Products

Polyisobutylene HRD-13H

    • Product Name: Polyisobutylene HRD-13H
    • Factroy Site: Yuanbaoshan District, Chifeng City, Inner Mongolia, P.R. China
    • Price Inquiry: sales8@alchemist-chem.com
    • Manufacturer: Inner Mongolia Eppen Biotech Co., Ltd.
    • CONTACT NOW
    VTB
    Specifications
    HS Code 896071
    Appearance Colorless to light yellow transparent viscous liquid
    Density At 20c 0.89-0.91 g/cm3
    Molecularweight Mn About 1300 g/mol
    Kinematicviscosity At 100c 250-350 mm2/s
    Flashpoint ≥180 °C
    Pourpoint ≤-20 °C
    Volatilematter ≤0.5%
    Ashcontent ≤0.02%
    Color Apha ≤50
    Watercontent ≤0.05%
    Acidvalue ≤0.05 mg KOH/g
    Vinylidenecontent ≥75%
    Solubility Soluble in hydrocarbons; insoluble in water

    As an accredited Polyisobutylene HRD-13H factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Polyisobutylene HRD-13H is packaged in 25 kg net-weight, polyethylene-lined fiber drums for safe industrial handling and storage.
    Container Loading (20′ FCL) Polyisobutylene HRD-13H securely packed and loaded into a 20-foot full container load (FCL) for shipment.
    Shipping Polyisobutylene HRD-13H is a non-hazardous polymer and is not classified as dangerous goods for transport. Ship in clean, dry, sealed packaging, protected from moisture, contamination, and excessive heat. Use standard industrial hygiene; no UN number, hazard class, or special shipping label is required.
    Storage Store Polyisobutylene HRD-13H in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizing agents. Keep containers tightly closed and clearly labeled to prevent contamination and moisture ingress. Avoid prolonged exposure to elevated temperatures. Store at ambient temperature, protect from physical damage, use secondary containment where required, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Store in a cool, dry, well-ventilated place; shelf life is typically 24 months under recommended conditions in unopened original packaging.
    Application of Polyisobutylene HRD-13H

    Which Mw and terminal vinylidene thresholds govern reactive PIBSA conversion in crankcase dispersants?

    The conversion of Polyisobutylene HRD-13H into polyisobutenyl succinic anhydride (PIBSA) requires two feedstock parameters to be verified before charging a maleation vessel: number-average molecular weight and terminal double-bond isomer distribution. Published analytical data for this specific grade are limited, so incoming inspection should follow gel permeation chromatography calibrated with narrow-distribution polyisobutylene standards and ISO 1133-1:2022 where melt flow rate is declared. High-reactivity PIB feedstocks for thermal maleation typically fall within 1000–1300 g/mol Mn and terminal vinylidene content above 70%. The Alder-ene addition of maleic anhydride across the terminal vinylidene group proceeds at 200–230°C under nitrogen pressure. The thermal maleation window is controlled within ±5°C; excursions above 235°C increase free maleic anhydride through the retro-ene reaction and generate toluene-insoluble gels. The molar feed ratio of maleic anhydride to PIB is usually maintained between 1.0:1 and 1.5:1, depending on terminal vinylidene content. Excess maleic anhydride is stripped in a wiped film evaporator at 3–10 kPa absolute pressure and recondensed. Free maleic anhydride in the PIBSA intermediate is controlled to 0.1–0.3 wt%; higher residual anhydride causes haze and uncontrolled polyamine crosslinking during the subsequent succinimide step. Amination with tetraethylenepentamine or polyethyleneamine at 150–170°C under vacuum produces a polyisobutenyl succinimide with total base number measured by ASTM D2896. Dispersancy response is not linear with total base number; products with a TBN of 20–30 mg KOH/g generally provide adequate soot suspension in heavy-duty diesel crankcase formulations, while higher TBN products require borated post-treatment. Production-scale glass-lined reactors show localized hot spots on wall baffles that form toluene-insoluble gels, and batch-to-batch variation in terminal vinylidene content above ±3% shifts the graft ratio. In-line filtration with 25 µm cartridge filters before the wiped film evaporator is required to protect the wiper blades from char particles. The resulting succinimide is shipped as a concentrate in process oil and formulated into heavy-duty diesel and passenger-car motor oils where ASTM D2270 viscosity index and ASTM D445 kinematic viscosity at 100°C are reconciled against detergent inhibitor package limits.

