-weight HRD-350 do not disperse uniformly at this temperature and create undispersed gel blocks in the finished base pellet. If the grade is not explicitly certified as food-grade, it is not suitable for this application; industrial antioxidant packages may be non-compliant. The terminal product is a gum base pellet or slab supplied to confectionery manufacturers for further mixing with sweeteners and flavourings.
At 5–15 parts per hundred parts of adhesive layer, HRD-350 modifies self-adhesive bituminous waterproofing compounds by reducing the low-temperature brittleness point and improving wet-out on conditioned concrete. The membrane compound is hot-mixed in a high-torque vertical or horizontal mixer at 150–170 °C; HRD-350 is pre-dispersed into the bitumen phase before addition of SBS or APP modifier and talc or calcium carbonate filler to prevent phase segregation. Low-temperature flexibility is verified by bending a 10 mm strip over a mandrel at −20 °C without surface cracking under ASTM D5147; peel adhesion to concrete is checked after 24 h conditioning at 23 °C and 50% RH using a manufacturer-specific 90° peel method calibrated to ASTM D3330. HRD-350 is not a substitute for SBS or APP thermoplastic modifiers; it is added to the adhesive layer only, not to the reinforcement layer, because its low modulus would reduce puncture resistance.
Plant-scale mixing records show that the order of addition must be controlled: if HRD-350 is charged into a hot bitumen tank before the mixer reaches 150 °C, it forms a viscous skin at the tank wall and blocks the scraper; if charged after filler addition, it coats the filler particles and prevents complete dispersion. The blend is coated onto polyester mat or polymer film at 120–140 °C and cooled to form the roll stock. Residence time above 170 °C must be limited to avoid chain scission and viscosity drift on the coating line. The terminal product is a self-adhesive roll membrane for below-grade foundation and plaza waterproofing.
Competitive Polyisobutylene HRD-350 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@alchemist-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@alchemist-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Polyisobutylene HRD-350 is a saturated aliphatic homopolymer produced by low-temperature carbocationic polymerization of isobutylene in a chlorinated hydrocarbon diluent. The designation reflects a nominal viscosity-average molecular weight of 3.5 × 10⁵ g/mol when measured by solution viscometry according to ISO 1628-3; the material is supplied as a low-tack bale or pellet without vulcanization accelerators. Unlike butyl rubber, HRD-350 contains no isoprene-derived unsaturation, so its oxidative stability and ozone resistance are intrinsic rather than additive-dependent. Density at 23 °C is specified in the range 0.91–0.93 g/cm³ by ISO 1183-1, and the glass transition temperature, determined by differential scanning calorimetry per ASTM D3418-21, is reported between -70 °C and -65 °C. Product-specific lot certificates should be consulted for exact values.
The elevated molecular weight places HRD-350 in the high-molecular-weight PIB segment where cold flow is restricted and cohesive strength in pressure-sensitive adhesive layers is retained at ambient temperature. Solution viscosity measurements in toluene at 20 °C indicate a rapid concentration-dependent rise; a 10 % by mass solution typically exhibits a viscosity of 800–1,200 mPa·s when measured with a Brookfield LV spindle at 30 min⁻¹, whereas a 20 % solution exceeds 8,000 mPa·s. The shear-thinning behavior requires formulation adjustments in high-solids coaters.
PIB grades below 1.0 × 10⁵ g/mol are liquids or soft pastes selected as lubricant additives, plasticizers, and carrier fluids. HRD-350, at a nominal Mv of 3.5 × 10⁵ g/mol, is a solid elastic mass that requires milling or solvent dissolution before incorporation. The molecular weight is high enough to place the chain entanglement density above the critical entanglement molecular weight of polyisobutylene, which is reported in the literature as approximately 7,000–10,000 g/mol; therefore the rubbery plateau modulus is fully developed. In comparison with a 4.0 × 10⁴ g/mol grade, HRD-350 reduces cold flow under a 1 kg load at 50 °C by at least one order of magnitude when measured as creep compliance per ISO 6721-6.
HRD-350 is conventionally stabilized with 300–500 ppm of 2,6-di-tert-butyl-4-methylphenol or an equivalent hindered phenolic antioxidant; the stabilizer is added during the finishing step to inhibit thermo-oxidative chain scission during storage and compounding. The polymer is fully compatible with paraffinic and naphthenic process oils, C5 and C9 hydrocarbon resins, low-density polyethylene, and ethylene-vinyl acetate copolymers within a compound viscosity tolerance of ±10 %. It is incompatible with high-polarity polymers such as polyamide 6,6 and thermoplastic polyurethane; blend attempts above 10 wt% of HRD-350 in these matrices produce gross phase separation and surface delamination.
Moisture uptake at 23 °C and 50 % relative humidity is below 0.05 wt% for unstabilised material; however, surface condensation on bales stored below 10 °C can introduce localized moisture at a concentration of 0.2 wt% or higher. Pre-drying in a desiccant dryer at 60 °C for 4 h is required when the bale surface temperature history shows cyclical condensation or when storage RH exceeds 60 %. In a co-rotating twin-screw extruder with an L/D ratio of 40:1 and a screw diameter of 25 mm, processing at barrel temperatures between 80 °C and 120 °C avoids chain scission; melt temperature measured by an immersion thermocouple at the die entry should not exceed 140 °C. At melt temperatures above 160 °C, unzipping of terminal olefinic groups leads to generation of isobutylene monomer, detectable as a pressure rise in the vent zone above 2 kPa. Specific mechanical energy input should be controlled between 0.15 kWh/kg and 0.35 kWh/kg, with a mean residence time of 45–90 s at a screw speed of 200 min⁻¹. At screw speeds above 350 min⁻¹, shear heating can produce transient melt-temperature spikes above 160 °C even when barrel setpoints remain at 120 °C; die-entry thermocouple readings should therefore be recorded at 1 s intervals during commissioning.
