    Specifications
    HS Code 634815
    Appearance Clear, viscous liquid
    Color Apha ≤ 50
    Density At 15 C 0.89 g/cm³
    Specific Gravity At 15 4 C 0.89
    Number Average Molecular Weight Mn 2,300
    Kinematic Viscosity At 100 C approx. 2,800 cSt
    Kinematic Viscosity At 150 C approx. 250 cSt
    Flash Point Coc ≥ 220 °C
    Pour Point ≤ -25 °C
    Volatile Matter 180 C 3 H ≤ 0.5 wt%
    Water Content ≤ 0.05 wt%
    Acid Value ≤ 0.02 mg KOH/g
    Ash Content ≤ 0.01 wt%
    Terminal Vinylidene Content ≥ 75%

    As an accredited Polyisobutylene HRD-23H factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Polyisobutylene HRD-23H is packaged in 25 kg net-weight moisture-resistant paper bags for safe industrial handling and storage.
    Container Loading (20′ FCL) A 20′ FCL container loaded with Polyisobutylene HRD-23H in industrial packaging, properly secured for safe ocean transport.
    Shipping Polyisobutylene HRD-23H is shipped as a non-hazardous polymer, not regulated for transport. Pack in sealed, labeled bags, drums, or bulk containers. Keep cool, dry, and ventilated, away from sunlight and ignition. Use standard PPE; avoid dust and moisture. Follow the supplier SDS and local transport regulations.
    Storage Store Polyisobutylene HRD-23H in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizing agents. Keep containers tightly closed, clearly labeled, and protected from moisture, dust, and contamination. Avoid prolonged high-temperature exposure. Do not store near food, feed, or incompatible materials. Provide spill containment and follow the manufacturer’s SDS and local regulations.
    Shelf Life Polyisobutylene HRD-23H is stable; shelf life is generally 24 months when stored cool, dry, sealed, and protected from moisture and contaminants.
    Application of Polyisobutylene HRD-23H

    Polyisobutylene HRD-23H enters the lubricant dispersant chain through a thermal ene reaction with maleic anhydride in a nitrogen-blanketed glass-lined reactor equipped with a thermal oil jacket and thermosiphon reflux condenser. The charge uses a maleic anhydride to polyisobutylene molar ratio of 1.2:1 to 1.6:1. Temperature is held at 200 °C to 230 °C for 18 h to 24 h. Agitator torque is monitored as a proxy for reaction mass viscosity build. The endpoint is determined by residual maleic anhydride below 0.5 wt% and by a stable acid number measured per ASTM D664. Vinylidene conversion is confirmed by the disappearance of the 890 cm⁻¹ C-H bending mode in infrared analysis. The resulting polyisobutenyl succinic anhydride is transferred to a wiped-film evaporator at 5 kPa to 10 kPa absolute pressure to strip unreacted maleic anhydride and low-boiling fragments. Amination with tetraethylenepentamine or heavy polyamine is conducted at 140 °C to 160 °C under a slow nitrogen sweep. The anhydride-to-amine molar ratio is maintained between 1.0:1.0 and 1.6:1.0. Water of imidization is collected overhead. Batch completion is verified by the reduction of the carbonyl band near 1708 cm⁻¹ and by total base number per ASTM D2896. Typical succinimide base number ranges from 10 mg KOH/g to 60 mg KOH/g depending on amine loading. Finished dispersants are dosed into passenger car motor oil at 2 wt% to 8 wt% on a neat-additive basis. Kinematic viscosity of the additized oil is controlled to 9.3 cSt to 12.5 cSt at 100 °C per ASTM D445. Moisture must remain below 0.03 wt% during anhydride synthesis. Water hydrolyzes the succinic anhydride ring and propagates oligomeric cross-links that increase turbidity and plug downstream filtration. The thermal ene route avoids chlorine but requires a higher reaction temperature than chlorinated polyisobutylene routes. Grade-specific vinylidene content and molecular weight for HRD-23H must be verified against the supplier certificate of analysis before scale-up.

    What Changes When HRD-23H Is Converted to Polyisobutylene Amine for Direct-Injection Gasoline Deposit Control?

