| HS Code | 133214 |
| Chemical Name | Polyisobutylene |
| Grade | HRD-10H |
| Cas Number | 9003-27-4 |
| Appearance | Colorless to light yellow transparent viscous liquid |
| Molecular Weight Mn | approx. 1000 g/mol |
| Density At 20c | approx. 0.89 g/cm3 |
| Viscosity At 100c | approx. 200-500 mPa.s |
| Flash Point | >180 °C |
| Pour Point | < -30 °C |
| Color Apha | <=50 |
| Volatile Matter | <=0.5% |
| Water Content | <=0.05% |
| Acid Value | <=0.05 mg KOH/g |
| Solubility | Soluble in aliphatic and aromatic hydrocarbons; insoluble in water |
| Vinylidene Content | >=80% |
As an accredited Polyisobutylene HRD-10H factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Polyisobutylene HRD-10H is supplied in 25 kg net, polyethylene-lined paper bags, palletized and stretch-wrapped for industrial shipment. |
| Container Loading (20′ FCL) | Polyisobutylene HRD-10H is loaded into a 20′ FCL container, securely stowed and lashed for safe ocean transportation. |
| Shipping | Polyisobutylene HRD-10H is shipped as a non-hazardous polymer in clean, sealed containers. No UN number or dangerous-goods classification applies for DOT, ADR, IMDG, or IATA transport. Keep containers closed, dry, and protected from heat, sunlight, and contamination; store in a cool, ventilated area. |
| Storage | Store Polyisobutylene HRD-10H in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and ignition. Keep containers tightly closed, clearly labeled, and in original packaging. Protect from moisture, dust, and contamination, and separate from strong oxidizers. Avoid prolonged exposure to elevated temperatures. Use secondary containment to prevent spills. Follow local regulations and the manufacturer’s safety data sheet. |
| Shelf Life | Polyisobutylene HRD-10H typically has a shelf life of about 24 months when stored unopened in a cool, dry, well-ventilated area away from sunlight. |
During loose-tube optical fibre cable production, water-blocking filling compounds are compounded in a jacketed disperser equipped with a high-shear saw-tooth impeller. Polyisobutylene HRD-10H is introduced as a rheology modifier into a naphthenic or paraffinic mineral oil carrier at 120 °C for 45–60 min to obtain a bubble-free polymer concentrate before fumed silica is dispersed. The PIB concentration in the finished filling gel is held at 6–14 wt%; below 6 wt% the thixotropic recovery at 25 °C is insufficient to prevent cable drip after vertical installation, while above 14 wt% low-temperature cone penetration and pumpability at −20 °C may move outside the operating window of gear-pump filling heads. Antioxidant addition of 0.2–0.5 wt% hindered phenolic type is required to limit thermo-oxidative chain scission during hot storage at 100 °C. Compliance testing follows the water penetration procedure in IEC 60794-1-2:2017, with additional dielectric and flash point verification under ASTM D92 and ASTM D150. The filling process applies vacuum degassing at −0.09 MPa for 20–30 min after silica addition, followed by delivery through 100–150 µm filtration and injection into buffer tubes at 1.5–3.0 MPa. End products include loose-tube optical fibre cables, stranded copper telecom riser cables, microduct water-blocking gels, and hybrid fibre-copper cable core flooding compounds. Published direct test data for HRD-10H in exact buffer-tube gel matrices is limited; the stated rheological window reflects the high-molecular-weight PIB class used in cable compounding.