    Table 1. Representative amination response for high-vinylidene PIB of comparable Mn; values are not HRD-13H lot-specific data.
    PIBSA/polyamine molar feed ratioASTM D2896 total base number, mg KOH/gASTM D445 KV100, mm²/sASTM D874 sulfated ash, wt%
    1.0:112–1885–1200.05–0.15
    1.2:120–25110–1500.10–0.20
    1.5:128–35130–1800.15–0.30

    Gasoline port fuel injector deposit control intermediates derived from Polyisobutylene HRD-13H are manufactured through a chlorination–amination sequence rather than the maleation route. The PIB is chlorinated in a glass-lined reactor at 80–110°C with chlorine gas metered to a bound chlorine content of 2–4 wt%. Excess chlorine is stripped with nitrogen at 90°C until free chlorine is below 10 ppm to prevent corrosion in downstream Hastelloy equipment. The chlorinated intermediate is reacted with anhydrous ammonia at 150–180°C and 0.5–1.0 MPa gauge in a Hastelloy C-276 autoclave. The crude polyisobutylene amine is filtered through 10 µm media and diluted with aromatic solvent. At a gasoline treat rate of 50–300 mg/kg, the amine provides intake valve deposit control measured by ASTM D6201. Published data for this specific HRD-13H configuration are limited, so engine testing is required to confirm keep-clean performance below 100 mg per valve. The main process limitation is secondary amine by-product formation when ammonia stoichiometry drops below 1.2:1; secondary amines increase total nitrogen content and aggravate elastomer swelling in fuel system O-rings. Residual solvent must be removed to below 0.5 wt% by vacuum distillation before the additive is sold as a concentrate.

    Hot-melt adhesive open time and substrate wetting thresholds

    Polyisobutylene HRD-13H is metered into a co-rotating twin-screw extruder with an L/D ratio of 40:1 at barrel temperatures from 140–170°C. The screw configuration is set with three kneading blocks to disperse the polymer into metallocene-catalyzed polyolefin elastomers or ethylene-vinyl acetate copolymers without exceeding a residence time of 2 min. The addition level is limited to 5–15 wt%; higher loadings reduce the shear adhesion failure temperature measured by ASTM D4498 and broaden the melt transition. At 10 wt%, open time on polyethylene terephthalate substrates is extended to 8–12 s when applied from a slot-die coater at 160°C, while initial loop tack according to ASTM D6195 remains within 3.5–5.0 N/25 mm. Below 5 wt%, hot tack on clay-coated board becomes inconsistent; above 15 wt%, adhesive transfer and fiber tear failure modes appear because polyisobutylene domains reduce cohesive strength. Antioxidant systems based on hindered phenols at 0.3–0.5 wt% and phosphite co-stabilizers at 0.2 wt% are required because PIB undergoes chain scission in hot melt tanks held at 170°C for more than 8 h. Melt viscosity is verified by ASTM D3236 with spindle SC 4-27 at 175°C. Incompatibility must be noted with high-styrene SBS block copolymers: phase separation becomes visible as surface haze below 40°C when the styrene content exceeds 30%.

    A cable filling compound for optical fiber loose-tube construction combines Polyisobutylene HRD-13H with low-viscosity polybutene and fumed silica under vacuum planetary mixing at 60–80°C. The PIB component raises the yield stress of the gel without creating a chemically crosslinked network, which allows buffer tube re-entry and fiber stripping. Published formulation data for this specific grade are limited; typical hydrophobic filling compounds for outdoor optical cable use PIB at 5–20 wt%, fumed silica at 3–8 wt%, and antioxidant at 0.2–0.5 wt%, with the balance a low-volatility polybutene. Cone penetration is maintained between 350 and 450 1/10 mm at 25°C according to ASTM D217 to ensure pumpability while preventing flow-out at 70°C. Oil separation after 24 h at 80°C is controlled below 2.0% when the fumed silica dispersion passes through a three-roll mill or high-shear rotor-stator device. The mill gap must be set at 25–40 µm; larger gaps leave undispersed silica agglomerates that create optical attenuation under microbending in IEC 60794-1-2 temperature cycling. Silicone oil must be excluded; migration to the fiber coating reduces long-term adhesion of the primary acrylate coating. Batch release tests include DIN 51807 water resistance, cone penetration, and density by ASTM D1475. The terminal gel must not exhibit syneresis after 30 days at 60°C. Production-scale filling equipment shows air entrapment when viscosity at 25°C exceeds 2000 mPa·s and pump cavitation when the feed hopper is not under nitrogen blanketing.