    Polyisobutylene amine is produced from high-reactivity polyisobutylene in a high-pressure stirred autoclave rated to at least 30 MPa syngas pressure. Hydroformylation uses a rhodium triphenylphosphine catalyst at 110 °C to 140 °C. The CO:H₂ molar ratio is maintained at 1:1. The aldehyde intermediate is then reductively aminated with ammonia and hydrogen over a nickel or cobalt fixed-bed catalyst. Total chlorine must stay below 5 mg/kg. Total sulfur must stay below 10 mg/kg. Chlorine and sulfur act as catalyst poisons and reduce turnover frequency. The resulting polyisobutylene amine is dosed into gasoline or diesel fuel at 50 mg/kg to 1,000 mg/kg as a deposit-control additive. Intake valve deposit mass is measured per ASTM D6201 on a 2.3 L four-cylinder engine. Injector fouling is assessed with CEC F-05-93 or its successor protocol. The keep-clean dose depends on the fuel’s olefin and aromatic profile. The amine terminus anchors to metal oxide surfaces. The polyisobutylene tail extends into the fuel film and dissolves deposit precursors. Published data for HRD-23H-specific hydroformylation turnover is limited. The operating window described here is derived from high-reactivity polyisobutylene class data and should be confirmed with the catalyst supplier.

    In lithium-complex grease finishing, polyisobutylene is added after saponification and dehydration. Base grease temperature is reduced to 105 °C to 120 °C before polymer addition. The tackifying dose is 2 wt% to 6 wt% of finished grease mass. Higher additions can move worked penetration beyond the NLGI 2 boundary unless thickener content is increased. The batch is processed in a high-shear homogenizer or colloid mill with a rotor gap of 0.25 mm to 0.50 mm. Vacuum deaeration is applied at 8 kPa absolute pressure for 20 min to 30 min. Oil separation is controlled below 4 wt% in the ASTM D6184 24-hour conical bleed test. Dropping point remains above 180 °C for lithium-complex thickener systems per ASTM D2265. The polymer modifies low-shear rheology and reduces fling-off in steel-mill bearing lubrication. It does not replace the extreme-pressure additive package. Over-shearing above 130 °C can cause chain scission. Chain scission reduces tack and creates batch-to-batch penetration drift.

    Hot-Melt Adhesive Compounding Limits for Mid-Molecular-Weight Polyisobutylene in SIS Block Copolymer Systems

    Adhesive compounding uses a heated twin-screw extruder with an L/D ratio of 40:1. Screws are segmented with forward conveying elements in the first 60% of the barrel and kneading blocks downstream. Styrene-isoprene-styrene block copolymer is metered at 22 wt% to 30 wt%. Hydrocarbon tackifying resin is metered at 40 wt% to 50 wt%. Polyisobutylene is metered at 10 wt% to 20 wt%. A hindered phenolic antioxidant is added at 0.5 wt%. Barrel temperatures are staged from 120 °C at the feed throat to 170 °C at the discharge. Melt pressure is maintained below 70 bar. Polyisobutylene contributes to tack and low-temperature flexibility. Content above 20 wt% lowers shear adhesion failure temperature measured per ASTM D4498. Melt viscosity is measured at 160 °C per ASTM D3236. Typical values for slot-die coating of tapes and labels range from 800 mPa·s to 5,000 mPa·s. T-peel adhesion is tested on stainless steel per ASTM D1876 after 24 h at 23 °C and 50% relative humidity. Processing above 180 °C for more than 2 h initiates chain scission. Chain scission is indicated by melt viscosity drop and increased smoke at the die.

    When Optical Cable Water-Blocking Gels Are Compounded Under Vacuum

    Polyisobutylene-based filling compounds for loose-tube optical cables are compounded in a planetary mixer equipped with a vacuum dome and heated jacket. A typical batch contains 60 wt% to 80 wt% polyisobutylene, 10 wt% to 25 wt% polyalphaolefin or mineral oil, 5 wt% to 10 wt% fumed silica, and 0.3 wt% antioxidant. The mixer is held at 130 °C to 150 °C and 0.1 kPa to 1 kPa absolute pressure for 60 min to 120 min. Vacuum removes dissolved air and moisture. Cone penetration is measured per ASTM D217. Typical penetration falls between 350 and 500 tenths of a millimetre. The gel must not flow from a stripped cable end after 24 h at 70 °C. Water penetration resistance is tested per IEC 60794-1-22 under a 1 m water head. Polyisobutylene forms the continuous elastomeric phase in the gel. It reduces moisture vapour transmission through the buffer tube and retains stress relaxation capacity during thermal cycling. Fumed silica acts as a thixotropic agent. Dispersion is checked with a Hegman gauge at 40 µm to 100 µm. Undispersed agglomerates are rejected because they can create loss-inducing microbends in the fibre.