Formulation of a dual-seal insulating glass unit edge seal places the polyisobutylene primary seal between the aluminium spacer and the secondary silicone or polysulfide seal. HRD-10H is dosed at 30–45 wt% into a sigma-blade kneader together with 10–20 wt% furnace carbon black and 20–35 wt% precipitated calcium carbonate; the carbon black improves UV opacity and mechanical integrity of the edge seal. The mixing sequence runs at 80–110 °C under −0.08 MPa vacuum. The polymer is masticated for 10 min before fillers are added in two stages to prevent agglomeration and to maintain batch-to-batch colour and needle penetration consistency. The compounded sealant is extruded through a heated gear pump with 40–60 µm screens at 90–100 °C and applied as a 1.0–1.5 mm continuous bead onto the spacer frame. Compliance with EN 1279-4:2018 requires that moisture vapour transmission and fogging behaviour remain within the specified limits after edge-seal ageing; ASTM E2188-19 and ASTM E2190-19 provide corresponding performance testing for insulating glass units in the North American market. Published moisture vapour transmission rates for high-molecular-weight PIB primary sealants are typically below 0.02 g/m²·day at 23 °C and 85% RH; grade-specific MVTR for HRD-10H in this exact formulation is not independently published. HRD-10H should not be combined with low-molecular-weight polybutene above 10 wt% in this application because volatile fractions can migrate into the air gap and increase fogging under solar exposure. End products include dual-seal IGUs for commercial curtain walls, triple glazing for low-energy residential facades, and edge seals in laminated architectural glass.
After the aluminium complex grease gel reaches its peak temperature and the soap structure has formed, HRD-10H is metered as a pre-diluted 10 wt% solution in naphthenic base oil at 120 °C. The final PIB concentration is 1.5–4.0 wt% of the finished grease mass. At concentrations below 1.0 wt% the stringiness and adhesion required for open gear lubricant retention on slow-moving gear flanks are not achieved; above 4.5 wt%, worked cone penetration under ASTM D217 may fall below 220 mm/10 and central lubrication system pumpability deteriorates. Counter-rotating paddle agitation at 300–500 min⁻¹ disperses the PIB solution before the grease passes through a high-pressure homogenizer set at 15–25 MPa to eliminate polymer-rich striations. Conformity is assessed under ISO 6743-9:2003 for family X grease classification and DIN 51825:2014 for lubricating greases K-group requirements; water washout behaviour is verified with ASTM D1264-18. HRD-10H is not recommended for lithium or silicone greases where low tack and transparent appearance are specified, because even 1 wt% addition produces visible hazing and increases unworked tack. End products include high-tack open gear lubricants, wire rope dressings, fifth-wheel greases, and slow-moving bearing compounds for mining and marine deck equipment.
For fuel additive synthesis, HRD-10H is applied as a high-reactivity polyisobutylene feedstock; the terminal vinylidene content must be confirmed on the batch certificate before charging. The thermal ene reaction is carried out in a stirred autoclave at 200–230 °C under 0.3–0.5 MPa nitrogen, with a maleic anhydride-to-PIB molar ratio of 1.2:1–1.5:1; residence time is 6–10 h depending on the target anhydride number and the supplier-certified terminal vinylidene content of HRD-10H. Unreacted maleic anhydride is removed by vacuum stripping at 160 °C and 10 kPa before the succinic anhydride intermediate is amidated with triethylenetetramine or tetraethylenepentamine at 140–160 °C. The terminal vinylidene content controls ene-reaction yield; high-reactivity PIB grades in this class generally require above 70 mol% vinylidene to achieve PIBSA yields above 80%, but the exact conversion curve for HRD-10H must be taken from the supplier certificate for the production batch. Engine test methods for finished deposit-control additives include ASTM D6201-19 for intake valve deposit formation and CEC F-20-98 for gasoline engine deposit control performance. Treat rates of the finished PIB-amine package in gasoline range from 50–300 mg/kg. End products include port fuel injector detergents, diesel injector clean-up packages, PIBSA-based lubricant dispersant intermediates, and multifunctional packages for refinery pipelines. Oxygen ingress during the ene reaction must be limited below 50 ppm in the nitrogen blanket because oxidative coupling produces high-viscosity gel fractions that foul the atomized stripping nozzles.