    If polyisobutylene is used as a food-contact masticatory base component, 21 CFR 172.615 becomes the binding compliance boundary

    When Polyisobutylene HRD-13H is evaluated for chewing gum base, the formulation is governed by 21 CFR 172.615, which lists polyisobutylene as a permitted masticatory substance when used in accordance with current good manufacturing practice. For food-contact articles, 21 CFR 177.1420 applies to isobutylene polymers and specifies extraction testing with distilled water and n-hexane as food simulants. Compliance documentation must identify residual isobutylene monomer, total nonvolatile residue, and catalyst residues from upstream manufacturing. If the specific grade has high molecular weight, the extraction risk is reduced, but published data for HRD-13H itself are limited and should be generated on each lot. The compounding temperature in a sigma-blade mixer is held at 80–110°C; addition levels of PIB in gum base are typically 5–20 wt% depending on the elastomer and resin blend. The PIB is incorporated after butyl rubber is masticated to avoid localized overheating. Softening point measured by ASTM D36 remains above 60°C. Antioxidants permitted for the application are limited to those listed in 21 CFR 172.615; amine-based stabilizers are excluded because of nitrosamine formation concerns. Residual maleic anhydride or chlorine from upstream production must be below detection limits if the PIB is not expressly cleared for those contaminants. The finished chewing gum remains subject to the food additive definitions in 21 CFR 172.615; it is not acceptable to use industrial PIB with unknown catalyst residues without an appropriate food-contact clearance.

    Table 2. Regulatory and standards matrix for Polyisobutylene HRD-13H downstream qualification.
    Regulation/standardScopeCritical test or parameterTypical control range
    21 CFR 172.615Chewing gum base masticatory substancesIdentity and residual monomerNot specified; current GMP
    21 CFR 177.1420Isobutylene polymers in food-contact articlesDistilled water and n-hexane extractionLot-specific
    EU Regulation (EC) No 1223/2009Cosmetic productsProduct safety reportNo Annex II restriction for PIB
    EU Regulation (EU) No 10/2011Plastic food-contact materialsOverall migration10 mg/dm²
    IEC 60794-1-2Optical fibre cable environmental testingTemperature cycling attenuationNo attenuation step
    ASTM D6201Spark-ignition engine intake valve depositsEngine testKeep-clean below 100 mg per valve for developmental fuels

    Sunscreen and long-wear decorative cosmetic formulations use Polyisobutylene HRD-13H as an oil-phase film former at concentrations of 1–10 wt%. The polymer is dissolved in isododecane or cyclopentasiloxane at 50–70°C in a jacketed vessel with counter-rotating blades before the aqueous phase is added under high-shear homogenization. Water resistance under the 40-minute immersion condition described in FDA sunscreen testing guidance is maintained when PIB is combined with alkylated polyvinylpyrrolidone; polyisobutylene alone does not provide sufficient emulsion stabilization above 10 wt% because the film becomes tacky and causes skin feel defects. The addition of hydrophobic fumed silica at 0.5–2.0 wt% offsets tack but increases yield stress, which may clog filling nozzles below 5 mm diameter. The final emulsion is packaged at 25–35°C; viscosity at 25°C is measured by ISO 2555 with spindle R4 at 10 rpm. Cosmetic compliance is anchored to EU Cosmetic Products Regulation (EC) No 1223/2009 and manufacturing hygiene under ISO 22716. No Annex II or Annex III restriction applies to polyisobutylene, but residual isobutylene monomer must be controlled because it is not a permitted fragrance ingredient. Production-scale failures include phase inversion when the oil phase is cooled below 45°C before homogenization; the emulsion drops out as visible translucent patches at 4°C in stability chambers.

    Stretch film cling force thresholds are not sufficient without blocking and unwind force data

    Polyisobutylene HRD-13H is dry-blended into linear low-density polyethylene at 0.5–3.0 wt% and melt-compounded in a single-screw extruder with an L/D ratio of 30:1. The PIB migrates to the film surface within 24–72 h after cast extrusion and imparts cling without adhesive transfer. Cling force measured by ASTM D5458 on 23 µm blown film generally reaches 100–350 g when PIB addition is 1–2 wt%; below 100 g the rolls telescope during winding and transport. Above 3 wt%, unwind force rises beyond 350 g and generates audible blocking at high-speed prestretch units operating at 150–300 m/min. The additive must be metered with a loss-in-weight feeder because pelletized polyisobutylene can bridge in the throat if hopper temperature exceeds 35°C. Tensile properties are verified by ASTM D882; elongation at break does not shift more than 10% relative to the neat resin at 2 wt% loading. The film also shows a reduction in coefficient of friction against stainless steel to 0.3–0.5 when tested by ASTM D1894, which suppresses chatter on high-speed wrappers. The PIB domain size in the LLDPE matrix should remain below 5 µm; larger domains create visible surface defects under polarized light. If the film is used for food packaging, 21 CFR 177.1420 and EU Regulation (EU) No 10/2011 apply to the final film, and the converter must confirm the specific migration limit for polyisobutylene. Published data for this specific HRD-13H grade are limited; converter trials are required to confirm blocking at the desired gauge.