    Rubber Inner Liner Compounds Accept Polyisobutylene as a Processing Plasticizer and Impermeability Modifier

    Polyisobutylene is melt-mixed into bromobutyl or chlorobutyl rubber inner liner formulations in an internal mixer with a fill factor of 0.70 to 0.78. Ram pressure is set at 5 bar to 8 bar. The polymer is charged at 70 °C to 90 °C with carbon black, processing oil, and curatives. Dump temperature must not exceed 130 °C. Typical addition is 5 phr to 20 phr. Higher loadings reduce green strength and may slow extrusion line speed. Gas permeability coefficient is measured on cured sheet at 23 °C and 0% relative humidity with a manometric permeability instrument. Tensile strength and elongation at break are measured per ASTM D412. Tear strength is measured per ASTM D624. Batch variance is controlled by monitoring final mixing energy. Torque rise variation above 15% indicates poor filler dispersion or premature curative dispersion. Polyisobutylene must not be combined with amine-based accelerators in the premix stage. Amine-terminated species can interact with residual unsaturation and accelerate scorch.

    Free Quote

    Competitive Polyisobutylene HRD-23H prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@alchemist-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@alchemist-chem.com

    Inquiry

    Get Free Quote of Inner Mongolia Eppen Biotech Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Polyisobutylene HRD-23H is supplied as a high-molecular-weight isobutylene homopolymer in solid, rubber-like bale or pellet form. The repeating unit is [−C(CH3)2−CH2−]n, and the chain is substantially saturated apart from a low concentration of terminal unsaturation formed during cationic polymerization. The HRD-23H designation corresponds to a manufacturer-defined viscosity-average molecular weight class, placing the material among the upper-molecular-weight polyisobutylene grades used in cohesive, permanently tacky, and barrier applications. Product-specific acceptance values are provided on the certificate of analysis; class-typical properties reported for comparable high-molecular-weight polyisobutylene grades include density of 0.91–0.93 g/cm³ measured according to ISO 1183-1, and a glass transition temperature of -70 °C to -65 °C by differential scanning calorimetry per ASTM D3418. Residual water content should be verified by ISO 15512; if moisture exceeds 0.1 wt%, pre-drying at 60–70 °C for 3–4 h is required before melt processing. The unfilled material is not vulcanizable with sulfur or peroxide systems because the backbone contains no significant allylic cure sites; property development relies on physical entanglement and filler reinforcement. Melt flow rate by ISO 1133-1 is typically below 0.1 g/10 min at 190 °C/21.6 kg and is not a routine release parameter for this molecular-weight class.

    What Distinguishes HRD-23H from Low-Molecular-Weight Polybutenes and Butyl Rubber?

    The differentiation is primarily molecular weight, backbone unsaturation, and viscoelastic response. Low-molecular-weight polybutenes with viscosity-average molecular weights of 2×10²–5×10³ g/mol are pourable fluids; HRD-23H is a solid elastomer with an entangled network, measurable elastic recovery, and no pour point at ambient temperature. Butyl rubber is an isobutylene-isoprene copolymer containing 0.5–2.5 mol% isoprene, which introduces allylic unsaturation and permits zinc-oxide/quinoid or sulfur-based vulcanization. HRD-23H lacks this reactive diene level, so conventional accelerated sulfur cure does not develop crosslinks. Free-radical exposure of high-molecular-weight polyisobutylene results predominantly in β-scission and molecular-weight reduction, whereas butyl rubber can be crosslinked under controlled peroxide or resin cure. In unfilled form, the low-temperature flexibility of HRD-23H is attributed to a glass transition below -65 °C, which compares with butyl values of -70 °C to -60 °C but without the cure-dependent compression set of butyl vulcanizates.