Roofing underlayment tapes and air-barrier lap tapes are calendered from butyl rubber compounds in which HRD-10H functions as a plasticiser, tack retention agent, and low-temperature conformability modifier. The compound is mixed in a tangential internal mixer with a fill factor of 70–75% at 90–120 °C; the PIB loading is 10–25 wt%, combined with 10–20 wt% butyl rubber, 30–45 wt% ground calcium carbonate, 5–12 wt% C5 hydrocarbon tackifier, and 0.1–0.3 wt% hindered phenolic antioxidant. The mixed compound is discharged as a continuous strip at 80–100 °C and calendered onto siliconised release paper at 0.5–2.0 mm thickness, followed by water-quench cooling to 25 °C before slitting. Cold flow resistance is evaluated according to EN 13880-3:2016; water tightness and peel adhesion on prepared concrete and metal substrates are assessed under EN 13969:2016 and ASTM D1970-20. At PIB loadings above 25 wt%, edge ooze and release-liner bleed occur after 7 days at 40 °C; below 10 wt%, low-temperature adhesion to roughened steel and concrete drops below the minimum required for self-adhered roofing underlayment installation below 5 °C. HRD-10H must be protected from humidity above 60% RH prior to mixing because absorbed moisture forms bubbles during calendering and reduces liner release consistency. End products include self-adhered roofing underlayments, window sill flashing tapes, pipe-wrap protection tapes, and air/vapour barrier lap strips.
Temporary protection films for coil-coated aluminium and stainless steel use a solventless hot-melt pressure-sensitive adhesive that is slot-die coated at 150–170 °C onto a corona-treated low-density polyethylene carrier. HRD-10H is incorporated at 5–15 wt% into a styrene-isoprene-styrene block copolymer matrix with 30–45 wt% hydrogenated hydrocarbon resin and 0.5–1.0 wt% antioxidant. The high molecular weight of HRD-10H slows migration into the polyethylene carrier and reduces ghosting after removal from stainless steel panels stored at 50 °C for 72 h. Peel adhesion is measured on stainless steel panels under ASTM D3654/D3654M-2019 at 180° peel angle and 300 mm/min crosshead speed; loop tack is evaluated according to ISO 29862:2018. For removable protection films the target peel range is 1.5–6.0 N/25 mm. The compound should not be used at service temperatures above 80 °C, because residue on matte and bright metal surfaces increases above this boundary. End products include surface protection films for architectural aluminium profiles, stainless steel sheeting, polycarbonate panels, and pre-painted automotive body panels.
Competitive Polyisobutylene HRD-10H prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@alchemist-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@alchemist-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Polyisobutylene HRD-10H is a fully saturated isobutylene homopolymer supplied under a grade designation that denotes a controlled-viscosity polyisobutylene rather than a sulfur-curable elastomer. The polymer backbone is built from repeating isobutylene units, yielding a low glass transition, low moisture permeability, and resistance to hydrolysis; intentional olefinic unsaturation is not a specification feature. CAS registry number 9003-27-4 describes the homopolymer class, but additive and stabilizer content is product-specific. Published independent test data for HRD-10H specifically are limited, so the numerical ranges and property boundaries in this document are presented as the specification envelope for medium-viscosity polyisobutylene grades and should be verified against the supplier’s certificate of analysis.
Physical form is not uniformly indicated by the grade designator. HRD-10H may be supplied as a clear, water-white to pale-yellow viscous liquid or soft bale solid, depending on the producer and the molar-mass setpoint. Neat colour is characterized by APHA colour per DIN EN ISO 6271, with fresh material typically below 50 APHA; heat history and oxygen exposure can increase colour. Packaging specifications should be confirmed because viscosity class alone does not distinguish between drum, pail, or bale formats.
The primary separation from low-molar-mass polybutenes is volatility under oven exposure and migration in compounded matrices. Polybutenes with viscosity-average molecular weight below 5,000 g/mol function as migratory plasticizers, showing measurable weight loss under ASTM D972 at 120°C for 24 h. HRD-10H belongs to a higher molar-mass band in which the polymer remains less volatile and more cohesive; the penalty is higher zero-shear viscosity and reduced ambient-temperature flow. Butyl rubber grades possess 1 to 2 mol% isoprene units that provide allylic sites for sulfur or quinoid cure. HRD-10H has no such cure sites and cannot be vulcanized with sulfur, zinc oxide, or phenolic resin systems. In a hot-melt adhesive, therefore, HRD-10H contributes tack retention and cohesive strength through chain entanglement rather than crosslink density.