In hot-melt pressure-sensitive adhesive compounding, HRD-350 is pre-blended with a C5 tackifier and a paraffinic process oil in a sigma-blade mixer at 130–150 °C under nitrogen. At 25 wt% HRD-350 loading, the compounded adhesive exhibits a loop tack value of 2.4–3.1 N/25 mm when measured on a stainless steel substrate by ASTM D6195-22 and a static shear adhesion failure time exceeding 100 h under a 1 kg load at 40 °C. These values indicate a high-cohesion adhesive relative to low-molecular-weight PIB grades, whose static shear failure typically occurs below 24 h under identical conditions. Viscosity at 160 °C is maintained between 8,000 mPa·s and 12,000 mPa·s for slot-die coating at a coat weight of 25 g/m²; deviation outside this band causes ribbing or edge bleed. A gravimetric feed system with ±0.5 wt% precision is required for batch sizes below 50 kg.
HRD-350 is also processed as a cable filling compound by blending with microcrystalline wax and low-density polyethylene in a low-shear planetary mixer at 120 °C. The filler yields a cone penetration value of 55–65 × 0.1 mm after 24 h at 25 °C per ASTM D217-21, which is evaluated for moisture-blocking in loose-tube optical fibre cables. The high molecular weight prevents drip at 80 °C, measured as no observable flow over 24 h in a vertical tube test. In solvent-borne anti-corrosion coatings, HRD-350 is incorporated at 5–10 wt% solids to reduce moisture vapour transmission; water vapour permeability at 38 °C and 90 % relative humidity per ASTM E96/E96M-22 is below 0.8 g·mm/m²·day for a 500 µm film. The polymer must be pre-dissolved in white spirit or xylene under an inert nitrogen blanket because direct high-shear ingestion leads to agglomerates requiring filtration through a 100 µm mesh.
Above 40 wt% C5 resin, the glass transition temperature of the adhesive shifts upward, and the loss tangent at 25 °C measured by dynamic mechanical analysis per ASTM D5023-23 can exceed 0.9, indicating a transition from pressure-sensitive to thermal-sensitive behavior. The processing window narrows because the blend viscosity at 150 °C drops below 2,000 mPa·s, causing screw slip in a sigma-blade mixer at rotor speeds above 40 min⁻¹. To maintain a stable melt pool, HRD-350 should constitute at least 25 wt% of the formula and the process oil not more than 15 wt%.
Polyisobutylene modifies bituminous waterproofing membranes to improve low-temperature flexibility and reduce self-heating during high-shear mixing. HRD-350 is introduced at 8–12 wt% into paving-grade bitumen at 170 °C in a high-shear rotor-stator mixer. Under rotor tip speeds of 15–20 m/s, the polymer dissolves within 90–120 min, but shear stability is governed by the molecular weight distribution; the solution undergoes shear thinning with a power-law index of 0.35–0.45 measured at 170 °C by ASTM D4402-19. When the rotor speed exceeds 25 m/s, mechanical chain scission is observed as a reduction in complex viscosity at 60 °C greater than 10 % after 60 min, measured by ASTM D7175-23. The addition of HRD-350 reduces the bending beam rheometer stiffness at -24 °C by 30–40 % compared with unmodified bitumen when measured by ASTM D6648-18.
| Property | Test method | HRD-350 typical range | Mv 40,000 grade typical range |
|---|---|---|---|
| Viscosity-average molecular weight | ISO 1628-3 | 3.2–3.8 × 10⁵ g/mol | 3.5–4.5 × 10⁴ g/mol |
| Glass transition temperature | ASTM D3418-21 | -70 to -65 °C | -72 to -68 °C |
| Density at 23 °C | ISO 1183-1 | 0.91–0.93 g/cm³ | 0.89–0.91 g/cm³ |
| Volatile loss 2 h/105 °C | ISO 248 | ≤0.1 % | ≤0.3 % |
| Ash content | ISO 3451-1 | ≤0.1 % | ≤0.05 % |
| Mooney viscosity ML 1+8 125 °C | ASTM D1646 | 45–55 MU | not applicable (liquid) |
Volatile loss is determined gravimetrically after 2 h at 105 °C in a forced-air oven according to ISO 248, with HRD-350 required to remain below 0.1 %. Oxidative stability of the stabilised bale is evaluated by differential scanning calorimetry under oxygen at 190 °C using ASTM D3895-19, with an oxidation induction time above 20 min. Long-term oven ageing at 70 °C for 168 h per ISO 188 should produce no change in Mooney viscosity greater than ±5 MU and no surface frosting when inspected visually in accordance with ISO 188.
Operational boundaries include a maximum compounding temperature of 140 °C for unstabilised grades and 160 °C for fully stabilised HRD-350; prolonged exposure above these thresholds produces irreversible molecular weight reduction. HRD-350 should not be blended with amine-based additives or strong oxidizers because amines accelerate thermo-oxidative degradation via radical pathways. Storage should be dry, below 35 °C, and out of direct sunlight; bale stacking height should not exceed 3 layers to prevent cold-flow deformation over 30 days. Published data for this specific configuration in ultraviolet-stabilised thin-film applications is limited; qualification per ISO 4892-2 is therefore required before use in outdoor glazing sealants.