    Class-typical ranges used for preliminary formulation selection are shown below; they do not replace product-specific certificates of analysis.

    CharacteristicHRD-23H classLow-MW polybuteneButyl rubber
    Viscosity-average molecular weight1.5×10⁶–2.5×10⁶ g/mol2×10²–5×10³ g/mol3×10⁵–5×10⁵ g/mol
    Density at 25 °C0.91–0.93 g/cm³0.84–0.91 g/cm³0.91–0.92 g/cm³
    Glass transition temperature-70 °C to -65 °C-70 °C to -55 °C-70 °C to -60 °C
    Backbone unsaturation<0.1 mol%, terminal onlyTrace0.5–2.5 mol% isoprene
    Sulfur-vulcanization responseNoneNonePositive
    Ambient volatilityNegligible; volatile matter ≤ 0.1 wt% by ISO 248MeasurableLow; volatile matter ≤ 0.3 wt% by ISO 248

    In hot-melt pressure-sensitive adhesive compounding, HRD-23H is introduced as a high-molecular-weight elastomeric backbone at 5–15 wt% of the elastomer phase to raise cohesive strength and static shear resistance. Production-scale sigma-blade or Z-blade kneaders are typically operated at jacket temperatures of 150–170 °C and rotor speeds of 30–60 min⁻¹; addition of HRD-23H into molten tackifier resin is staged over 45–90 min to avoid excessive motor load. Because the low-molecular-weight tail content varies by lot, kneader torque may shift by 5–10% at constant rotor speed; real-time amperage monitoring is used to detect feed error. Finished adhesive properties are evaluated by ASTM D6195 for loop tack, ASTM D3330/D3330M-04 for peel adhesion, and ASTM D3654/D3654M-06 for static shear. Increasing HRD-23H above 15 wt% typically increases static shear resistance but can reduce loop tack and wet-out on low-energy surfaces. Long-chain entanglement reduces migration into porous paper and nonwoven substrates compared with liquid polybutene; migration kinetics should be revalidated when the adhesive is in direct contact with polyolefin films under storage temperatures above 40 °C.

    Thermo-oxidative Degradation Thresholds and Stabilizer Partitioning

    Thermo-oxidative chain scission is the dominant degradation pathway for HRD-23H above 170–180 °C. Thermogravimetric analysis under nitrogen according to ISO 11358-1 shows onset mass loss for high-molecular-weight polyisobutylene near 280 °C; in air the onset shifts to 220–240 °C, with exothermic oxidative events detectable by ASTM D3418 or ISO 11357-6. On a co-rotating twin-screw extruder with a screw diameter of 25–40 mm and L/D 40:1, barrel settings of 130–160 °C, and screw speeds of 80–120 min⁻¹ are representative for masterbatch dilution. Melt temperature should remain below 170 °C; higher screw speeds can produce melt-pressure instability and torque reduction due to molecular-weight loss. A torque drop exceeding 15% at constant screw speed is a production-scale indicator of chain scission. Hindered phenol primary antioxidants at 0.1–0.5 wt% and phosphite secondary antioxidants at 0.1–0.3 wt% are added to suppress chain scission, but partitioning between the polyisobutylene phase and fillers such as fumed silica or talc depends on additive solubility parameter and surface polarity. Published data for HRD-23H-specific stabilizer partitioning is limited; addition levels must be verified by oven-aging at 100 °C for 168 h with retention of viscosity or tensile energy to break.

    For lubricant and fuel-additive development, HRD-23H is evaluated as a high-viscosity thickener rather than a shear-stable engine-oil viscosity index improver. Low-molecular-weight polybutenes with Mv below 5×10³ g/mol are preferred for dispersant building blocks and fuel deposit-control additives because they remain fluid and show lower susceptibility to permanent shear loss in high-speed journal bearings. HRD-23H can be diluted in hydrocarbon oils to produce high-viscosity gels and greases; in such formulations, the grade contributes oil retention and water resistance, evaluated by cone penetration per ASTM D217 and oil separation per ASTM D6184. Dilution is carried out at 120–150 °C under low-shear mixing; high-shear homogenization above 150 min⁻¹ can mechanically degrade the polymer and reduce gel viscosity. Kinematic viscosity of the neat HRD-23H is not reported by ASTM D445; solution viscosity by ISO 1628-1 or complex viscosity by parallel-plate rheometry is the correct characterisation route.