Viscosity comparisons should be made under equivalent shear conditions. Low-molar-mass polybutenes typically display Newtonian behaviour over a wide shear range, whereas medium-viscosity polyisobutylene may show shear-thinning above 10 s⁻¹ in cone-plate geometry. Measurement per ISO 3219 at 100°C is more informative than melt flow rate, because PIB is not a polyolefin with a defined MFR under ISO 1133-1.
| Property | Test method | Representative range | Relevance to HRD-10H |
|---|---|---|---|
| Kinematic viscosity at 100°C | ASTM D445 / ISO 3104 | 150–400 mm²/s | Lot acceptance and pump sizing |
| Density at 25°C | ISO 1183-1 | 0.91–0.93 g/cm³ | Volume-to-mass conversion in dosing |
| Glass transition temperature | ISO 11357-2 | -70°C to -60°C | Low-temperature flexibility and tack |
| Volatility 10 h at 120°C | ASTM D972 | <0.5 wt% | High-temperature processing stability |
| Polydispersity Mw/Mn | ISO 16014-3 | 1.5–2.5 | Phase morphology and cold flow |
| Moisture content | ISO 15512 | <0.1 wt% | Pre-drying not usually required below this limit |
These values are class boundaries from published polyisobutylene literature and are not a substitute for the HRD-10H certificate of analysis.
In hot-melt adhesive mixing, HRD-10H is added after the tackifier and wax have reached a homogeneous molten phase at 160°C to 180°C in an anchor-rotor mixer. Typical addition levels are 2 wt% to 8 wt% in styrenic block copolymer systems, where the PIB phase reduces melt viscosity and increases wet-out on low-energy substrates. Peel adhesion change is substrate-dependent and should be quantified by ASTM D903 on stainless steel or polypropylene rather than by extrapolation from viscosity data alone. Oven aging at 177°C for 168 h may reveal antioxidant demand because the saturated backbone does not eliminate radical initiation at tertiary carbon centres; published data for this exact grade are limited.
Compatibility with hydrocarbon tackifier resins is maintained at resin-to-PIB mass ratios below approximately 4:1; above this boundary, phase separation can appear as surface haze after 48 h at 60°C in forced-air circulation, with optical assessment per ASTM D1003. Paraffinic oil concentrations above 10 wt% can drive surface exudation, measured as filter-paper mass increase after 72 h contact under 5 kPa at 70°C. In styrene-ethylene-butylene-styrene formulations, the use of HRD-10H above 10 wt% may soften the styrenic domains; tensile strength and elongation should be measured according to ISO 37 or ASTM D638-14 to confirm that cohesive failure mode is not lost. The exact compatibility envelope for HRD-10H should be determined on the production mixer because lot-to-lot molar-mass distribution influences phase stability.
Dynamic oscillatory measurements at 60°C reveal a pronounced rubbery plateau for medium-viscosity polyisobutylene. The crossover frequency from storage modulus to loss modulus shifts to lower frequencies as molar mass and polydispersity increase; this crossover is a more sensitive specification indicator than single-point viscosity when blending with tackifiers. A controlled-strain rheometer with 25 mm parallel plates and a 1 mm gap can detect lot-to-lot differences in relaxation spectrum that affect adhesive cold flow. The relaxation time at ambient temperature can exceed 100 s for high-molar-mass PIB, leading to elastic memory in extrusion; HRD-10H is selected to reduce that memory while retaining enough chain entanglement for cohesive strength.
In a 75 mm co-rotating twin-screw compounder with an L/D 44:1 configuration, HRD-10H is usually introduced through a heated liquid-feed port or as a pre-compounded masterbatch rather than through the main throat. Barrel temperatures above 200°C are avoided because oxidative chain scission accelerates above this point under oxygen, reducing viscosity and generating low-molar-mass volatiles. Specific energy input of 0.12 kWh/kg to 0.18 kWh/kg has been observed in rubber compounds containing 5 wt% PIB, but screw configuration and throughput alter this value. Melt temperature at the die is controlled at 120°C to 150°C to maintain viscosity and prevent stringing. Vacuum devolatilization in twin-screw extrusion is configured at -0.08 MPa to -0.09 MPa to strip volatile oligomers without excessive residence time.