    Free Quote

    Competitive Polyisobutylene HRD-13H prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@alchemist-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@alchemist-chem.com

    Inquiry

    Get Free Quote of Inner Mongolia Eppen Biotech Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Polyisobutylene HRD-13H is a high-reactivity isobutylene homopolymer intermediate intended for functionalization rather than direct compounding. The product belongs to the polyisobutylene class identified by CAS 9003-27-4 and is differentiated from mixed-C4 polybutenes by its linear isobutylene repeat unit and its terminal vinylidene architecture. In downstream processing, this architecture determines how efficiently maleic anhydride can be added by the thermal ene route. The grade designation is read operationally as a high-reactivity product line with a nominal viscosity band; however, because the manufacturer has not published a consolidated public specification for HRD-13H in standard third-party databases, the parameters presented below are method-level acceptance parameters and class-typical ranges for high-reactivity polyisobutylene of the same viscosity designation. Supplier certificate-of-analysis values should replace class-typical ranges for any release decision.

    What incoming acceptance parameters define HRD-13H?

    Incoming inspection of HRD-13H should include viscosity, molecular weight distribution, terminal vinylidene content, water, density, flash point, and colour. Viscosity is measured at 100 °C because the polymer is too viscous for reproducible room-temperature capillary flow. The test grid in Table 1 uses standard methods applicable to polyisobutylene; the numerical ranges shown are representative of a high-reactivity PIB grade carrying the 13H viscosity designation and are not a substitute for the supplier certificate of analysis.

    Property Test method Unit Typical class range / requirement
    Kinematic viscosity at 100 °C ASTM D445 mm²/s 12.5–14.5
    Density at 20 °C ISO 12185 g/cm³ 0.890–0.915
    Flash point, Cleveland open cup ASTM D92 °C > 170
    Colour ASTM D1500 — ≤ 0.5
    Number-average molecular weight, Mn GPC with PIB calibration Da 1,200–1,600
    Dispersity, Mw/Mn GPC ratio 1.8–2.5
    Terminal vinylidene content ¹H NMR mol% 65–85
    Water content ASTM D6304 mg/kg ≤ 50

    Of these methods, ¹H NMR is the most product-specific. The exo-olefin protons of terminal vinylidene groups are integrated at 4.74 ppm and 4.84 ppm against a known internal standard. Gas chromatography of low-molecular-weight oligomers is not sufficient for Mn and dispersity because the sample contains oligomers up to several thousand daltons.

    For bulk handling, HRD-13H is typically transferred at 50–80 °C through jacketed stainless-steel pipework using positive-displacement gear pumps. At lower temperatures, the viscosity rises sharply and can exceed the suction capability of centrifugal pumps. Tanks should be blanketed with dry nitrogen at 5–20 kPa; entry of atmospheric moisture and oxygen contributes to colour development and may affect downstream maleation repeatability. Mass-flow measurement is preferred over volumetric metering because a viscosity swing of ±0.5 mm²/s at 100 °C can shift the polymer charge in a volume-controlled PIBSA reactor and alter the final anhydride number.

    When HRD-13H replaces conventional PIB in maleation reactors

    Conventional low-reactivity PIB exhibits terminal vinylidene levels below 10 mol%; therefore, its conversion to polyisobutenyl succinic anhydride requires chlorination or high-temperature radical promotion. HRD-13H, as a high-reactivity grade, is expected to contain 65–85 mol% terminal vinylidene, permitting thermal ene addition of maleic anhydride at 200–230 °C under nitrogen pressure. The reactor charge is usually maintained at a maleic anhydride:polymer molar excess of 1.5:1 to 2.0:1 to drive conversion. Free maleic anhydride after vacuum stripping is controlled below 0.5 wt% to avoid side reactions in subsequent amine condensation.

    The main processing difference is not only speed; it is the removal of chlorine from the reactive sequence. Chlorinated PIB intermediates can cause chloride stress-corrosion in stainless steel and require post-washing to control hydrolyzable chloride. The thermal-ene route used with HRD-13H avoids that unit operation, although it introduces a different safety boundary: maleic anhydride vapour pressure at reaction temperature requires a sealed reactor, rupture-disk sizing per ISO 4126-1, and local ventilation at the charging station. Published data for the exact maleation heat release of HRD-13H are limited; reactor thermal design should therefore use calorimetric screening on the specific lot before scaling to a production vessel.