    Specification verification for HRD-23H-containing compounds typically references the following standard designations.

    Test methodParameter and typical specification framework
    ISO 1628-1Intrinsic viscosity in decalin or toluene; viscosity-average molecular weight class
    ISO 1183-1Density 0.91–0.93 g/cm³
    ISO 15512Water content ≤ 0.1 wt%
    ISO 247Ash ≤ 0.05 wt%
    ISO 248Volatile matter ≤ 0.1 wt%
    ASTM D3418Glass transition temperature -70 °C to -65 °C
    ISO 11357-6Oxidative induction time or oxidation onset by differential scanning calorimetry
    ISO 11358-1Thermogravimetric degradation onset under nitrogen
    FDA 21 CFR 177.1420Finished food-contact article compliance must be established for the specific formulation
    REACH (EC) 1907/2006Substance registration and SVHC screening according to Article 33
    RoHS 2011/65/EUHeavy metal restrictions apply to finished electrical equipment, not neat polymer

    Slump resistance in preformed sealant tapes is achieved by combining HRD-23H with fillers such as ground calcium carbonate at 20–40 wt% and low-molecular-weight polybutene as the tack-adjusting diluent. The high-molecular-weight polyisobutylene fraction reduces cold flow at 60 °C, with slump or penetration measured by ASTM D217 or a 24 h compression creep test. Production-scale planetary mixers are run at 120–150 °C until the filler is fully wetted; addition of filler before the polymer has formed a coherent melt can produce dry lumps that survive downstream straining. The tape typically retains pressure-sensitive adhesion to polyethylene and aluminum without a separate primer, but adhesion to untreated polypropylene is limited. In outdoor sealing applications, 0.2–0.5 wt% carbon black or hindered-amine stabilizer may be incorporated to reduce ultraviolet surface crazing; published data for HRD-23H-specific weathering performance is limited, and outdoor qualification should include accelerated weathering per ISO 4892-2.

    When Cable-Filler Formulations Require Low-Temperature Flexibility and Low Dielectric Loss

    In water-blocking cable-filler compounds, HRD-23H is blended with low-viscosity hydrocarbon oils, fumed silica, and, where required, an antioxidant package to produce thixotropic gels. Viscosity at 25 °C by ASTM D2196 is typically adjusted to 10,000–50,000 mPa·s for void-filling and water-blocking performance. The glass transition of high-molecular-weight polyisobutylene below -65 °C supports low-temperature flexibility; cable-filler formulations containing HRD-23H are often required to pass bending tests at -40 °C without cracking. Unfilled polyisobutylene has a dielectric constant of approximately 2.2–2.3 at 1 MHz per ASTM D150, with dissipation factor below 0.001; filled compound values depend on filler type and moisture content. Polar plasticizers and polar processing aids raise dielectric loss and should be avoided; low-molecular-weight naphthenic oils may exude at elevated temperatures if the polyisobutylene phase is not sufficiently entangled. Published data for HRD-23H in filled cable-filler configurations is limited; qualification should include cable bending at -40 °C, water penetration testing, and dielectric strength per IEC 60243-1 on the finished cable core.

    Material handling on open two-roll mills at 100–120 °C requires stable band formation; release agents containing low-molecular-weight amides can plate out and reduce clarity in thin films. HRD-23H should not be combined with strong oxidizers, halogenated solvents at elevated temperature, or high-vinyl polybutadiene resins that phase-separate and create melt fracture. Pre-drying at 60–70 °C for 3–4 h is recommended when water content exceeds 0.1 wt% by ISO 15512. The product is not suitable for sulfur-vulcanization or peroxide cure; applications requiring permanent crosslinks and compression-set resistance must be reformulated with a curable elastomer such as butyl or EPDM. Avoid prolonged melt residence above 170 °C and high-shear mixing at speeds above 150 min⁻¹ because chain scission reduces molecular weight and cohesive performance.