The saturated polyisobutylene backbone provides lower oxygen and moisture permeability than many mineral oil and polybutene plasticizers. Oxygen transmission rate in compounded films is measured per ASTM D3985 at 23°C and 0% RH; water vapour transmission is measured per ISO 15106-2 at 38°C and 90% RH. Higher molar mass reduces permeability but raises application viscosity, so HRD-10H is positioned for sealants and adhesives where low migration is more critical than low-temperature pumpability. In porous substrates, plasticizer migration is evaluated by contact staining under 70°C and 50% RH for 7 days; substituting 5 wt% polybutene with HRD-10H reduces stain radius when measured according to ASTM D2203. Published data for this specific configuration are limited.
Low-temperature compression and probe-tack tests are needed because the glass transition of PIB is below -60°C. Probe tack per ASTM D2979 on a stainless steel probe at 23°C to 25°C can separate grades that have identical kinematic viscosity but different low-molar-mass tails; a broader molar-mass distribution increases cold flow and probe tack while reducing shear holding power. Shear adhesion failure temperature is measured per ASTM D4498 with a 1 kg load and 25 mm × 25 mm lap area.
Polyisobutylene HRD-10H is used in solvent-free butyl-type sealant compounds at 5 wt% to 15 wt% to increase slump resistance while retaining low-temperature deformability. Slump is measured per ISO 7390 at 50°C; low-temperature flexibility is evaluated by bending a 6 mm bead after 24 h conditioning at -20°C. Because HRD-10H does not contain cure sites, it forms discrete PIB domains in a diene rubber continuous phase and does not co-crosslink. Compression set of such blends is higher than a vulcanized butyl formulation; for parts requiring compression set below 30% after 22 h at 70°C per ISO 815-1, HRD-10H cannot directly replace butyl rubber. The product’s role is that of a migration-resistant plasticizer and tackifier, not a network former.
Polyisobutylene homopolymers may be used in articles intended for food contact under 21 CFR 177.1420 when end-use limitations and good manufacturing practices are met; the specific HRD-10H status depends on residual monomer, catalyst residues, and stabilizer selection. Under REACH (EC) 1907/2006, the polymer may qualify for the polymer registration exemption if the monomer is registered and the substance meets the current ECHA polymer definition; a supplier confirmation is required rather than a blanket statement. RoHS 2011/65/EU restrictions apply to additives and colourants, not the base polymer; homogeneous-material limits are 100 ppm for cadmium and 1000 ppm for lead, mercury, hexavalent chromium, PBB, and PBDE. Heavy-metal screening is commonly performed by X-ray fluorescence per IEC 62321-3-1.
| Reference | Scope | Typical acceptance basis |
|---|---|---|
| FDA 21 CFR 177.1420 | Isobutylene homopolymers in food-contact articles | Supplier FDA status letter |
| REACH (EC) 1907/2006 | Polymer registration exemption | Monomer registration and SDS |
| RoHS 2011/65/EU | Restricted heavy metals in homogeneous materials | 100 ppm Cd; 1000 ppm other restricted substances |
| ISO 15512 | Water content | <0.1 wt% before processing |
| ASTM D445 | Kinematic viscosity at 100°C | Supplier lot range |
In rubber compounding, HRD-10H is used as a processing and tackifying additive in inner-liner, curing-bladder, and damping compounds. The addition level of 2 phr to 8 phr is introduced early in the mixing cycle to reduce stock temperature and increase green tack without adding sulfur-available unsaturation. Mooney viscosity reduction is measured at ML 1+4, 100°C per ISO 289-1; because the effect is compound-specific, published data for this exact grade are limited. In chlorobutyl compounds, the saturated PIB phase can reduce mill sticking and improve extrudate surface, but the product should be evaluated with standard accelerated aging per ISO 188 at 100°C for 72 h to confirm retention of tensile and elongation. Storage should be in closed containers below 40°C and away from direct sunlight. Prolonged exposure to air at elevated temperature increases peroxide content, which can be detected by iodometric titration; polar additives and strong oxidizing agents are excluded unless compatibility has been demonstrated. Cutting equipment designed for low-Tg polymers is required for bale forms because the material can cold-flow under sustained load.