    The resulting PIBSA is condensed with polyethylene polyamines at 150–170 °C, typically in a jacketed reactor with vacuum stripping to remove water of condensation. The choice of HRD-13H over a lower-viscosity PIB increases the hydrocarbon chain length per succinimide group, which raises dispersancy persistence in heavy-duty diesel formulations but also increases the viscosity of the final dispersant. Formulators compensate by shifting to a lower molar charge ratio or by selecting a heavier diluent oil.

    Viscosity-temperature and heat-transfer limitations

    The viscosity-temperature relationship of HRD-13H should be modelled using ASTM D341 for extrapolation of viscosity to storage and pumping conditions. A high-reactivity PIB in the 13H band remains a Newtonian liquid over normal shear rates, but its low thermal conductivity limits heat transfer in jacketed storage tanks and reactor preheaters. Laminar-flow heat exchangers are typically used because turbulent flow is impractical at line velocities below 1 m/s. Coil or plate exchangers should be designed with wall temperatures below 180 °C to avoid local film degradation; the bulk temperature should not exceed 80 °C during extended storage, and residence time above 120 °C should be limited to short in-line heating.

    For injection into a continuous reactor, a thermal mass flowmeter and a positive-displacement gear pump with 1–5 m³/h capacity can provide stable feed. Batch-to-batch variation in low-shear viscosity has been traced to variation in high-molecular-weight tails; this is why dispersity is monitored even when the Mn is within specification.

    Complying with REACH and controlling oxidative degradation

    HRD-13H is a polymer within the meaning of REACH and is generally exempt from registration as a polymer under Title II, Article 2(9), provided it meets the conditions for polymer status and the monomers are registered. The product is not supplied under a recognised food-contact clearance; compliance with FDA 21 CFR 178.3570 or equivalent is a final-formulation exercise, not an inherent property of the raw polymer. Occupational exposure control should consider hydrocarbon aspiration hazard, mist generation, and combustible-liquid storage under local fire codes; flash-point classification follows ASTM D92 but regional transport classification may also require ASTM D93 or ISO 2719.

    HRD-13H should not be blended with strong oxidizers, free halogens, or acidic clays in storage. The polymer is hydrophobic, but prolonged contact with copper alloys at temperatures above 80 °C can catalyse colour formation. For applications requiring low ash and low chlorine, the supplier should be asked for lot-specific values because high-reactivity BF3-catalysed PIB can retain catalyst residues if not adequately deactivated and filtered.

    Parameter Conventional PIB High-reactivity PIB class represented by HRD-13H Metallocene HR-PIB
    Terminal vinylidene content 5–10 mol% 65–85 mol% 85–95 mol%
    Number-average molecular weight 500–5,000 Da 1,000–2,500 Da for the 13H viscosity band 1,000–5,000 Da
    Typical catalyst system AlCl₃ or BF3 BF3 Metallocene
    Maleation route Chlorination or radical promotion Thermal ene addition Thermal ene addition, faster
    Primary downstream intermediate Chlorinated PIB or PIBSA PIBSA and polyisobutenyl succinimides PIBSA with higher vinylidene reactivity

    The operational distinction between HRD-13H and conventional PIB is therefore not only chemical composition but engineering route. Conventional PIB may require chlorinated intermediate handling and imposes corrosion and wastewater controls; HRD-13H shifts the plant to thermal maleation with lower chloride load, but with stricter control of reactor temperature and nitrogen pressure. Compared with metallocene HR-PIB, HRD-13H is expected to provide a broader molecular weight distribution and lower terminal vinylidene content; this can reduce raw-material cost per tonne of dispersant but may require higher stripping temperatures to reach the same free maleic anhydride limit. Compared with lower-viscosity grades in the same high-reactivity family, HRD-13H provides a higher hydrocarbon-to-functional-group ratio, which improves high-temperature varnish control in diesel crankcase dispersants but increases feed viscosity and may require a heated addition system.

    In fuel detergent intermediate production, HRD-13H can be hydroformylated or epoxidized to yield polyisobutenyl amines or polyisobutenyl alcohols. The terminal exo-olefin geometry is the critical parameter because internal olefins are significantly less reactive in catalytic hydroformylation. A vinylidene content at the upper end of the class range reduces the required molar excess of synthesis gas and lowers heavy-end formation in the subsequent amination step. Downstream tests for the finished detergent package are application-specific and include ASTM D6201 for intake valve deposit control in gasoline engines; the raw polymer itself is not rated by that test and must be evaluated as part of the finished formulation.